Very high cycle fatigue behaviors of bainite/martensite multiphase steel treated by quenching-partitioning-tempering process

被引:58
作者
Gao, Guhui [1 ]
Zhang, Baoxiang [2 ]
Cheng, Cheng [1 ]
Zhao, Ping [3 ]
Zhang, Han [1 ,4 ]
Bai, Bingzhe [1 ,3 ]
机构
[1] Beijing Jiaotong Univ, Sch Mech Elect & Control Engn, Mat Sci & Engn Res Ctr, Beijing 100044, Peoples R China
[2] GRIKIN Adv Mat Co Ltd, Beijing Gen Res Inst Nonferrous Met, Beijing 102200, Peoples R China
[3] Tsinghua Univ, Sch Mat Sci & Engn, Key Lab Adv Mat, Beijing 100084, Peoples R China
[4] Max Planck Inst Eisenforsch GmbH, Max Planck Str 1, D-40237 Dusseldorf, Germany
基金
中国国家自然科学基金;
关键词
Very high cycle fatigue; Retained austenite; Bainite; Quenching and partitioning; Crack initiation; HIGH-STRENGTH STEELS; CHROMIUM-BEARING STEEL; SUBSURFACE CRACK INITIATION; LONG-LIFE FATIGUE; DUAL-PHASE STEELS; CR-C STEEL; RETAINED AUSTENITE; FRACTURE-TOUGHNESS; STAINLESS-STEEL; INCLUSION SIZE;
D O I
10.1016/j.ijfatigue.2016.06.025
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
A bainite/martensite (B/M) multiphase steel was treated by a novel bainite-based Q-P-T treatment with various process parameters to obtain multiphase microstructure composed of bainite, martensite and different types of retained austenite (nanometer-sized film-like and micrometer-sized blocky retained austenite). We investigate here the effect of retained austenite on the very high cycle fatigue (VHCF) behavior, especially the fatigue crack initiation in VHCF regime. Results show that the non-inclusion induced crack initiation is the main fatigue failure mechanism in the B/M steel with blocky retained austenite. The blocky retained austenite transforms easily to martensite due to local plastic deformation under cyclic loading, which is prone to induce the formation of micro-cracks. In contrast, the film-like retained austenite is beneficial to the VHCF property of B/M steel due to the dislocation absorption and transformation induced plasticity effects. Therefore, the B/M steel with film-like retained austenite exhibits excellent VHCF property, namely, the fatigue limit in VHCF regime reaches 770 MPa while the tensile strength is 1410 MPa. (C) 2016 Elsevier Ltd. All rights reserved.
引用
收藏
页码:203 / 210
页数:8
相关论文
共 41 条
[1]  
Bathias C., 2004, Gigacycle fatigue in mechanical practice
[2]  
Bollenhagen MC, 2010, INT J FATIGUE, V32, P936
[3]   VHCF behaviour of case-hardened specimens made of two grades of steel SAE 5120 differing in microstructure [J].
Bomas, Hubert ;
Burkart, Klaus ;
Zoch, Hans-Werner .
INTERNATIONAL JOURNAL OF FATIGUE, 2014, 60 :63-73
[4]   Fatigue behaviour of duplex stainless steels in the very high cycle regime [J].
Chai, Guocai .
INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (11) :1611-1617
[5]   The formation of subsurface non-defect fatigue crack origins [J].
Chai, Guocai .
INTERNATIONAL JOURNAL OF FATIGUE, 2006, 28 (11) :1533-1539
[6]   Local plasticity exhaustion in a very high cycle fatigue regime [J].
Chai, Guocai ;
Zhou, Nian ;
Ciurea, Sorina ;
Andersson, Marcus ;
Peng, Ru Lin .
SCRIPTA MATERIALIA, 2012, 66 (10) :769-772
[7]   Roles of microstructure in fatigue crack initiation [J].
Chan, Kwai S. .
INTERNATIONAL JOURNAL OF FATIGUE, 2010, 32 (09) :1428-1447
[8]   TENSILE PROPERTIES OF 0.05 TO 0.20 PCT-C TRIP STEELS [J].
CHANANI, GR ;
ZACKAY, VF ;
PARKER, ER .
METALLURGICAL TRANSACTIONS, 1971, 2 (01) :133-&
[9]   A new iteration method for the thermographic determination of fatigue limit in steels [J].
Curà, F ;
Curti, G ;
Sesana, R .
INTERNATIONAL JOURNAL OF FATIGUE, 2005, 27 (04) :453-459
[10]   Effect of microstructure on fatigue behavior of advanced high strength steels produced by quenching and partitioning and the role of retained austenite [J].
de Diego-Calderon, I. ;
Rodriguez-Calvillo, P. ;
Lara, A. ;
Molina-Aldareguia, J. M. ;
Petrov, R. H. ;
De Knijf, D. ;
Sabirov, I. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 641 :215-224