Self-organized (100)-/(001)-preferred orientation in Pb(Zr,Ti)O3 films grown on polycrystalline substrates by metalorganic chemical vapor deposition

被引:14
|
作者
Yokoyama, S [1 ]
Ozeki, T [1 ]
Oikawa, T [1 ]
Funakubo, H [1 ]
机构
[1] Tokyo Inst Technol, Dept Innovat & Engineered Mat, Midori Ku, Yokohama, Kanagawa 2268502, Japan
关键词
PZT; MOCVD; deposition rate; orientation; self-organized growth;
D O I
10.1080/10584580390259885
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Lead zirconate titanate [Pb(Zr-x Ti1-x)O-3 , PZT] films were grown on (100), (110) and (111)SrRuO3 //SrTiO3 substrates at 600degreesC by metalorganic chemical vapor deposition (MOCVD). The crystal orientation dependence of the growth rate was investigated for these films. The growth rate of (100)-/(001)-oriented epitaxial films was approximately 1.7 and 2.0 times higher than that of (110)-/(101)- and (111)-/(11 (1) over bar)-oriented epitaxial films, respectively. On the other hand, the growth rate of (100)-/(001)-preferred oriented PZT films grown on (111)Pt/TiO2 /SiO2 /(100)Si substrates was almost the same with that of (100)-/(001)-oriented epitaxial films. The deposition rate of these films was approximately 1.5 mum/h. High growth rate of (100)-/(001)-oriented PZT grains makes (100)-/(001)-preferred orientation on (111)Pt/TiO2 /SiO2 /(100)Si substrate. From transmission electron microscopy observation, (100)-/(001)-oriented grains were found to be directly grown on (111)-oriented Pt grains without obvious another oriented grains. As a result, orientation-controlled PZT films were successfully grown on (100)Si substrates having (111)-oriented Pt bottom electrodes.
引用
收藏
页码:1429 / 1436
页数:8
相关论文
共 50 条
  • [42] Highly textured Pb(Zr0.3Ti0.7)O3 thin films on GaN/sapphire by metalorganic chemical vapor deposition
    Dey S.K.
    Cao W.
    Bhaskar S.
    Li J.
    J Mater Res, 2006, 6 (1526-1531): : 1526 - 1531
  • [43] Effect of substrate temperature on electrical characteristics of (Pb, La)(Zr, Ti)O3 ultrathin films deposited by metalorganic chemical vapor deposition
    Chubu Univ, Aichi, Japan
    Jpn J Appl Phys Part 1 Regul Pap Short Note Rev Pap, 9 B (5086-5090):
  • [44] RuO2 bottom electrodes for ferroelectric (Pb, La)(Zr, Ti)O3 thin films by metalorganic chemical vapor deposition
    Chubu Univ, Aichi, Japan
    Jpn J Appl Phys Part 1 Regul Pap Short Note Rev Pap, 8 A (4104-4107):
  • [45] Influence of the purity of source precursors on the electrical properties of Pb(Zr,Ti)O3 thin films prepared by metalorganic chemical vapor deposition
    Fujisawa, H
    Yoshida, M
    Shimizu, M
    Niu, H
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1998, 37 (9B): : 5132 - 5136
  • [46] METALORGANIC CHEMICAL-VAPOR-DEPOSITION OF FERROELECTRIC PB(ZR,TI)O-3 THIN-FILMS
    SHIOSAKI, T
    SHIMIZU, M
    INTEGRATED FERROELECTRICS, 1995, 9 (1-3) : 13 - 20
  • [47] Crystal orientation of GaN films grown on (001)GaAs substrates by plasma-assisted metalorganic chemical vapor deposition
    Sato, M
    SILICON CARBIDE AND RELATED MATERIALS 1995, 1996, 142 : 875 - 878
  • [48] Preparation and structural analysis of micro-patterned Pb(Zr,Ti)O3 film by metalorganic chemical vapor deposition
    Yokoyama, Shintaro
    Takahashi, Kenji
    Okamoto, Shoji
    Nagai, Atsushi
    Minamidate, Jun
    Saito, Keisuke
    Ohashi, Naoki
    Haneda, Hajime
    Sakata, Osami
    Kimura, Shigeru
    Nishida, Ken
    Katoda, Takashi
    Funakubo, Hiroshi
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2006, 45 (6A): : 5102 - 5106
  • [49] Thin film growth of Pb(Zr, Ti)O3 by photoenhanced metalorganic chemical vapor deposition using NO2
    Shimizu, Masaru
    Katayama, Takuma
    Sugiyama, Masataka
    Shiosaki, Tadashi
    1600, (32):
  • [50] Microwave dielectric properties for (Pb,La)(Zr,Ti)O3 thin films on MgO (001) substrate grown by chemical solution deposition
    Moon, SE
    Kwak, MH
    Kim, YT
    Ryu, HC
    Lee, SJ
    Kang, KY
    INTEGRATED FERROELECTRICS, 2005, 77 : 37 - 44