Observation of type IV cracking in welded joints of high chromium ferritic heat resistant steels

被引:37
作者
Shinozaki, K
Li, D
Kuroki, H
Harada, H
Ohishi, K
Sato, T
机构
[1] Kure Res Lab, Dept Mat Res, Hitachi, Ibaraki, Japan
[2] Hiroshima Univ, Grad Sch Engn, Dept Mech Syst Engn, Hiroshima 7398527, Japan
关键词
D O I
10.1179/136217103225005444
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Type IV cracking in welded joints of high Cr ferritic heat resistant steels at 923 K is investigated in the present study. First, internal pressure creep tests were performed to investigate the features of cracking at 923 K and at stresses of 108-167 MPa. Results showed that at low stresses cracks occurred in the fine grained heat affected zone (FGHAZ), showing low deformation, a vast amount of creep voids and short creep life: these were identified to be type IV cracks. However, as the stress was increased the crack locations moved further away from the fusion line, the creep void area density decreased, and the slope of the main crack ratio curve increased. At high stress, cracks occurred in the base metal and were identified to be normal cracks. Second, creep tests were carried out on one pass welded specimens to clarify the relationship between the creep property deterioration in the FGHAZ and the weld thermal cycle. Type IV cracking was repeated successfully and results showed good correspondence with the position of cracks among the softened region, the highest creep void area density and the fracture location. Both internally pressurised and one pass welded specimens showed that at low stress the FGHAZ was the weak zone and creep voids played an important role in type IV cracking.
引用
收藏
页码:289 / 295
页数:7
相关论文
共 23 条
  • [1] BHADESHIA HKD, 2000, P INT WORKSH INN STR, P89
  • [2] Design of ferritic creep-resistant steels
    Bhadeshia, HKDH
    [J]. ISIJ INTERNATIONAL, 2001, 41 (06) : 626 - 640
  • [3] The influence of microstructural aspects on the service behaviour of advanced power plant steels
    Cerjak, H
    Hofer, P
    Schaffernak, B
    [J]. ISIJ INTERNATIONAL, 1999, 39 (09) : 874 - 888
  • [4] Cerjak H., 1996, SCI TECHNOL WELD JOI, V1, P36
  • [5] CERJAK H, 2001, 5 WORKSH ULTR STEEL, P158
  • [6] Possible effect of Co on coarsening of M23C6 carbide and Orowan stress in a 9% Cr steel
    Gustafson, Å
    Ågren, J
    [J]. ISIJ INTERNATIONAL, 2001, 41 (04) : 356 - 360
  • [7] Creep deformation and the corresponding microstructural evolution in high-Cr ferritic steels
    Igarashi, M
    Muneki, S
    Hasegawa, H
    Yamada, K
    Abe, F
    [J]. ISIJ INTERNATIONAL, 2001, 41 : S101 - S105
  • [8] ISEDA A, 1991, TETSU TO HAGANE, V81, P582
  • [9] Kanemaru O, 1997, MATER SCI RES INT, V3, P31
  • [10] Development of high strength 15Cr ferritic creep resistant steel with addition of tungsten and cobalt
    Kimura, K
    Seki, K
    Toda, Y
    Abe, F
    [J]. ISIJ INTERNATIONAL, 2001, 41 : S121 - S125