Corrosion properties of plastically deformed AZ80 magnesium alloy

被引:0
|
作者
Zhang Zhi-min [1 ]
Xu Hong-yan [1 ]
Li Bao-cheng [1 ]
机构
[1] N Univ China, Sch Mat Sci & Engn, Taiyuan 030051, Peoples R China
来源
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA | 2010年 / 20卷
基金
中国国家自然科学基金; 山西省归国人员基金;
关键词
corrosion property; plastic deformation; AZ80 magnesium alloy; MECHANICAL-PROPERTIES; DIE-CAST; MG ALLOY; MICROSTRUCTURE; AZ91D; AZ31; BEHAVIOR; AM60;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
AZ80 magnesium alloys were deformed at 200, 250, 300, 350 and 400 C with different deformation degree of 50%, 75%, 83%, 87% and 90%, respectively. The corrosion properties of different deformed AZ80 samples were studied by galvanic test in 3.5% NaCl solution. The results show that plastic deformation could improve the corrosion resistance of AZ80 alloy; and the corrosion rate of AZ80 deformed at 250 C with the deformation degree of 83% was the lowest, which was 33% of the as-cast AZ80 alloy. Further studies of the microstructure show that the refined grain size and continuously distribution of beta phase around the grain boundary did have a positive effect on the improvement of corrosion resistance of AZ80 alloys. For AZ80 alloys, the smaller the grain size is, the more homogeneous the structure is, and the better the corrosion resistance
引用
收藏
页码:S697 / S702
页数:6
相关论文
共 50 条
  • [41] Effect of Nd-Rich Phases on the Corrosion Behavior of AZ80 Magnesium Alloy in Alkaline Solution
    Zou, Qi
    Le, Qichi
    Chen, Xingrui
    Ban, Chunyan
    Jia, Yonghui
    Guo, Ruizhen
    Wang, An
    JOM, 2021, 73 (12) : 4376 - 4386
  • [42] Effect of aging time on corrosion behavior of as-forged AZ80 magnesium alloy
    Liao, Hui-juan
    Zhou, Xiao-feng
    Li, Hui-zhong
    Deng, Min
    Liang, Xiao-peng
    Liu, Ruo-mei
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2015, 25 (12) : 3921 - 3927
  • [43] The influences of the expansion equal channel angular extrusion operation on the strength and ductility of AZ80 magnesium alloy
    Sepahi-Boroujeni, S.
    Fereshteh-Saniee, F.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 636 : 249 - 253
  • [44] Effect of temperature on the hot deformation behavior of AZ80 magnesium alloy
    Prakash, Paresh
    Toscano, Dwayne
    Shaha, Sugrib Kumar
    Wells, Mary A.
    Jahed, Hamid
    Williams, Bruce W.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 794
  • [45] Influence of aging modes on microstructure and mechanical properties of AZ80 magnesium alloy
    ZHANG Ju-mei1
    2.Department of Materials Science and Engineering
    Xi’an University of Science & Technology
    ChinaFoundry, 2007, (04) : 296 - 299
  • [46] Effects of thermomechanical treatment process on the microstructure and properties of AZ80 magnesium alloy
    Cai, Gangyi
    Huang, Xiaoting
    Deng, Penghui
    MATERIALS SCIENCE AND ENGINEERING, PTS 1-2, 2011, 179-180 : 354 - +
  • [47] Tribological and Electrochemical Corrosion Properties of CNT-Incorporated Plasma Electrolytic Oxidation (PEO) Coatings on AZ80 Magnesium Alloy
    Kara, Rabia
    Zengin, Huseyin
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2022, 35 (07) : 1195 - 1206
  • [48] Eutectic phase strengthening and strain rate sensitivity behavior of AZ80 magnesium alloy
    Ren, Lingbao
    Zhou, Mingyang
    Lu, Tianhui
    Fan, Lingling
    Guo, Yangyang
    Zhang, Yuwenxi
    Boehlert, Carl J.
    Quan, Gaofeng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 770
  • [49] Ultrasonic Effects on Microstructure Evolution and Mechanical Properties of AZ80 Magnesium Alloy
    Xue Hansong
    Li Di
    Yang Gang
    Zhang Dingfei
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (06) : 1401 - 1405
  • [50] Influence of aging modes on microstructure and mechanical properties of AZ80 magnesium alloy
    Zhang Ju-mei
    Jiang Bai-ling
    Wang Zhi-hu
    Yuan Sen
    Nan Hong-qiang
    Luo Hong-bin
    CHINA FOUNDRY, 2007, 4 (04) : 296 - 299