Influence of FSP Parameters on Wear and Microstructural Characterization of Dissimilar TIG Welded Joints with Si-rich Filler Metal

被引:27
作者
Hashmi, Abdul Wahab [1 ]
Mehdi, Husain [2 ]
Mabuwa, Sipokazi [3 ]
Msomi, Velaphi [3 ]
Mohapatra, Prabhujit [4 ]
机构
[1] MNIT Jaipur, Dept Mech Engn, Adv Mfg & Mechatron Lab, Jaipur, Rajasthan, India
[2] Delhi Technol Univ, Dept Mech Engn, Delhi, India
[3] Cape Peninsula Univ Technol, Mech Engn Dept, POB 1906, ZA-7535 Bellville, South Africa
[4] VIT Univ, Sch Adv Sci, Vellore, Tamil Nadu, India
关键词
Friction stir processing; Microstructure; Microhardness; Tensile strength; ALUMINUM-ALLOY JOINTS; GAS TUNGSTEN ARC; MECHANICAL-PROPERTIES; MG ALLOYS; FRICTION; BEHAVIOR; EVOLUTION; TEMPERATURE; FABRICATION; AZ31B;
D O I
10.1007/s12633-022-01848-8
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The welding process is used to join similar or dissimilar alloys, resulting in severe joint softening, uneven grain structure, and inevitable deficiencies. The friction stir process (FSP) can reduce the grain size and enhance the tensile properties. In this work, the FSP was applied to Si-rich TIG welded joints to enhance the tensile properties and microstructure of the TIG-welded joints by variation of rotational tool speed (TRS), and it was observed that the TIG welding defects (solidification defects, micro-voids, porosity, coarse grain structure) were removed, and the grain size of the TIG weldment was decreased. The coarse eutectic Al13Fe4 and Mg2Si phases were transformed into very small phases in the TIG + FSPed joints. The homogenization of the primary alpha-Al exists in the TIG welded joints was continuously enhanced as the TRS increased. The processed zone with high TRS (1100 rpm) demonstrated higher tensile strength (102.76 MPa), whereas the TIG weldment using filler ER4043 was employed to have an average tensile strength of 72.14 MPa. The ultrafine grain structure of 5.14 mu m was found in the TIG + FSPed weldment with a TRS of 1100 rpm, while the coarse grain size of 20.85 mu m was found in the TIG weldment.
引用
收藏
页码:11131 / 11145
页数:15
相关论文
共 72 条
  • [1] Effect of Through-Thickness Friction Stir Processing Parameters on Weld Repair and Modification of Fusion-Welded AA6061 Aluminum Alloy
    Aliakbari, Saeed
    Ketabchi, Mostafa
    Mirsalehi, Seyyed Ehsan
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (05) : 2688 - 2696
  • [2] Friction stir welding of AA2024-T3: development of numerical simulation considering thermal history and heat generation
    Amini, Cyrus
    Hasanifard, Soran
    Zehsaz, Mohammad
    Jerez-Mesa, Ramon
    Antonio Travieso-Rodriguez, J.
    [J]. INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 117 (7-8) : 2481 - 2500
  • [3] Fabrication of in situ Cu/SiC composites using multi-pass friction stir processing: Evaluation of microstructural, porosity, mechanical and electrical behavior
    Barmouz, Mohsen
    Givi, Mohammad Kazem Besharati
    [J]. COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2011, 42 (10) : 1445 - 1453
  • [4] On the role of processing parameters in producing Cu/SiC metal matrix composites via friction stir processing: Investigating microstructure, microhardness, wear and tensile behavior
    Barmouz, Mohsen
    Givi, Mohammad Kazem Besharati
    Seyfi, Javad
    [J]. MATERIALS CHARACTERIZATION, 2011, 62 (01) : 108 - 117
  • [5] BYELI AV, 1992, J PHYS D APPL PHYS, V25, pA292, DOI 10.1088/0022-3727/25/1A/044
  • [6] Arc characteristics of laser-TIG double-side welding
    Chen, Y. B.
    Miao, Y. G.
    Li, L. Q.
    Wu, L.
    [J]. SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2008, 13 (05) : 438 - 444
  • [7] Experimental study on welding characteristics of CO2 laser TIG hybrid welding process
    Chen, Y. B.
    Lei, Z. L.
    Li, L. Q.
    Wu, L.
    [J]. SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2006, 11 (04) : 403 - 411
  • [8] Joint performance of laser-TIG double-side welded 5A06 aluminum alloy
    Chen Yan-bin
    Miao Yu-gang
    Li Li-qun
    Wu Lin
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2009, 19 (01) : 26 - 31
  • [9] Effect of initial base metal temper on microstructure and mechanical properties of friction stir processed A1-7B04 alloy
    Chen, Yu
    Ding, Hua
    Cai, Zhihui
    Zhao, Jingwei
    Li, Jizhong
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 650 : 396 - 403
  • [10] Fatigue behaviour of AA6082-T6 MIG welded butt joints improved by friction stir processing
    da Silva, J.
    Costa, J. M.
    Loureiro, A.
    Ferreira, J. M.
    [J]. MATERIALS & DESIGN, 2013, 51 : 315 - 322