Effect of the section size, holding temperature and time on the kinetics of the ausferritic transformation and mechanical properties of as-cast ausferritic ductile iron

被引:6
作者
de la Torre, Urko [1 ]
Gonzalez-Martinez, Rodolfo [1 ]
Mendez, Susana [1 ]
机构
[1] Basque Res & Technol Alliance BRTA, AZTERLAN, Aliendalde Auzunea 6, E-48200 Durango, Bizkaia, Spain
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 788卷
关键词
Ductile iron; Ausferrite; As-cast; ADI; Section size; Engineered cooling; AUSTEMPERING TEMPERATURES; MICROSTRUCTURE; SOLIDIFICATION; TOUGHNESS; STRENGTH; FATIGUE; MODEL; BAINITE;
D O I
10.1016/j.msea.2020.139536
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The present research work studies the effect of section size, holding temperature and time on the microstructure and mechanical properties of as-cast ausferritic ductile iron. To that aim, Y block standard samples of 12.5 and 25.0 mm thickness were produced through a controlled cooling process. The holding temperatures of 300 degrees C and 400 degrees C were studied. The transformation time was changed in the range of 10-180 min. Furthermore, interrupted cooling experiments on the temperature range of 550 degrees C to 300 degrees C were performed to reveal the ausferritic nose. The experimental results indicated that for a holding temperature of 300 degrees C, an effect of the section size is noticed due to the cooling rate differences before the temperature arrest, while for a holding temperature of 400 degrees C no significant change on the microstructure evolution was observed. Besides, at the studied temperatures of 300 degrees C and 400 degrees C, and holding times of 80 and 65 min, respectively, after the beginning of the ausferritic reaction, the microstructure and the mechanical properties remained constant. The low cooling rate (air cooling) from the early shake out, to the temperature arrest, allowed the formation of some upper acicular ferrite during the cooling process from the ausferrite formation start temperature (defined for the considered alloy around 550 degrees C) down to the holding temperature, even for low temperatures (300 degrees C).
引用
收藏
页数:9
相关论文
共 45 条
[41]  
Tiryakioglu M., 1997, Int. J. Cast Met. Res, V9, P259, DOI DOI 10.1080/13640461.1997.11819667
[42]   Influence of tempering on the mechanical properties of austempered ductile iron [J].
Wen, DC ;
Lei, TS .
MATERIALS TRANSACTIONS JIM, 1999, 40 (09) :980-988
[43]   Model for the maximum fraction of retained austenite in austempered ductile cast iron [J].
Yescas, MA ;
Bhadeshia, HKDH .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2002, 333 (1-2) :60-66
[44]  
Yu K.O., 2001, MODELING CASTING SOL, DOI [10.1201/9781482277333, DOI 10.1201/9781482277333.]
[45]   Microstructure and mechanical properties of austempered ductile iron with different strength grades [J].
Zhang, Jiwang ;
Zhang, Ning ;
Zhang, Mintang ;
Lu, Liantao ;
Zeng, Dongfang ;
Song, Qingpeng .
MATERIALS LETTERS, 2014, 119 :47-50