Effect of Fe additions on microstructure and mechanical properties of a multi-component Nb-16Si-22Ti-2Hf-2Al-2Cr alloy at room and high temperatures

被引:29
|
作者
Zhang, S. M. [1 ]
Zhou, J. R. [1 ]
Sha, J. B. [1 ]
机构
[1] Beihang Univ, Sch Mat Sci & Engn, Beijing 100191, Peoples R China
基金
中国国家自然科学基金;
关键词
Intermetallics; (aluminides; silicides); Fracture toughness; Mechanical properties; Casting; Heat treatment; Microstructure; IN-SITU COMPOSITES; SILICIDE-BASED COMPOSITES; FRACTURE-TOUGHNESS; STRENGTH; TI; ENGINES;
D O I
10.1016/j.intermet.2014.10.013
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The phase constitutions, microstructural evolutions, and mechanical properties of Nb-16Si-22Ti-2Hf-2Al-2Cr-xFe alloys (where x = 1, 2, 4, 6 at.%, hereafter referred to as 1Fe, 2Fe, 4Fe and 6Fe alloys, respectively) prepared by arc-melting were investigated. It was observed that the nominal Fe content affected the solidification path of the multi-component alloy. The as-cast 1Fe alloy primarily consisted of a dendritic-like Nb-SS phase and (alpha+gamma)-Nb5Si3 silicide, and the as-cast 2Fe and 4Fe alloys primarily consisted of an Nb-SS phase, (alpha+gamma)-Nb5Si3 silicide and (Fe + Ti)-rich region. In addition to the Nb-SS phase, a multi-component Nb4FeSi silicide was present in the as-cast 6Fe alloy. When heat-treated at 1350 C for 100 h, the 1Fe and 6Fe alloys almost exhibited the same microstructures as the corresponding as-cast samples; for the 2Fe and 4Fe alloys, the (Fe + Ti)-rich region decomposed, and Nb4FeSi silicide formed. The fracture toughness of the as-cast and heat-treated Nb-16Si-22Ti-2Hf-2Al-2Cr-xFe samples monolithically decreased with the nominal Fe contents. It is interesting that at room temperature, the strength of the heat-treated samples was improved by the Fe additions, whereas at 1250 degrees C and above, the strength decreased, suggesting the weakening role of the Nb4FeSi silicide on the high-temperature strength. As the nominal Fe content increased from 1 at% to 6 at.%, for example, the 0.2% yield strength increased from 1675 MPa to 1820 MPa at room temperature; also, the strength decreased from 183 MPa to 78 MPa at 1350 degrees C. (C) 2014 Elsevier Ltd. All rights reserved.
引用
收藏
页码:146 / 155
页数:10
相关论文
共 50 条
  • [41] Microstructure and mechanical properties of directionally solidified and heat treated Nb-14Si-24Ti-2Cr alloy
    Wang, L. G.
    Weng, J. F.
    Guan, K.
    Su, L. F.
    Jia, L. N.
    Zhang, H.
    MATERIALS RESEARCH INNOVATIONS, 2012, 16 (04) : 276 - 280
  • [42] Microstructure and tensile properties of isothermally forged Ni-43Ti-4Al-2Nb-2Hf alloy
    Song, Xiao-Yun
    Li, Yan
    Zhang, Fei
    RARE METALS, 2013, 32 (05) : 475 - 479
  • [43] Effects of microstructure characteristics on the mechanical properties and elastic modulus of a new Ti-6Al-2Nb-2Zr-0.4B alloy
    Yang, Zhijun
    Cao, Junhui
    Yu, Weixin
    Hou, Shusen
    Wang, Guanglong
    Lang, Shaoting
    Ding, Peng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 820
  • [44] Elevated temperature compressive behavior of Nb-22Ti-16Si-7Cr-3Al-3Ta-2Hf alloy with minor Ho addition
    Tian, Y. X.
    Guo, J. T.
    Cheng, G. A.
    Sheng, L. Y.
    Zhou, L. Z.
    He, L. L.
    Ye, H. Q.
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2008, 99 (02) : 228 - 232
  • [45] Sintering behaviour of Nb-16Si-25Ti-8Hf-2Cr-2Al alloy powder fabricated by a hydrogenation-dehydrogenation method
    Park, Ki Beom
    Choi, Jaeho
    Lee, Sung Yong
    Park, Jae-Young
    Na, Tae-Wook
    Choi, Jong-In
    Kang, Jang-Won
    Park, Hyung-Ki
    MATERIALS SCIENCE AND TECHNOLOGY, 2020, 36 (12) : 1372 - 1380
  • [46] Effect of initial microstructure on phase transformation and mechanical properties of Ti-3Al-5Mo-4Cr-2Zr-1Fe alloy
    Zhu, Qisong
    Lu, Bing
    Xue, Jiayu
    Li, Feng
    Feng, Liang
    Chang, Hui
    MATERIALS SCIENCE AND TECHNOLOGY, 2023, 39 (17) : 2921 - 2937
  • [47] The Effect of Heat Treatment on the Microstructure and Mechanical Properties of the Novel Low-Cost Ti-3Al-5Mo-4Cr-2Zr-1Fe Alloy
    Sun, Meng
    Li, Dong
    Guo, Yanhua
    Wang, Ying
    Dong, Yuecheng
    Dan, Zhenhua
    Chang, Hui
    MATERIALS, 2020, 13 (17)
  • [48] Microstructural evolution and oxidation behaviour of Mo-Si-B coatings on an Nb-16Si-22Ti-7Cr-2Al-2Hf alloy at 1250 °C prepared by spark plasma sintering
    Wen, S. H.
    Zhou, C. G.
    Sha, J. B.
    SURFACE & COATINGS TECHNOLOGY, 2018, 352 : 320 - 329
  • [49] Effect of microstructure on fracture characteristics of Ti-6Al-2Sn-2Mo-2Zr-2Cr-Si alloy
    Niinomi, M
    Fukunaga, K
    Tono, G
    Koike, J
    Eylon, D
    Fujishiro, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (01): : 55 - 62
  • [50] EFFECT OF CARBON AND OXYGEN ADDITIONS ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ti-4.3Fe-7.1Cr-3Al ALLOY
    Song, Xiping
    Chen, Long
    Li, Kun
    Chen, Guoliang
    INTERNATIONAL JOURNAL OF MODERN PHYSICS B, 2009, 23 (6-7): : 814 - 820