Degradation of biodegradable implants: The influence of microstructure and composition of Mg-Zn-Ca alloys

被引:47
作者
Roche, V [1 ]
Koga, G. Y. [2 ]
Matias, T. B. [2 ]
Kiminami, C. S. [2 ]
Bolfarini, C. [2 ]
Botta, W. J. [1 ,2 ]
Nogueira, R. P. [1 ,3 ]
Jorge Junior, A. M. [1 ,2 ,4 ]
机构
[1] Grenoble Alpes Univ, LEPMI, CNRS, F-38000 Grenoble, France
[2] Univ Fed Sao Carlos, Dept Mat Engn, BR-13565905 Sao Carlos, SP, Brazil
[3] Khalifa Univ Sci & Technol, Gas Res Ctr, Abu Dhabi, U Arab Emirates
[4] Grenoble Alpes Univ, SIMAP, CNRS, F-38000 Grenoble, France
基金
巴西圣保罗研究基金会;
关键词
Mg-Zn-Ca alloys; Biomaterials; Implants; Biodegradation; Degradation scalability; Ultrafine grains; Amorphous materials; BULK METALLIC GLASSES; CORROSION BEHAVIOR; MAGNESIUM ALLOYS; MECHANICAL-PROPERTIES; ANODIC-DISSOLUTION; GRAIN-SIZE; IN-VIVO; ELECTROCHEMICAL CORROSION; AMORPHOUS-ALLOYS; PURE MAGNESIUM;
D O I
10.1016/j.jallcom.2018.09.346
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This work reports on the degradation of two (Zn-poor and Zn-rich) Mg-Zn-Ca crystalline alloys produced by mold casting yielding different kinds of microstructures with several scales. The dependence of corrosion properties and hydrogen evolution with alloy compositions, sizes and kinds of microstructure was exhaustively analyzed. The results were compared with amorphous alloys of same compositions. Zn-rich composition with average grain sizes of less than 500 nm presented marginal and an acceptable level of hydrogen, which was lower than for larger grains or Zn-poor composition. This behavior was explained by the reduction of the intrinsic metallic surface reactivity and the higher stability of the oxide film, which reduce the corrosion rate and, consequently, the hydrogen evolution. Mg-Zn-Ca crystalline alloys with Zn-alloying threshold and homogeneous grain size (<500 nm) appear hence to be of great potential for use in biodegradable implants. (C)2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:168 / 181
页数:14
相关论文
共 71 条
[1]   ANODIC DISSOLUTION OF BERYLLIUM IN ANHYDROUS MEDIA [J].
AIDA, H ;
EPELBOIN, I ;
GARREAU, M .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1971, 118 (02) :243-&
[2]   Evaluation of microstructural effects on corrosion behaviour of AZ91D magnesium alloy [J].
Ambat, R ;
Aung, NN ;
Zhou, W .
CORROSION SCIENCE, 2000, 42 (08) :1433-1455
[3]   The negative difference effect and unipositive Mg+ [J].
Atrens, Andrej ;
Dietzel, Wolfgang .
ADVANCED ENGINEERING MATERIALS, 2007, 9 (04) :292-297
[4]   The relation between severe plastic deformation microstructure and corrosion behavior of AZ31 magnesium alloy [J].
Ben Hamu, G. ;
Eliezer, D. ;
Wagner, L. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 468 (1-2) :222-229
[5]   The relation between microstructure and corrosion behavior of Mg-Y-RE-Zr alloys [J].
Ben-Hamu, G. ;
Eliezer, D. ;
Shin, K. S. ;
Cohen, S. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2007, 431 (1-2) :269-276
[6]   Corrosion behaviour of stressed magnesium alloys [J].
Bonora, PL ;
Andrei, M ;
Eliezer, A ;
Gutman, EM .
CORROSION SCIENCE, 2002, 44 (04) :729-749
[7]   Potentiodynamic polarisation study of bulk metallic glasses based on the Mg-Zn-Ca ternary system [J].
Cao, J. D. ;
Laws, K. J. ;
Birbilis, N. ;
Ferry, M. .
CORROSION ENGINEERING SCIENCE AND TECHNOLOGY, 2012, 47 (05) :329-334
[8]   Ca-Mg-Zn bulk metallic glasses as bioresorbable metals [J].
Cao, J. D. ;
Kirkland, N. T. ;
Laws, K. J. ;
Birbilis, N. ;
Ferry, M. .
ACTA BIOMATERIALIA, 2012, 8 (06) :2375-2383
[9]   Anomalous dissolution of metals and chemical corrosion [J].
Drazic, DM ;
Popic, JP .
JOURNAL OF THE SERBIAN CHEMICAL SOCIETY, 2005, 70 (03) :489-511
[10]   Electrochemical corrosion behavior of magnesium and titanium alloys in simulated body fluid [J].
Fekry, A. M. ;
El-Sherif, Rabab M. .
ELECTROCHIMICA ACTA, 2009, 54 (28) :7280-7285