Effect of Al3Zr particles on hot-compression behavior and processing map for Al-Cu-Li based alloys at elevated temperatures

被引:28
|
作者
Yang, Qing-bo [1 ]
Deng, Yan-jun [2 ]
Yang, Mou [1 ]
Zhang, Zhi-qing [1 ,3 ,4 ]
Li, Wei-guo [5 ]
Liu, Qing [1 ]
机构
[1] Chongqing Univ, Coll Mat Sci & Engn, Chongqing 400045, Peoples R China
[2] Changan Auto Global R&D Ctr, Chongqing 401120, Peoples R China
[3] China Xipeng Aluminum Ind Pk, Chongqing 401326, Peoples R China
[4] Chongqing Univ, Chongqing Univ Univ Cincinnati Joint Coop Inst, Chongqing 401331, Peoples R China
[5] Chongqing Univ, Coll Aerosp Engn, Chongqing 400045, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Cu-Li based alloy; Al3Zr particle; hot compression; processing map; ZR-TI ALLOYS; DEFORMATION-BEHAVIOR; PRECIPITATION EVOLUTION; MICROSTRUCTURAL EVOLUTION; MECHANICAL-PROPERTIES; COARSENING BEHAVIOR; SC; RECRYSTALLIZATION; RESISTANCE; WORKING;
D O I
10.1016/S1003-6326(20)65261-X
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The influence of Al3Zr particles on the hot compression behavior and processing map (PM) of Al-Cu-Li based alloys under isothermal plane-strain compression in the temperature range of 400-500 degrees C and at the strain rates of 0.01-10 s(-1) was investigated. The corresponding microstructure was analyzed using optical microscopy (OM), electron back-scattered diffraction (EBSD) and transmission electron microscope (ULM). The results showed that dynamic recovery (DRV) played a greater role than dynamic recrystallization (DRX) in dynamic softening. At low temperatures, the Al3Zr particles were the significant barriers to inhibit DRV and DRX grain growth. When the temperature reached 500 degrees C, the Al3Zr particles readily spread along grain boundaries just like a necklace due to the dissolution of Al3Zr particles and rapid diffusion of Zr through grain boundary, resulting in generating the macroscopic cracks and forming an instability domain at 490-500 degrees C, 0.01 s(-1) in the PM.
引用
收藏
页码:872 / 882
页数:11
相关论文
共 50 条
  • [41] Flow stress behavior of Al-Cu-Li-Zr alloy containing Sc during hot compression deformation
    Wen-jie Liang
    Qing-lin Pan
    Yun-bin He
    Yun-chun Li
    Xiao-gang Zhang
    Journal of Central South University of Technology, 2008, 15 : 289 - 294
  • [42] Flow stress behavior of Al-Cu-Li-Zr alloy containing Sc during hot compression deformation
    Liang Wen-jie
    Pan Qing-lin
    He Yun-bin
    Li Yun-chun
    Zhang Xiao-gang
    JOURNAL OF CENTRAL SOUTH UNIVERSITY OF TECHNOLOGY, 2008, 15 (03): : 289 - 294
  • [43] Flow stress behavior of Al-Cu-Li-Zr alloy containing Sc during hot compression deformation
    梁文杰
    潘清林
    何运斌
    李运春
    张小刚
    JournalofCentralSouthUniversityofTechnology, 2008, (03) : 289 - 294
  • [44] New insight into precipitation of Al3Zr and correlative effect on recrystallization behavior in a rapidly-solidified Al-Zn-Mg-Cu-Zr alloy
    Wang, Zhiping
    Xiao, Hongyu
    Chen, Wei
    Li, Yugang
    Geng, Jiwei
    Li, Xianfeng
    Xia, Peikang
    Wang, Mingliang
    Chen, Dong
    Wang, Haowei
    MATERIALS CHARACTERIZATION, 2022, 191
  • [45] Hot deformation behavior of the new Al-Mg-Si-Cu aluminum alloy during compression at elevated temperatures
    Zhang, Hui
    Li, Luoxing
    Yuan, Deng
    Peng, Dashu
    MATERIALS CHARACTERIZATION, 2007, 58 (02) : 168 - 173
  • [46] Effect of Li Content on Hot-Tearing Susceptibility of Ternary Al-Cu-Li Alloys: Experimental Investigation, Criterion Prediction, and Simulation Assessment
    Guo, Youjie
    Zhang, Liang
    Wu, Guohua
    Wang, Yixiao
    Qi, Fangzhou
    Xu, Xuanxi
    Tong, Xin
    Li, Peisen
    Ren, Guangxiao
    Geng, Yingjing
    Li, Liangbin
    Xiong, Xunman
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2023, 54 (12): : 4850 - 4867
  • [47] Effect of Li Content on Hot-Tearing Susceptibility of Ternary Al-Cu-Li Alloys: Experimental Investigation, Criterion Prediction, and Simulation Assessment
    Youjie Guo
    Liang Zhang
    Guohua Wu
    Yixiao Wang
    Fangzhou Qi
    Xuanxi Xu
    Xin Tong
    Peisen Li
    Guangxiao Ren
    Yingjing Geng
    Liangbin Li
    Xunman Xiong
    Metallurgical and Materials Transactions A, 2023, 54 : 4850 - 4867
  • [48] Effect of Zr on the high cycle fatigue and mechanical properties of Al-Si-Cu-Mg alloys at elevated temperatures
    Liu, Guangyu
    Blake, Paul
    Ji, Shouxun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 809
  • [49] Deformation Behavior and Processing Parameters of Cu-3Ag-0.6Zr Alloy during Compression at Elevated Temperatures
    Xue, Zhiyong
    Gu, Lingyun
    Ren, Yu
    Hao, Xiaoyang
    Xu, Ping
    INTERNATIONAL SYMPOSIUM ON MATERIALS APPLICATION AND ENGINEERING (SMAE 2016), 2016, 67
  • [50] Effect of different aging processes on the corrosion behavior of new Al-Cu-Li-Zr-Sc alloys
    Peng, Zhuowei
    Pan, Qinglin
    Cai, Shan
    Li, Jinfeng
    Liang, Wenjie
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (12): : 2266 - 2277