Structural, microstructure and electrical properties of La2O3-doped Bi0.5(Na0.68K0.22Li0.01)0.5TiO3 lead-free piezoelectric ceramics synthesized by the combustion technique

被引:27
|
作者
Bhupaijit, Pamornnarumol [1 ]
Kornphom, Chittakorn [1 ,2 ]
Vittayakorn, Naratip [3 ]
Bongkarn, Theerachai [1 ,2 ,4 ]
机构
[1] Naresuan Univ, Fac Sci, Dept Phys, Phitsanulok 65000, Thailand
[2] Naresuan Univ, Fac Sci, Res Ctr Acad Excellence Appl Phys, Phitsanulok 65000, Thailand
[3] King Mongkuts Inst Technol Ladkrabang, Fac Sci, Dept Chem, Bangkok 10520, Thailand
[4] Naresuan Univ, Res Ctr Acad Excellence Petr Petrochem & Adv Mat, Phitsanulok 65000, Thailand
关键词
Combustion technique; Perovskite structure; Dielectric; Piezoelectric; Ferroelectric; FERROELECTRIC PROPERTIES;
D O I
10.1016/j.ceramint.2015.03.226
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of firing temperatures on phase formation, microstructure and physical properties of [Bi-0.5(Na0.68K0.22Li0.1)(0.5)TiO3] doped with La2O3 at 0.1 wt% (BNKLLT) ceramics prepared by the combustion method was studied. Glycine was used as fuel and the ratio of raw material (corresponding oxidant metal nitrate) with fuel was about 1:0.56. The samples were calcined at 600-900 degrees C for 2 h and sintered at 1075-1150 degrees C for 2 h. The single rhombohedral peroveskite phase of BNKLLT powders was observed from the sample calcined at 750 degrees C for 2 h. The BNKLLT ceramics exhibited a pure peroveskite phase in all samples. The microstructures of the BNKLLT powders exhibited an agglomerated form while the grain ceramics exhibited a square shape. The average particle size and average grain size increased with increasing firing temperatures. The density, dielectric constant (epsilon(r) and epsilon(m)), P-r and d(33) tended to increase with increasing sintering temperatures up to 1100 degrees C and then decreased. The maximum density (5.73 g/cm(2)), maximum dielectric constant (epsilon(r)similar to 2572 and epsilon(m)similar to 5536), good ferroelectic properties (P-r similar to 35.78 mu C/cm(2) and E-c similar to 22.42 kV/cm) and highest d(33) (210 pC/N) were obtained by the sample sintered at 1100 degrees C for 2 h. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:S81 / S86
页数:6
相关论文
共 50 条
  • [21] Role of ZnO nanoparticle doping on depolarization temperature, piezoelectric and energy harvesting properties of lead-free Bi0.5(Na0.84K0.16)0.5TiO3 ceramics
    Manotham, Supalak
    Butnoi, Pichitchai
    Jaita, Pharatree
    Tantraviwat, Doldet
    Boothrawong, Narongdetch
    Rujijanagul, Gobwute
    MATERIALS RESEARCH BULLETIN, 2020, 128
  • [22] Structure, electrical properties and depolarization temperature of (Bi0.5Na0.5)TiO3-BaTiO3 lead-free piezoelectric ceramics
    Xu, Chenggang
    Lin, Dunmin
    Kwok, K. W.
    SOLID STATE SCIENCES, 2008, 10 (07) : 934 - 940
  • [23] Phase transition, dielectric and piezoelectric properties of NaNbO3-Bi0.5Li0.5TiO3 lead-free ceramics
    Fu, Lingling
    Lin, Dunmin
    Zheng, Qiaoji
    Wu, Xiaochun
    Wu, Lang
    Sun, Hailing
    Wan, Yang
    Fan, Ximing
    Xu, Chenggang
    CURRENT APPLIED PHYSICS, 2012, 12 (06) : 1523 - 1528
  • [24] Dielectric properties and depolarization temperature of Bi0.5(Na, K)0.5 TiO3-BiFeO3 lead-free ceramics
    Zhou, Qin
    Zhou, Changrong
    Yang, Huabin
    Yuan, Changlai
    Li, Weizhou
    PHYSICA B-CONDENSED MATTER, 2010, 405 (02) : 613 - 618
  • [25] Enhanced piezoelectric, electrocaloric and energy storage properties at high temperature in lead-free Bi0.5(Na1-xKx)0.5TiO3 ceramics
    Wang, Xiangjian
    Gao, Hongcheng
    Hao, Xihong
    Lou, Xiaojie
    CERAMICS INTERNATIONAL, 2019, 45 (04) : 4274 - 4282
  • [26] Enhancement in dielectric and ferroelectric properties of lead free Bi0.5(Na0.5K0.5)0.5TiO3 ceramics by Sb-doping
    Kumar, Krishan
    Singh, B. K.
    Gupta, M. K.
    Sinha, N.
    Kumar, Binay
    CERAMICS INTERNATIONAL, 2011, 37 (08) : 2997 - 3004
  • [27] Ferroelectric Properties of Bi0.5(Na0.8K0.2)0.5TiO3 Ceramics
    Camargo, Javier
    Ramajo, Leandro
    Rubio-Marcos, Fernando
    Castro, Miriam
    ELECTROCERAMICS VI, 2014, 975 : 3 - +
  • [28] Effect of La2O3-Enriched Bi0.5(Na0.68K0.22Li0.1)0.5TiO3 on Properties of (K0.44Na0.52Li0.04)(Nb0.84Ta0.10Sb0.06)O3 Ceramics Prepared by Solid State Combustion
    Kornphom, Chittakorn
    Jutimoosik, Jaru
    Bongkarn, Theerachai
    JOURNAL OF ELECTRONIC MATERIALS, 2019, 48 (06) : 3919 - 3930
  • [29] The effect of annealing temperature on the piezoelectric and dielectric properties of lead-free Bi0.5(Na0.85K0.15)0.5TiO3 thin films
    Won, Sung Sik
    Ahn, Chang Won
    Kim, Ill Won
    JOURNAL OF THE KOREAN PHYSICAL SOCIETY, 2012, 61 (06) : 928 - 932
  • [30] Structure and electrical properties of (Li, Sr, Sb)-modified K0.5Na0.5NbO3 lead-free piezoelectric ceramics
    Hao, Jigong
    Chu, Ruiqing
    Xu, Zhijun
    Zang, Guozhong
    Li, Guorong
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 479 (1-2) : 376 - 380