Depth-Resolved FTIR-ATR Imaging Studies of Coating Degradation during Accelerated and Natural Weathering-Influence of Biobased Reactive Diluents in Polyester Melamine Coil Coating

被引:9
作者
Warnheim, Alexander [1 ,2 ]
Edvinsson, Camilla [1 ]
Sundell, Per-Erik [3 ]
Heydari, Golrokh [3 ]
Deltin, Tomas [4 ]
Persson, Dan [1 ]
机构
[1] Res Inst Sweden, Dept Corros, Div Mat & Prod, S-16407 Kista, Sweden
[2] KTH Royal Inst Technol, Sch Engn Sci Chem Biotechnol & Health, Dept Chem, Div Surface & Corros Sci, S-10044 Stockholm, Sweden
[3] SSAB Europe, S-78184 Borlange, Sweden
[4] Nord United Coatings, S-25225 Helsingborg, Sweden
关键词
OUTDOOR EXPOSURE; IR; PERFORMANCE; HUMIDITY; HYDROLYSIS; PREDICTION; PHOTOLYSIS; MECHANISM; MODEL;
D O I
10.1021/acsomega.2c02523
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Improved methods to assess the degradation of coil coatings to approximate lifetime have been an area of academic and industrial interest for decades. This work aims to elucidate the differences in the degradation behavior of two coil coating systems: one standard commercial formulation and one formulation with a significant addition of biorenewable reactive diluents. Depth-resolved degradation behavior of samples exposed to accelerated and natural field weathering is assessed. Focal plane array attenuated total reflection-Fourier transform infrared spectroscopy was used to acquire high-resolution chemical data from a sloping cross section. The results agreed with conventional photoacoustic spectroscopy. Degradation profiles for the two coatings were significantly different, with the biobased samples showing a more durable behavior. This study provides a method for detailed assessment of coating degradation, giving a good estimation of its durability. This is both a way to compare the performance of coating systems and to improve the understanding of the impact of exposure conditions, paving the way for the development of more sustainable coil coatings.
引用
收藏
页码:23842 / 23850
页数:9
相关论文
共 52 条
[1]  
[Anonymous], 2006, Fourier Transform Infrared Spectrometry
[2]  
Atlas Material Testing Solutions, WEATH DAT FLOR BENCH
[3]   Effect of the polyester chemical structure on the stability of polyester-melamine coatings when exposed to accelerated weathering [J].
Batista, Marcos A. J. ;
Moraes, Raul P. ;
Barbosa, Jayne C. S. ;
Oliveira, Pedro C. ;
Santos, Amilton M. .
PROGRESS IN ORGANIC COATINGS, 2011, 71 (03) :265-273
[4]  
BAUER DR, 1984, ACS SYM SER, V243, P271
[7]   THE ROLE OF HUMIDITY IN THE PHOTOOXIDATION OF ACRYLIC MELAMINE COATINGS [J].
BAUER, DR ;
MIELEWSKI, DF .
POLYMER DEGRADATION AND STABILITY, 1993, 40 (03) :349-355
[8]   Detection of in Situ Early Corrosion on Polymer-Coated Metal Substrates [J].
Braasch, Dwaine A. ;
Gillis, Mathew ;
Pramanik, Monoj ;
Ferguson, Richard C. ;
Delatte, David ;
Blanton, Michael ;
Rawlins, James Wayne .
ACS APPLIED MATERIALS & INTERFACES, 2019, 11 (40) :37193-37208
[9]   Attenuated total reflection Fourier transform infrared microspectroscopy: Theory and application to polymer samples [J].
Buffeteau, T ;
Desbat, B ;
Eyquem, D .
VIBRATIONAL SPECTROSCOPY, 1996, 11 (01) :29-36
[10]   New opportunities in micro- and macro-attenuated total reflection infrared spectroscopic imaging: Spatial resolution and sampling versatility [J].
Chan, KLA ;
Kazarian, SG .
APPLIED SPECTROSCOPY, 2003, 57 (04) :381-389