In situ TiC/Inconel 625 nanocomposites fabricated by selective laser melting: Densification behavior, microstructure evolution, and wear properties

被引:49
作者
Chen, Lan [1 ]
Sun, Yuzhou [1 ]
Li, Lin [2 ]
Ren, Yunpeng [1 ]
Ren, Xudong [1 ]
机构
[1] Jiangsu Univ, Dept Mech Engn, Zhenjiang 212013, Jiangsu, Peoples R China
[2] Univ Manchester, Dept Aerosp & Civil Engn, Manchester M13 9PL, Lancs, England
基金
中国国家自然科学基金;
关键词
Selective laser melting; Nanocomposites; TiC; Microstructure; Wear; STAINLESS-STEEL COMPOSITE; MECHANICAL-PROPERTIES; MARANGONI CONVECTION; ALLOY; SLM; GROWTH; HEAT; TEMPERATURE; RESISTANCE; TEXTURE;
D O I
10.1016/j.apsusc.2020.145981
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
An Inconel 625-based nanocomposite reinforced with TiC nanoparticles (TiC/IN625) was successfully prepared by selective laser melting. The effects of laser fluence on the densification, microstructure, crystal structure, microhardness, and wear performance of the prepared nanocomposites were systematically investigated. A low laser fluence induced many defects, such as pores, cavities, and unmelted particles, whereas a high laser fluence resulted in a significantly increased densification. The increase in the laser fluence resulted in the continuous development of the microstructure of TiC/IN625 nanocomposites. A laser fluence of 139 J/mm(3) led to insufficient growth, while a sufficient growth was achieved at the laser fluence of 167 J/mm(3); at 208 J/mm(3), refined columnar/cellular dendrites were formed. Compared to IN625, smaller grains (less than 5 mu m) and a larger proportion of sub-grain boundaries appeared in the TiC/IN625 nanocomposites due to grain refinement. The TiC phases precipitated in situ in the grain boundaries, and a high level of dislocation was introduced into the TiC/IN625 nanocomposites. The maximum microhardness of the TiC/IN625 nanocomposites was 440 HV at the laser fluence of 208 J/mm(3). The lowest coefficient of friction and wear rate were 0.33 and 3.5 x 10(-4) mm(3) N-1 m(-1), respectively.
引用
收藏
页数:14
相关论文
共 50 条
[11]   Laser Metal Deposition Additive Manufacturing of TiC Reinforced Inconel 625 Composites: Influence of the Additive TiC Particle and Its Starting Size [J].
Gu, Dongdong ;
Cao, Sainan ;
Lin, Kaijie .
JOURNAL OF MANUFACTURING SCIENCE AND ENGINEERING-TRANSACTIONS OF THE ASME, 2017, 139 (04)
[12]   Combined strengthening of multi-phase and graded interface in laser additive manufactured TiC/Inconel 718 composites [J].
Gu, Dongdong ;
Hong, Chen ;
Jia, Qingbo ;
Dai, Donghua ;
Gasser, Andres ;
Weisheit, Andreas ;
Kelbassa, Ingomar ;
Zhong, Minlin ;
Poprawe, Reinhart .
JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2014, 47 (04)
[13]   Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by Selective Laser Melting (SLM): Densification, growth mechanism and wear behavior [J].
Gu, Dongdong ;
Hagedorn, Yves-Christian ;
Meiners, Wilhelm ;
Wissenbach, Konrad ;
Poprawe, Reinhart .
COMPOSITES SCIENCE AND TECHNOLOGY, 2011, 71 (13) :1612-1620
[14]   Evaluation of Marangoni convection and free surface velocity of molten tungsten for tungsten divertor [J].
Hamaguchi, Kohei ;
Hoashi, Eiji ;
Okita, Takafumi ;
Ibano, Kenzo ;
Ueda, Yoshio .
FUSION ENGINEERING AND DESIGN, 2019, 140 :117-122
[15]   Effects of TiC on the microstructure and properties of TiC/TiAl composite coating prepared by laser cladding [J].
He, X. ;
Song, R. G. ;
Kong, D. J. .
OPTICS AND LASER TECHNOLOGY, 2019, 112 :339-348
[16]   Microstructure and laser irradiation characteristics of TiC-free and TiC-doped tungsten-based coatings prepared by supersonic atmospheric plasma spraying [J].
Hou, Qingyu ;
Ma, Xiaoyu ;
Lu, Rongcheng ;
Wang, Wei ;
Wang, Ping ;
Huang, Zhenyi .
SURFACE & COATINGS TECHNOLOGY, 2019, 358 :796-805
[17]   A review on laser deposition-additive manufacturing of ceramics and ceramic reinforced metal matrix composites [J].
Hu, Yingbin ;
Cong, Weilong .
CERAMICS INTERNATIONAL, 2018, 44 (17) :20599-20612
[18]  
Iida T., 1988, PHYS PROPERTIES LIQU
[19]   Evolution of structure and properties of the nickel-based alloy EP718 after the SLM growth and after different types of heat and mechanical treatment [J].
Ivanov, D. ;
Travyanov, A. ;
Petrovskiy, P. ;
Cheverikin, V ;
Alekseeva, E. ;
Khvan, A. ;
Logachev, I .
ADDITIVE MANUFACTURING, 2017, 18 :269-275
[20]   Controllable mesostructure, magnetic properties of soft magnetic Fe-Ni-Si by using selective laser melting from nickel coated high silicon steel powder [J].
Kang, N. ;
El Mansori, M. ;
Guittonneau, F. ;
Liao, H. ;
Fu, Y. ;
Aubry, E. .
APPLIED SURFACE SCIENCE, 2018, 455 :736-741