Thermal Aging Effects on the Mechanical Behavior of Glass-Fiber-Reinforced Polyphenylene Sulfide Composites

被引:12
|
作者
Deng, Jiangang [1 ,2 ]
Song, You [1 ,2 ]
Xu, Zhuolin [1 ,2 ]
Nie, Yu [1 ,2 ]
Lan, Zhenbo [1 ,2 ]
机构
[1] State Grid Elect Power Res Inst, Wuhan Nari Ltd Liabil Co, Wuhan 430074, Peoples R China
[2] State Grid Elect Power Res Inst, Nanjing 210000, Peoples R China
关键词
GF; PPS; thermal aging; mechanical property; color difference; POLY(PHENYLENE SULFIDE); CRYSTALLIZATION; PERFORMANCE; MEMBRANE;
D O I
10.3390/polym14071275
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this article, the thermal aging behavior of polyphenylene sulfide (PPS) composites, reinforced by 20% glass fibers (GFs), in thermal aging temperatures ranging from 85 to 145 degrees C was studied. Tensile and bending properties and color changes in the thermally aged samples were investigated. The results showed that thermal aging at this temperature range resulted in the degradation of mechanical properties. Both the tensile and flexural strength of the GF/PPS composites were significantly reduced after thermal aging at 145 degrees C. Decreased strength and brittle fracture were observed because thermal aging at high temperatures resulted in the deterioration of the interfaces between the GFs and PPS matrix. The degradation of the mechanical properties of the composite samples can be reflected by the color change, which means that the mechanical properties of the GF/PPS composite samples under thermal aging are predictable using color change analysis.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] An Experimental Investigation into Mechanical and Thermal Properties of Hybrid Woven Rattan/Glass-Fiber-Reinforced Epoxy Composites
    Irawan, Agustinus Purna
    Anggarina, Paula Tjatoerwidya
    Utama, Didi Widya
    Najid, Najid
    Abdullah, Mohd Zulkfly
    Siregar, Januar Parlaungan
    Cionita, Tezara
    Fitriyana, Deni Fajar
    Jaafar, Jamiluddin
    Hadi, Agung Efriyo
    Rihayat, Teuku
    POLYMERS, 2022, 14 (24)
  • [22] Investigations of three-dimensional fiber orientation on mechanical impact behavior of short glass-fiber-reinforced PEEK composites
    Ge, Yuzhou
    Zhan, Zhangjie
    Wu, Wanxia
    Zhao, Jian
    Roman, Allen Jonathan
    Gim, Jinsu
    Su, Dongxiao
    Zuo, Xiubin
    Turng, Lih-Sheng
    Osswald, Tim A.
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2024,
  • [23] AGING OF GLASS-FIBER-REINFORCED PEI IN SALINE ATMOSPHERE
    VINA, J
    SANCHEZ, A
    LAMELA, MJ
    BELZUNCE, FJ
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1994, 13 (24) : 1778 - 1779
  • [24] Flow behavior of glass-fiber-reinforced thermoplastics
    Edelmann, K
    Neitzel, M
    KUNSTSTOFFE-PLAST EUROPE, 1997, 87 (12): : 1796 - +
  • [25] Viscoelastic Behavior of Glass-Fiber-Reinforced Silicone Composites Exposed to Cyclic Loading
    Beter, Julia
    Schrittesser, Bernd
    Lechner, Bernhard
    Mansouri, Mohammad Reza
    Marano, Claudia
    Fuchs, Peter Filipp
    Pinter, Gerald
    POLYMERS, 2020, 12 (09)
  • [26] LONGITUDINAL COMPRESSION STRENGTH OF GLASS-FIBER-REINFORCED COMPOSITES
    KIM, RY
    CRASTO, AS
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1994, 13 (04) : 326 - 338
  • [27] Numerical failure analysis of glass-fiber-reinforced composites
    Tanimoto, Y
    Nishiwaki, T
    Nemoto, K
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2004, 68A (01): : 107 - 113
  • [28] Influence of annealing on the performance of short glass fiber-reinforced polyphenylene sulfide (PPS) composites
    Arici, A
    Sinmazçelik, T
    Çapan, L
    Yilgör, I
    Yilgör, E
    JOURNAL OF COMPOSITE MATERIALS, 2005, 39 (01) : 21 - 33
  • [29] Environmental fatigue of pultruded glass-fiber-reinforced composites
    Liao, K
    Schultheisz, CR
    Hunston, DL
    Brinson, LC
    COMPOSITE MATERIALS: FATIGUE AND FRACTURE, SEVENTH VOLUME, 1998, 1330 : 217 - 234
  • [30] GLASS-FIBER-REINFORCED COMPOSITES IN BUILDING CONSTRUCTION.
    Green, Andrew
    Transportation Research Record, 1987, : 73 - 76