Effect of water density and air pressure on partial oxidation of bitumen in supercritical water

被引:69
作者
Sato, Takafumi [1 ]
Phan Hieu Trung [1 ]
Tomita, Tomoyuki [1 ]
Itoh, Naotsugu [1 ]
机构
[1] Utsunomiya Univ, Dept Mat & Environm Chem, Utsunomiya, Tochigi 3218585, Japan
关键词
Heavy oil; Supercritical water; Partial oxidation; Bitumen; Water gas shift reaction; GAS SHIFT REACTION; REACTION-KINETICS; HYDROCARBONS; METHANE;
D O I
10.1016/j.fuel.2011.10.016
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
Partial oxidation of bitumen was examined in supercritical water from 653 to 723 K at a water/oil ratio from 0 to 3 and up to 5.1 MPa of initial air pressure. The contents in the reactor were separated into water rich phase and oil rich phase. Most of oxygen was quickly consumed within 30 min and the main gases produced were CO, CO2 and methane. The low temperature gave higher CO/(CO + CO2) ratio and suppressed coke formation. The amount of total gas tended to decrease and the ratio of CO/(CO + CO2) increased about two times by the increase in water/oil ratio from 0.5 to 3. The high water/oil ratio was preferred for selective partial oxidation to produce CO, which means that the effect of the enhancement of partial oxidation by supercritical water was probably larger than that of CO oxidation by water and water gas shift reaction. The increase in initial air pressure increased the amount of CO and CO2 and decreased the ratio of CO/(CO + CO2). The total oxidation route was enhanced under high air pressure. (C) 2011 Elsevier Ltd. All rights reserved.
引用
收藏
页码:347 / 351
页数:5
相关论文
共 28 条
[1]   Catalytic hydrodesulfurization of dibenzothiophene through partial oxidation and a water-gas shift reaction in supercritical water [J].
Adschiri, T ;
Shibata, R ;
Sato, T ;
Watanabe, M ;
Arai, K .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1998, 37 (07) :2634-2638
[2]   Roles of water for chemical reactions in high-temperature water [J].
Akiya, N ;
Savage, PE .
CHEMICAL REVIEWS, 2002, 102 (08) :2725-2750
[3]  
[Anonymous], NIST CHEM WEBBOOK
[4]   Hydrogenation of hydrocarbons through partial oxidation in supercritical water [J].
Arai, K ;
Adschiri, T ;
Watanabe, M .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2000, 39 (12) :4697-4701
[5]   Partial oxidation of propane in sub- and supercritical water [J].
Armbruster, U ;
Martin, A ;
Krepel, A .
JOURNAL OF SUPERCRITICAL FLUIDS, 2001, 21 (03) :233-243
[6]   Effects of Supercritical Water in Vacuum Residue Upgrading [J].
Cheng, Zhen-Min ;
Ding, Yong ;
Zhao, Li-Qun ;
Yuan, Pei-Qing ;
Yuan, Wei-Kang .
ENERGY & FUELS, 2009, 23 (5-6) :3178-3183
[7]   Thermal cracking of Athabasca bitumen: Influence of steam on reaction chemistry [J].
Dutta, RP ;
McCaffrey, WC ;
Gray, MR ;
Muehlenbachs, K .
ENERGY & FUELS, 2000, 14 (03) :671-676
[8]   Partial oxidative gasification of phenol for hydrogen in supercritical water [J].
Guan, Qingqing ;
Wei, Chaohai ;
Shi, Huashun ;
Wu, Chaofei ;
Chai, Xin-Sheng .
APPLIED ENERGY, 2011, 88 (08) :2612-2616
[9]   OXIDATION OF HYDROGEN AND CARBON-MONOXIDE IN SUBCRITICAL AND SUPERCRITICAL WATER - REACTION-KINETICS, PATHWAYS, AND WATER-DENSITY EFFECTS .2. ELEMENTARY REACTION MODELING [J].
HOLGATE, HR ;
TESTER, JW .
JOURNAL OF PHYSICAL CHEMISTRY, 1994, 98 (03) :810-822
[10]   Partial hydrothermal oxidation of unsaturated high molecular weight carboxylic acids for enhancing the cold flow properties of biodiesel fuel [J].
Jin, Fangming ;
Zeng, Xu ;
Cao, Jianglin ;
Kawasaki, Kohei ;
Kishita, Atsushi ;
Tohji, Kazuyuki ;
Enomoto, Heiji .
FUEL, 2010, 89 (09) :2448-2454