Structural, microstructure and electrical properties of La2O3-doped Bi0.5(Na0.68K0.22Li0.01)0.5TiO3 lead-free piezoelectric ceramics synthesized by the combustion technique

被引:27
|
作者
Bhupaijit, Pamornnarumol [1 ]
Kornphom, Chittakorn [1 ,2 ]
Vittayakorn, Naratip [3 ]
Bongkarn, Theerachai [1 ,2 ,4 ]
机构
[1] Naresuan Univ, Fac Sci, Dept Phys, Phitsanulok 65000, Thailand
[2] Naresuan Univ, Fac Sci, Res Ctr Acad Excellence Appl Phys, Phitsanulok 65000, Thailand
[3] King Mongkuts Inst Technol Ladkrabang, Fac Sci, Dept Chem, Bangkok 10520, Thailand
[4] Naresuan Univ, Res Ctr Acad Excellence Petr Petrochem & Adv Mat, Phitsanulok 65000, Thailand
关键词
Combustion technique; Perovskite structure; Dielectric; Piezoelectric; Ferroelectric; FERROELECTRIC PROPERTIES;
D O I
10.1016/j.ceramint.2015.03.226
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of firing temperatures on phase formation, microstructure and physical properties of [Bi-0.5(Na0.68K0.22Li0.1)(0.5)TiO3] doped with La2O3 at 0.1 wt% (BNKLLT) ceramics prepared by the combustion method was studied. Glycine was used as fuel and the ratio of raw material (corresponding oxidant metal nitrate) with fuel was about 1:0.56. The samples were calcined at 600-900 degrees C for 2 h and sintered at 1075-1150 degrees C for 2 h. The single rhombohedral peroveskite phase of BNKLLT powders was observed from the sample calcined at 750 degrees C for 2 h. The BNKLLT ceramics exhibited a pure peroveskite phase in all samples. The microstructures of the BNKLLT powders exhibited an agglomerated form while the grain ceramics exhibited a square shape. The average particle size and average grain size increased with increasing firing temperatures. The density, dielectric constant (epsilon(r) and epsilon(m)), P-r and d(33) tended to increase with increasing sintering temperatures up to 1100 degrees C and then decreased. The maximum density (5.73 g/cm(2)), maximum dielectric constant (epsilon(r)similar to 2572 and epsilon(m)similar to 5536), good ferroelectic properties (P-r similar to 35.78 mu C/cm(2) and E-c similar to 22.42 kV/cm) and highest d(33) (210 pC/N) were obtained by the sample sintered at 1100 degrees C for 2 h. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:S81 / S86
页数:6
相关论文
共 50 条
  • [1] Dielectric temperature stability of Nb-modified Bi0.5(Na0.78K0.22)0.5TiO3 lead-free ceramics
    Liu, Yun
    Li, Yuanliang
    Zheng, Zhanshen
    Kang, Wenshuo
    Xi, Kaibiao
    Mi, Yueshan
    CERAMICS INTERNATIONAL, 2021, 47 (04) : 4933 - 4936
  • [2] Microstructural and Ferroelectric Properties of Bi0.5(Na,K)0.5TiO3-Based Modified by Bi0.5Li0.5TiO3 Lead-Free Piezoelectric Ceramics
    Dung, D. D.
    Thiet, D. V.
    Quyet, N. V.
    Bac, L. H.
    Cho, S.
    MATERIALS TRANSACTIONS, 2015, 56 (09) : 1378 - 1382
  • [3] Phase transition and electrical characteristics of Bi0.5(Na0.78K0.22)0.5 TiO3-BiFeO3 lead-free piezoelectric ceramics
    Lee, Ku-Tak
    Park, Jung-Soo
    Cho, Jeong-Ho
    Jeong, Young-Hun
    Paik, Jong-Hoo
    Yun, Ji Sun
    CERAMICS INTERNATIONAL, 2015, 41 (08) : 10298 - 10303
  • [4] Effect of Co2+ substitution in B-sites of the perovskite system on the phase formation, microstructure, electrical and magnetic properties of Bi0.5(Na0.68K0.22Li0.10)0.5TiO3 ceramics
    Bhupaijit, Pamornnarumol
    Kaewsai, Chonnarong
    Suriwong, Tawat
    Pinitsoontorn, Supree
    Yotthuan, Surirat
    Vittayakorn, Naratip
    Bongkarn, Theerachai
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2022, 29 (09) : 1798 - 1808
  • [5] Dielectric and piezoelectric characteristics of lead-free Bi0.5(Na0.84K0.16)0.5TiO3 ceramics substituted with Sr
    Yoo, JY
    Oh, DG
    Jeong, Y
    Hong, J
    Jung, MY
    MATERIALS LETTERS, 2004, 58 (29) : 3831 - 3835
  • [6] Effect of Bi0.5(Na0.9K0.1)0.5TiO3 on Phase Structure and Electrical Properties of (K0.5Na0.5)NbO3 Lead-free Ceramics
    Huang, Tao
    Xiao, Ding-Quan
    Liang, Wen-Feng
    Wu, Jia-Gang
    Zhu, Jian-Guo
    FERROELECTRICS, 2014, 458 (01) : 194 - 199
  • [7] Preparation and electrical properties of Bi0.5Na0.5TiO3-BaTiO3-KNbO3 lead-free piezoelectric ceramics
    Ni, Haimin
    Luo, Laihui
    Li, Weiping
    Zhu, Yuejin
    Luo, Haosu
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (09) : 3958 - 3962
  • [8] Dielectric and piezoelectric properties of Bi0.5Na0.5TiO3-Bi0.5K0.5TiO3-BiCrO3 lead-free piezoelectric ceramics
    Zhou, Changrong
    Liu, Xinyu
    Li, Weizhou
    Yuan, Changlai
    JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 478 (1-2) : 381 - 385
  • [9] Effect of potassium concentration on the structure and electrical properties of lead-free Bi0.5 (Na,K)0.5 TiO3-BiAlO3 piezoelectric ceramics
    Ullah, Aman
    Ahn, Chang Won
    Hussain, Ali
    Lee, Sun Young
    Kim, Jin Soo
    Kim, Ill Won
    JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (06) : 3148 - 3154
  • [10] Effect of Co2+ substitution in B-sites of the perovskite system on the phase formation, microstructure, electrical and magnetic properties of Bi0.5(Na0.68K0.22Li0.10)0.5TiO3 ceramics
    Pamornnarumol Bhupaijit
    Chonnarong Kaewsai
    Tawat Suriwong
    Supree Pinitsoontorn
    Surirat Yotthuan
    Naratip Vittayakorn
    Theerachai Bongkarn
    International Journal of Minerals, Metallurgy and Materials, 2022, 29 : 1798 - 1808