Comparison investigation of hot corrosion exposed to Na2SO4 salt and oxidation of MoSi2-based coating on Nb alloy at 1000 °C

被引:16
作者
Sun, Le [1 ]
Fu, Qian-Gang [1 ]
Sun, Jia [1 ]
Zhang, Guang-peng [1 ]
机构
[1] Northwestern Polytech Univ, Carbon Carbon Composites Res Ctr, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Hot corrosion; MoSi2-based coating; Oxidation; Basic fluxing; Nb alloy; SI BASED ALLOY; NIOBIUM ALLOY; SODIUM; PROTECTION; RESISTANCE; BEHAVIOR; OXYGEN;
D O I
10.1016/j.surfcoat.2020.125388
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Hot corrosion behavior of MoSi2-based coating on Nb alloy exposed to Na2SO4 salt was investigated by contrast with the oxidation performance at 1000 degrees C for 0.5 h 1 h and 2 h. The phases and microstructures evolutions of the corroded coatings were analyzed by scanning electron microscope (SEM), energy dispersive spectrometer (EDS), X-ray diffraction (XRD) and X-ray photoelectron spectroscopy (XPS). With the oxidation time prolonging, the profile of splats disappeared gradually. After oxidation for 2 h, SiO2 particles were generated on the surface of the coating and the mass loss was 1.59 mg/cm(2), implying that oxidation is a slow degradation process. MoSi2-based coating exhibited a serious corrosion with Na2SO4 salt, forming corroded products such as cristobalite scale and sodium molybdates. With the elongation of corrosion time, the surface morphology of cristobalite layer underwent the transformation from lotus leaves into granules due to basic fluxing of the cristobalite preferentially on the grain boundary. The formed cristobalite scale would spall off due to its loose structure and coefficient of thermal expansion (CTE) mismatch with MoSi2-based coating, leading to a serious mass loss with 2.5 mg/cm(2) after hot corrosion for 2 h.
引用
收藏
页数:12
相关论文
共 35 条
[21]   Hot corrosion phenomena of Nb-Ti-Si based alloy and its silicide coating induced by different corrosive environments at 900 °C [J].
Qiao, Yanqiang ;
Kong, Jianping ;
Guo, Xiping .
CERAMICS INTERNATIONAL, 2018, 44 (07) :7978-7990
[22]   Hot corrosion behavior of silicide coating on an Nb-Ti-Si based ultrahigh temperature alloy [J].
Qiao, Yanqiang ;
Guo, Xiping ;
Li, Xuan .
CORROSION SCIENCE, 2015, 91 :75-85
[23]   Hot corrosion of materials: a fluxing mechanism? [J].
Rapp, RA .
CORROSION SCIENCE, 2002, 44 (02) :209-221
[24]   Oxidation behavior of the B-modified silicide coating on Nb-Si based alloy at intermediate temperatures [J].
Shao, Wei ;
Zhou, Chungen .
CORROSION SCIENCE, 2018, 132 :107-115
[25]   Hot corrosion: a modification of reactants causing degradation [J].
Shifler, David A. .
MATERIALS AT HIGH TEMPERATURES, 2018, 35 (1-3) :225-235
[26]   Hot corrosion of chemical vapour deposited SiC and Si3N4 in molten Na2SO4 salt [J].
Song, DY ;
Kitaoka, S ;
Kawamoto, H .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (04) :1031-1036
[27]   Hot corrosion behaviour of Pt modified aluminized NiCrAlYSi coating on a Ni-based single crystal superalloy [J].
Sun, J. ;
Liu, S. B. ;
Li, W. ;
Yu, H. J. ;
Jiang, S. M. ;
Gong, J. ;
Sun, C. .
CORROSION SCIENCE, 2019, 149 :207-217
[28]   Different oxidation protection mechanisms of HAPC silicide coating on niobium alloy over a large temperature range [J].
Sun, Jia ;
Li, Tao ;
Zhang, Guang-Peng ;
Fu, Qian-Gang .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 790 :1014-1022
[29]   A long-term ultrahigh temperature application of layered silicide coated Nb alloy in air [J].
Sun, Jia ;
Fu, Qian-Gang ;
Li, Tao ;
Wang, Chen ;
Huo, Cai-Xia ;
Zhou, Hong ;
Yang, Guan-Jun ;
Sun, Le .
APPLIED SURFACE SCIENCE, 2018, 439 :1111-1118
[30]   Silicide Coating Fabricated by HAPC/SAPS Combination to Protect Niobium Alloy from Oxidation [J].
Sun, Jia ;
Fu, Qian-Gang ;
Guo, Li-Ping ;
Wang, Lu .
ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (24) :15838-15847