Measuring the residual stress in dental composites using a ring slitting method

被引:41
作者
Park, JW
Ferracane, JL
机构
[1] Kyungpook Natl Univ, Sch Dent, Dept Conservat Dent, Taegu 700422, South Korea
[2] Oregon Hlth & Sci Univ, Dept Restorat Dent, Div Biomat & Biomech, Portland, OR 97201 USA
关键词
residual stress; ring slitting method; dental composite; elastic modulus; degree of conversion;
D O I
10.1016/j.dental.2005.03.006
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The objective of this experiment was to employ the ring slitting method for the measurement of the residual stress (RS) produced in dental composite materials after polymerization. This study was designed to determine the effect of slitting and measuring time on the residual stress. Methods. Rings were made in a split brass mold from three composites (Z100/3MESPE; Herculite/Kerr; Heliomolar/Ivoclar) and cured in a Triad 11 (Dentspty). Two points were scribed, and the rings were slit at either I h (Early-group) or 24 h (Delayed-group) after curing the composite. The change in the distance between the scribed points was measured using an image analyzer system at both 1 and 24 h after slitting. From the measured change, circumferential RS was calculated and statistically analyzed with ANOVA/Tukey's (P < 0.05). The degree of conversion of each composite at 1 and 24 h-was measured with FTIR and analyzed using Student's t-test (P < 0.05). Results. In general, the residual stress (range= 0.42-2.84 MPa) was highest for Z100 and lowest for Heliomolar, but this depended upon the test conditions. The early cut (1 h slitting), 24 h measurement groups showed the highest residual stress values. Significance. This study, describes a ring slitting method to measure residual stress generated in dental composites during and. after curing. The stress of composite can be affected by the cutting and measurement time. (c) 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:882 / 889
页数:8
相关论文
共 37 条
[31]   SYNTHESIS AND EVALUATION OF NEW OXASPIRO MONOMERS FOR DOUBLE RING-OPENING POLYMERIZATION [J].
STANSBURY, JW .
JOURNAL OF DENTAL RESEARCH, 1992, 71 (07) :1408-1412
[32]   Post-irradiation polymerization of composites containing bis-GMA and TEGDMA [J].
Tarumi, H ;
Imazato, S ;
Ehara, A ;
Kato, S ;
Ebi, N ;
Ebisu, S .
DENTAL MATERIALS, 1999, 15 (04) :238-242
[33]   Influence of residual stresses on the wear behavior of alumina/alumina-zirconia laminated composites [J].
Toschi, F ;
Melandri, C ;
Pinasco, P ;
Roncari, E ;
Guicciardi, S ;
de Portu, G .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2003, 86 (09) :1547-1553
[34]   Influence of residual stress on the relationship between pipe pressure and C-ring tests [J].
Whittle, AJ ;
Burford, RP ;
Hoffman, MJ .
POLYMER ENGINEERING AND SCIENCE, 2000, 40 (11) :2311-2316
[35]   THE DETERMINATION OF RESIDUAL-STRESSES IN PLASTIC PIPE AND THEIR ROLE IN FRACTURE [J].
WILLIAMS, JG ;
HODGKINSON, JM ;
GRAY, A .
POLYMER ENGINEERING AND SCIENCE, 1981, 21 (13) :822-828
[36]   Overview -: Residual stress part 1 -: Measurement techniques [J].
Withers, PJ ;
Bhadeshia, HKDH .
MATERIALS SCIENCE AND TECHNOLOGY, 2001, 17 (04) :355-365
[37]  
Yoshikawa T, 2001, J Adhes Dent, V3, P177