Effect of cryogenic temperature on static fracture of concrete having different structural sizes: Experimental tests

被引:42
作者
Jin, Liu [1 ]
Yu Wenxuan [1 ]
Jia, Likun [1 ]
Zhang, Renbo [1 ]
Hao, Yifei [2 ]
Du Xiuli [1 ]
机构
[1] Beijing Univ Technol, Minist Educ, Key Lab Urban Secur & Disaster Engn, Beijing 100124, Peoples R China
[2] Tianjin Univ, Sch Civil Engn, Tianjin 300072, Peoples R China
基金
中国国家自然科学基金;
关键词
Concrete materials; Compressive failure; Splitting tensile strength; Cryogenic temperatures; Static test; Size effect; SPLITTING-TENSILE-STRENGTH; FIBER-REINFORCED CONCRETE; NUMERICAL-SIMULATION; MECHANICAL-PROPERTIES; COMPRESSIVE STRENGTH; AGGREGATE SIZE; PERFORMANCE; SHAPE;
D O I
10.1016/j.coldregions.2021.103431
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
Cryogenic temperature is one of the extreme environments for the application of concrete. Compared with the vast amounts of researches on the size effect of concrete at ambient temperature, the investigation on size effect at cryogenic temperature is very limited. This work presents a series of experimental investigations on the static uniaxial-compressive/ splitting-tensile failure of concrete with different structural sizes (100, 150, and 300 mm) at four target temperature levels (+20 degrees C, -30 degrees C, -60 degrees C, and - 90 degrees C). The experimental results indicate that when the temperature decreases, the concrete specimens present more brittle failure patterns and the number of damaged aggregate particles on the failure surface increases. Additionally, both the measured uniaxialcompressive and splitting-tensile strengths increase linearly, and structural size exhibits a significant influence on the nominal strengths. The obvious size effect can be observed on compressive and splitting-tensile strengths at cryogenic temperature. Compared to uniaxial-compressive strength, cryogenic temperature performs more significant effect on the splitting-tensile strength and its corresponding size effect. Finally, based on the statistical size effect law, a modified prediction formula considering quantitative coupling effect of temperature and structural size was proposed, which can predict the nominal strength of concrete with different structural size at different cryogenic temperatures.
引用
收藏
页数:15
相关论文
共 49 条
[41]  
Weibul, 1939, INGENIOERSVETENSKAPS, V151, P1
[42]   Experimental studies and analysis on compressive strength of normal-weight concrete at low temperatures [J].
Xie, Jian ;
Yan, Jia-Bao .
STRUCTURAL CONCRETE, 2018, 19 (04) :1235-1244
[43]   Experimental study on the axial-compression performance of concrete at cryogenic temperatures [J].
Xie, Jian ;
Li, Xiaomei ;
Wu, Honghai .
CONSTRUCTION AND BUILDING MATERIALS, 2014, 72 :380-388
[44]  
Yamane Sho., 1978, Properties of Concrete at Very Low Temperatures
[45]  
Yan D.M., 2006, Experimental and theoretical study on the dynamic properties of concrete
[46]   Mechanical properties of normal strength mild steel and high strength steel S690 in low temperature relevant to Arctic environment [J].
Yan, Jia-Bao ;
Liew, J. Y. Richard ;
Zhang, Min-Hong ;
Wang, Jun-Yan .
MATERIALS & DESIGN, 2014, 61 :150-159
[47]   Comparison of permafrost degradation under natural ground surfaces and embankments of the Qinghai-Tibet Highway [J].
Yu, Fan ;
Qi, Jilin ;
Yao, Xiaoliang ;
Liu, Yongzhi .
COLD REGIONS SCIENCE AND TECHNOLOGY, 2015, 114 :1-8
[48]  
Zhou H., 2010, EXPT STUDY SIZE EFFE
[49]   An experimental investigation on the correlation between the aggregate size effect and the structural size effect [J].
Zhu, Ran ;
Alam, Syed Yasir ;
Loukili, Ahmed .
ENGINEERING FRACTURE MECHANICS, 2020, 234 (234)