共 50 条
The effect of nucleating agents on physical properties of poly-3-hydroxybutyrate (PHB) and poly-3-hydroxybutyrate-co-3-hydroxyvalerate (PHB-co-HV) produced by Burkholderia cepacia ATCC 17759
被引:27
|作者:
Zhu, Chengjun
[1
]
Nomura, Christopher T.
[2
]
Perrotta, Joseph A.
[1
]
Stipanovic, Arthur J.
[2
]
Nakas, James R.
[1
]
机构:
[1] SUNY Coll Environm Sci & Forestry, Dept Environm & Forest Biol, Syracuse, NY 13210 USA
[2] SUNY Coll Environm Sci & Forestry, Dept Chem, Syracuse, NY 13210 USA
基金:
美国国家科学基金会;
关键词:
Polyhydroxyalkanoates;
Nucleating agents;
Levulinic acid;
Glycerol;
Physical properties;
BIODEGRADABLE PLASTICS;
CRYSTALLIZATION;
POLYHYDROXYALKANOATES;
POLYPROPYLENE;
BIOSYNTHESIS;
FERMENTATION;
ACID;
POLY(BETA-HYDROXYBUTYRATE-CO-BETA-HYDROXYVALERATE);
POLY(3-HYDROXYBUTYRATE-CO-3-HYDROXYVALERATE);
ISODIMORPHISM;
D O I:
10.1016/j.polymertesting.2012.03.004
中图分类号:
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
In the absence of nucleating agents, polyhydroxyalkanoates (PHAs) generally exhibit slow crystallization rates which make them less favorable for injection molding purposes. The copolymer, PHB-co-HV (poly-3-hydroxybutyrate-co-3-hydroxyvalerate), exhibited increased T-c as compared to the homopolymer PHB (poly-3-hydroxybutyrate). Increasing the mol fraction of HV monomer in the PHB-co-HV initially led to a decrease in the T-m of the copolymer from 175.4 degrees C to a minimum of 168.5 degrees C, at 20 mol% of HV and, subsequently, increased in PHB-co-HV copolymers with higher fractions of HV, indicating a typical isodimorphic relationship. Two nucleating agents, heptane dicarboxylic derivative HPN-68L and ULTRATAL (R) 609, were tested to increase the T-c and reduce the time for crystallization necessary for injection molding. HPN-68L decreased the T-decomp of the homopolymer and all copolymers by almost 50 degrees C. However, the use of ULTRATALC (R) 609 as a nucleating agent slightly enhanced the T-decomp and had negligible effect on the T(m)s of all polymers. Also, PHB and PHB-co-HV with 5% (w/w) talc exhibited higher T-c than polymers without ULTRATALC (R) 609. A careful comparison of T-c, T-m and T-decomp, for PHB-co-HV with 20 mol% of HV indicated that this copolymer is the best option for injection molding, with both a high T-decomp and more rapid crystallization. (C) 2012 Elsevier Ltd. All rights reserved.