Aging of plasma-deposited carbon layers: effect of their thickness and material structure

被引:10
|
作者
Clergereaux, R [1 ]
Escaich, D
Martin, S
Gaillard, F
Raynaud, P
机构
[1] LGET, Toulouse, France
[2] CEA, LITEN, Grenoble, France
关键词
carbon layer; plasma deposition; structural properties; aging;
D O I
10.1016/j.tsf.2004.11.148
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Carbon layers are frequently deposited by plasma-enhanced chemical vapor deposition (PE-CVD). This technology is very promising because of its highly efficient control of film quality, easy integration in current microelectronic technologies, low cost, high efficiency, and reproducibility. Here, we report a study on carbon layer aging under different conditions: photochemical, 400 K in air or N-2 atmosphere, O-2, H2O, and NaCl. We focus specifically on infrared (Fourier transform infrared, or FTIR) and spectroscopic ellipsometry (SE) analyses. Thin films were deposited in a capacitively coupled radiofrequency (RF) plasma in CH4. Six different plasma conditions were used: three different RF plasma powers (20, 80, and 150 W) used on both electrodes [on the polarized one (cathode) and on the floating one (anode)]. Furthermore, films with three different thicknesses (10, 100, and 1000 nm) were deposited. First of all, an interface of about 50 nm on the anode and of about 200 nm on the cathode at 20 W increasing with the RF plasma power appears at the interface between the substrate and the film. Next, the film composition in the ternary diagram Csp(2)-cdp(3)-H shows that thicker films deposited on the anode are rather apparently polymer-like, in contrast with the ones deposited on the cathode, which are rather graphite-like (a-CH double right arrow a-C). Moreover, these films show different aging mechanisms in air. This paper will thus concentrate on the study of the aging mechanisms based on the comparison of films that underwent aging under different conditions. In the case of polymer-like films, aging mechanisms are attributed to oxidation. In contrast, for the films formed at the cathode, these phenomena are attributed to film oxidation and hydrolysis. As aging leads to modifications in electrical and optical properties, a method to avoid these causes is suggested. (c) 2004 Elsevier B.V All rights reserved.
引用
收藏
页码:216 / 220
页数:5
相关论文
共 50 条
  • [21] Structure of Plasma-Deposited Poly(acrylic acid) Films
    Fahmy, Alaa
    Mix, Renate
    Schoenhals, Andreas
    Friedrich, Joerg F.
    PLASMA PROCESSES AND POLYMERS, 2011, 8 (02) : 147 - 159
  • [22] EVIDENCE OF HEXAGONAL DIAMOND IN PLASMA-DEPOSITED CARBON-FILMS
    SILVA, SRP
    AMARATUNGA, GAJ
    SALJE, EKH
    KNOWLES, KM
    JOURNAL OF MATERIALS SCIENCE, 1994, 29 (19) : 4962 - 4966
  • [23] In situ crystallization kinetics studies of plasma-deposited, hydrogenated amorphous silicon layers
    Sharma, K.
    Verheijen, M. A.
    van de Sanden, M. C. M.
    Creatore, M.
    JOURNAL OF APPLIED PHYSICS, 2012, 111 (03)
  • [24] Thickness dependence of properties of plasma-deposited amorphous SiO2 films
    He, L.-N., 1600, Japan Society of Applied Physics (40):
  • [25] ELECTRONIC STRUCTURE STUDIES OF PLASMA-DEPOSITED AMORPHOUS SILICON.
    Drevillon, B.
    Senemaud, C.
    Cardinaud, C.
    Driss Khodja, M.
    Codet, C.
    Philosophical Magazine B: Physics of Condensed Matter; Electronic, Optical and Magnetic Properties, 1986, 54 (05): : 335 - 342
  • [26] THE NEUTRALIZATION OF SODIUM-IONS IN PLASMA-DEPOSITED SIO2 LAYERS
    GEORGIEV, SS
    THIN SOLID FILMS, 1984, 121 (04) : 271 - 277
  • [27] Thickness dependence of properties of plasma-deposited amorphous SiO2 films
    He, LN
    Hasegawa, S
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2001, 40 (07): : 4672 - 4676
  • [28] Adhesion of plasma-deposited silicon oxide barrier layers on PDMS containing polypropylene
    Hoppe, C.
    Mitschker, F.
    Awakowicz, P.
    Kirchheim, D.
    Dahlmann, R.
    de los Arcos, T.
    Grundmeier, G.
    SURFACE & COATINGS TECHNOLOGY, 2018, 335 : 25 - 31
  • [29] THE COMPATIBILITY OF ALUMINUM LAYERS ON PLASMA-DEPOSITED W AND WSI2 FILMS
    FANG, YK
    YANG, HM
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 1988, 35 (05) : 706 - 708
  • [30] Physicochemical and mechanical properties of plasma-deposited cermet coatings with a NiMo matrix and a reinforcing phase of a nanodimensional carbon material
    Kalita V.I.
    Komlev D.I.
    Nozhkina A.V.
    Inorganic Materials: Applied Research, 2014, 5 (3) : 250 - 254