Influence of temperature on the atmospheric corrosion of the Mg-Al alloy AM50

被引:111
作者
Esmaily, M. [1 ]
Shahabi-Navid, M. [1 ]
Svensson, J. -E. [1 ]
Halvarsson, M. [2 ]
Nyborg, L. [3 ]
Cao, Y. [3 ]
Johansson, L. -G. [1 ]
机构
[1] Chalmers Univ Technol, Dept Chem & Biol Engn, SE-41296 Gothenburg, Sweden
[2] Chalmers Univ Technol, Dept Appl Phys, SE-41296 Gothenburg, Sweden
[3] Chalmers Univ Technol, Dept Mat & Mfg Technol, SE-41296 Gothenburg, Sweden
关键词
Magnesium; Alloy; SEM; Atmospheric corrosion; MAGNESIUM ALLOYS; RELATIVE-HUMIDITY; BEHAVIOR; NACL; CHLORIDE; AZ91D; MICROSTRUCTURE; WATER; ZINC; CO2;
D O I
10.1016/j.corsci.2014.10.040
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of temperature on the NaCl-induced atmospheric corrosion of the Mg-Al alloy AM50 has been investigated in the laboratory. The corroded samples were analyzed gravimetrically and by SEM, EDX, XRD, and FTIR. The atmospheric corrosion of 99.97% Mg was also studied for reference. While the NaCl-induced atmospheric corrosion of AM50 is strongly reduced with decreasing temperature, 99.97% Mg does not exhibit such a trend. The temperature dependence of the atmospheric corrosion of alloy AM50 is attributed to the aluminum content in the alloy. Several crystalline magnesium hydroxy carbonates formed at 4 and 22 degrees C but were absent at -4 degrees C. (C) 2014 The Authors. Published by Elsevier Ltd.
引用
收藏
页码:420 / 433
页数:14
相关论文
共 54 条
[1]  
Advedesian M.M., 1999, ASM SPECIALTY HDB
[2]   Corrosion behaviour of AZ91D and AM50 magnesium alloys with Nd and Gd additions in humid environments [J].
Arrabal, R. ;
Matykina, E. ;
Pardo, A. ;
Merino, M. C. ;
Paucar, K. ;
Mohedano, M. ;
Casajus, P. .
CORROSION SCIENCE, 2012, 55 :351-362
[3]   WATER-VAPOR PARTIAL PRESSURES AND WATER ACTIVITIES IN POTASSIUM AND SODIUM-HYDROXIDE SOLUTIONS OVER WIDE CONCENTRATION AND TEMPERATURE RANGES [J].
BALEJ, J .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 1985, 10 (04) :233-243
[4]   DEVELOPMENT OF CORROSION-RESISTANT MAGNESIUM ALLOYS .2. STRUCTURE OF CORROSION PRODUCTS ON RAPIDLY SOLIDIFIED MG-16AL ALLOYS [J].
BALIGA, CB ;
TSAKIROPOULOS, P .
MATERIALS SCIENCE AND TECHNOLOGY, 1993, 9 (06) :513-519
[5]   The corrosion of pure magnesium in aerated and deaerated sodium sulphate solutions [J].
Baril, G ;
Pébère, N .
CORROSION SCIENCE, 2001, 43 (03) :471-484
[6]   Activity of water in aqueous systems; A frequently neglected property [J].
Blandamer, MJ ;
Engberts, JBFN ;
Gleeson, PT ;
Reis, JCR .
CHEMICAL SOCIETY REVIEWS, 2005, 34 (05) :440-458
[7]   The influence of CO2, ACl3•6H2O, MgCl2•6H2O, Na2SO4 and NaCl on the atmospheric corrosion of aluminum [J].
Blucher, D. Bengtsson ;
Svensson, J. -E. ;
Johansson, L. -G. .
CORROSION SCIENCE, 2006, 48 (07) :1848-1866
[8]   Scanning kelvin probe force microscopy -: A useful tool for studying atmospheric corrosion of MgAl alloys in situ [J].
Blücher, DB ;
Svensson, JE ;
Johansson, LG ;
Rohwerder, M ;
Stratmann, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2004, 151 (12) :B621-B626
[9]   The NaCl-induced atmospheric corrosion of aluminum -: The influence of carbon dioxide and temperature [J].
Blücher, DB ;
Svensson, JE ;
Johansson, LG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2003, 150 (03) :B93-B98