Mechanical and Physical Properties of Differently Alloyed Sintered Steels as a Function of the Sintering Temperature

被引:7
|
作者
Hojati, Milad [1 ]
Danninger, Herbert [1 ]
Gierl-Mayer, Christian [1 ]
机构
[1] Vienna Univ Technol, Inst Chem Technol & Analyt, A-1060 Vienna, Austria
关键词
powder metallurgy; iron-manganese masteralloy; sintering; Astaloy CrM; mechanical properties; physical properties; MAGNETIC-PROPERTIES; FE-CU; ELECTRICAL-CONDUCTIVITY; FERROUS MATERIALS; IRON; MICROSTRUCTURE; COPPER; COMPACTS; BEHAVIOR;
D O I
10.3390/met12010013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, the effect of processes occurring during the sintering of four powder metallurgy steel grades on the resulting properties were investigated. This included three grades prepared from plain iron powder with admixed graphite, one grade alloyed also with elemental copper and another with Fe-Mn-Si masteralloy. One further grade was prepared from Cr-Mo pre-alloyed powder with admixed graphite. The effect of the sintering processes was examined in the temperature range of 700-1300 degrees C in an inert atmosphere (Ar). In order to study oxygen removal, DTA/TG runs linked with mass spectrometry (MS) as well as C/O elemental analysis were performed. Charpy impact tests and fractography studies were performed to study the effect of the temperature on the formation and growth of sintering contacts. Characterization also included metallography, dimensional change, sintered density, and hardness measurements to describe the dissolution of carbon and alloying elements during the process. Physical properties that were measured were electrical conductivity and coercive force. The results showed that, in all steels, the reduction of oxides that occur during the heating stage plays a key role in the formation and growth of the sintering contacts as well as in the completion of alloying processes. In the chromium alloy steel, the presence of the stable chromium oxides delays these processes up to higher temperatures, while in the other steels that are based on plain iron powder, these processes take place earlier in the heating stage, at lower temperatures. Compared to the standard Fe-C and Fe-Cu-C grades, the Cr-Mo steel requires more sophisticated sintering to ensure oxygen removal, but on the other hand it offers the best properties. The masteralloy variant, finally, can be regarded as a highly attractive compromise between manufacturing requirements, alloy element content, and product properties.
引用
收藏
页数:19
相关论文
共 50 条
  • [1] Dependence of the mechanical properties of sintered hydroxyapatite on the sintering temperature
    Prokopiev, Oleg
    Sevostianov, Igor
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 431 (1-2): : 218 - 227
  • [2] Sintering and mechanical properties of mechanically alloyed Fe-Al-(B) nanostructures
    Izadi, S.
    Akbari, G. H.
    Janghorban, K.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 496 (1-2) : 699 - 702
  • [3] Effect of sintering temperature on microstructures and mechanical properties of spark plasma sintered nanocrystalline aluminum
    Liu, Zhen-Feng
    Zhang, Zhao-Hui
    Lu, Ji-Fang
    Korznikov, Alexander V.
    Korznikova, Elena
    Wang, Fu-Chi
    MATERIALS & DESIGN, 2014, 64 : 625 - 630
  • [4] Bonding Evolution with Sintering Temperature in Low Alloyed Steels with Chromium
    Fuentes-Pacheco, L.
    Campos, M.
    SCIENCE OF SINTERING, 2009, 41 (02) : 161 - 173
  • [5] Effects of sintering temperature on microstructure and mechanical properties of spark plasma sintered titanium
    Asl, Mehdi Shahedi
    Namini, Abbas Sabahi
    Motallebzadeh, Amir
    Azadbeh, Maziyar
    MATERIALS CHEMISTRY AND PHYSICS, 2018, 203 : 266 - 273
  • [6] The effect of lanthanum boride on the sintering, sintered microstructure and mechanical properties of titanium and titanium alloys
    Yang, Y. F.
    Luo, S. D.
    Qian, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 618 : 447 - 455
  • [7] The Effect of the Sintering Temperature and Addition of Niobium and Vanadium on the Microstructure and Mechanical Properties of Microalloyed PM Steels
    Erden, Mehmet Akif
    METALS, 2017, 7 (09)
  • [8] Mechanism for Improving the Mechanical Properties of Sintered Iron–Copper Composites Alloyed with Molybdenum
    V. V. Skorokhod
    O. I. Getman
    V. V. Panichkina
    P. Ya. Radchenko
    O. I. Bykov
    A. V. Samelyuk
    Powder Metallurgy and Metal Ceramics, 2017, 56 : 370 - 378
  • [9] Titanium Powder Sintering in a Graphite Furnace and Mechanical Properties of Sintered Parts
    Yu, Changzhou
    Cao, Peng
    Jones, Mark Ian
    METALS, 2017, 7 (02):
  • [10] Effect of Sintering Temperature on the Mechanical Properties of Vacuum Sintered Co-(Zn)-Ni-Al Alloys
    Arputhavalli, G. Johnsy
    Agilani, S.
    Jebasingh, S.
    Joseph, S. Vijay
    SCIENCE OF SINTERING, 2020, 52 (03) : 329 - 338