Retarding mechanism of Zn2+ species in geopolymer material using Raman spectroscopy and DFT calculations

被引:5
作者
Chamssine, Fawzi [1 ]
Gasparotto, Luiz H. S. [2 ]
Souza, Miguel Angelo Fonsecade [2 ]
Khalifeh, Mahmoud [1 ]
de Oliveira Freitas, Julio Cezar [2 ]
机构
[1] Univ Stavanger, Fac Sci & Technol, Dept Energy & Petr Engn, N-4036 Stavanger, Norway
[2] Univ Fed Rio Grande do Norte, UFRN, BR-59078970 Natal, Brazil
关键词
ZINC; CARBONATION; FTIR; SLAG;
D O I
10.1038/s41598-022-25552-0
中图分类号
O [数理科学和化学]; P [天文学、地球科学]; Q [生物科学]; N [自然科学总论];
学科分类号
07 ; 0710 ; 09 ;
摘要
Geopolymers are the most promising alternative to Ordinary Portland Cement for oil-well cementing and well abandonment. To that end, the slurry needs a required pumping time ensured by the addition of retarders. Although zinc has been widely known to prolong the setting time of geopolymers, its mechanism of action has yet to be fully elucidated. It is herein hypothesized that zinc ions impede the first stages of silicate oligomerization (Si-O-Al), culminating in longer setting times. Pumping time measurements showed that Zn(NO3)(2) delayed the setting time by 5 h in comparison to the zinc-less sample. DFT calculations revealed Si(OH)(4) to react with [Zn(OH)(4)](2-) via a barrierless transition state, evidencing a kinetic ground for the retardation effect. Additionally, Raman spectroscopy corroborated the DFT results by showing that Q(3) species in the proposed mechanism are formed more rapidly in the presence of zinc ions than in its absence.
引用
收藏
页数:9
相关论文
共 38 条
[21]   Quartz metastability at high pressure: what new can we learn from polarized Raman spectroscopy? [J].
Morana, Marta ;
Mihailova, Boriana ;
Angel, Ross J. ;
Alvaro, Matteo .
PHYSICS AND CHEMISTRY OF MINERALS, 2020, 47 (08)
[22]   Electrokinetic properties which control the coagulation of silicate cement suspensions during early age hydration [J].
Nachbaur, L ;
Nkinamubanzi, PC ;
Nonat, A ;
Mutin, JC .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 1998, 202 (02) :261-268
[23]   Factors affecting line shapes and intensities of Q3 and Q4 Raman bands of Cs silicate glasses [J].
Nesbitt, H. Wayne ;
O'Shaughnessy, Cedrick ;
Henderson, Grant S. ;
Bancroft, G. Michael ;
Neuville, Daniel R. .
CHEMICAL GEOLOGY, 2019, 505 :1-11
[24]   Kinetics of silicate exchange in alkaline aluminosilicate solutions [J].
North, MR ;
Swaddle, TW .
INORGANIC CHEMISTRY, 2000, 39 (12) :2661-2665
[25]  
Oriakhi C. O., 2009, CHEM QUANTITATIVE LA
[26]   LEACHING EFFECTS ON SILICATE POLYMERIZATION - AN FTIR AND SI-29 NMR-STUDY OF LEAD AND ZINC IN PORTLAND-CEMENT [J].
ORTEGO, JD ;
BARROETA, Y ;
CARTLEDGE, FK ;
AKHTER, H .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1991, 25 (06) :1171-1174
[27]   Effect of carbonation on alkali-activated slag paste [J].
Palacios, M. ;
Puertas, F. .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2006, 89 (10) :3211-3221
[28]   Automated exploration of the low-energy chemical space with fast quantum chemical methods [J].
Pracht, Philipp ;
Bohle, Fabian ;
Grimme, Stefan .
PHYSICAL CHEMISTRY CHEMICAL PHYSICS, 2020, 22 (14) :7169-7192
[29]   In situ ATR-FTIR study of the early stages of fly ash geopolymer gel formation [J].
Rees, Catherine A. ;
Provis, John L. ;
Lukey, Grant C. ;
van Deventer, Jannie S. J. .
LANGMUIR, 2007, 23 (17) :9076-9082
[30]  
Rüscher CH, 2010, CERAM ENG SCI PROC, V31, P17