Influence of metallurgical variables on sensitisation kinetics in austenitic stainless steels

被引:73
作者
Dayal, RK [1 ]
Parvathavarthini, N [1 ]
Raj, B [1 ]
机构
[1] Indira Gandhi Ctr Atom Res, Kalpakkam 603102, Tamil Nadu, India
关键词
time-temperature sensitisation diagram; metallurgical variables; sensitisation test methods; low temperature sensitisation; laser surface treatment;
D O I
10.1179/174328005X14348
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Austenitic stainless steels are the most favoured construction materials for various components required in chemical, petrochemical, fertiliser and nuclear industries. However, these steels are prone to sensitisation. In the sensitised condition, the steels are quite susceptible to intergranular corrosion and intergranular stress corrosion cracking in chloride and caustic environments resulting in the premature failure of the fabricated components during p recommissioning and service periods. The topic of sensitisation has been of interest in studies worldwide. The studies included mechanism of sensitisation, test methods, data generation, and influence of several variables and protection methods. This article covers a review of important contributions to this topic with special emphasis on the influence of metallurgical variables. The present state of understanding is discussed in the following areas: mechanisms, test methods, sensitisation diagrams, influence of chemical composition, cold work and grain size, low temperature sensitisation, modelling and laser surface treatment. The need for further investigation in certain areas is highlighted.
引用
收藏
页码:129 / 155
页数:27
相关论文
共 181 条
[91]  
KOSO M, 1989, SUOMITOMO MET, V41, P47
[92]  
LABARBERA A, 1987, C LAS TREATM MAT BAD, P179
[93]  
LEE CH, 1992, J KOREAN I METALS MA, V30, P43
[94]   Influence of Si content on the intergranular corrosion of SUS 309L stainless steels [J].
Lin, DY ;
Chang, TC .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 359 (1-2) :396-401
[95]  
LJUNGBERG L, 1982, INT LTS WORKSH PAL A
[96]  
LORIA EA, 1986, J TEST EVAL, V14, P81, DOI 10.1520/JTE10326J
[97]   PERSPECTIVE ON INTERGRANULAR CORROSION OF TYPE-304 STAINLESS-STEEL [J].
LORIA, EA .
JOURNAL OF METALS, 1982, 34 (10) :16-22
[98]  
LORIA EA, 1978, J MET, V31, P163
[99]   THE EFFECT OF METHODS OF CUTTING AND GRINDING ON SENSITIZATION IN SURFACE-LAYERS ON AISI-304 STAINLESS-STEEL [J].
MAJIDI, AP ;
STREICHER, MA .
CORROSION, 1984, 40 (09) :445-458
[100]   4 NONDESTRUCTIVE ELECTROCHEMICAL TESTS FOR DETECTING SENSITIZATION IN TYPE-304 AND TYPE-304L STAINLESS-STEELS [J].
MAJIDI, AP ;
STREICHER, MA .
NUCLEAR TECHNOLOGY, 1986, 75 (03) :356-369