The Partial Replacement of Halloysite Nanotubes (HNTs) and Precipitated Silica by Recycled Poly(ethylene terephthalate) Powder on Cure Behavior, Tensile Properties and Morphology of Natural Rubber Composites

被引:2
作者
Nabil, H. [1 ]
Ismail, H. [1 ]
Azura, A. R. [1 ]
机构
[1] Univ Sains Malaysia, Dept Polymer Engn, Sch Mat & Mineral Resources Engn, Nibong Tebal 14300, Penang, Malaysia
来源
COMPOSITE SCIENCE AND TECHNOLOGY, PTS 1 AND 2 | 2011年 / 471-472卷
关键词
Recycled polyethylene terephthalate; Natural Rubber; Halloysite nanotubes; Silica; MECHANICAL-PROPERTIES;
D O I
10.4028/www.scientific.net/KEM.471-472.622
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this article, halloysite nanotubes (HNTs) and precipitated silica were replaced by recycled polyethylene terephthalate powder (R-PET) in natural rubber composites. Five different compositions of NR/HNTs/R-PET and NR/Silica/R-PET composites [i.e. 100/20/0, 100/15/5, 100/10/10, 100/5/15, and 100/0/20 parts per hundred rubber (phr)] were prepared on a two-roll-mill. Comparison of the curing behavior, tensile properties, and morphological characteristics of natural rubber composites was studied. The results indicated that the replacement of HNTs and silica by R-PET decreased the tensile strength, tensile modulus, and elongation at break of composites, but NR/Silica/R-PET composites showed the lower trend than that NR/HNTs/R-PET did. The negative effect of these properties could be explained by the decrement of crosslink density, R-PET is unable to be transferred the stress due to the weal rubber-fillers interactions, and the reducing of ductility of rubber matrix. The curing results revealed that, with replacement of HNTs and Silica by R-PET, the scorch time (ts(2)) and cure time (tc(90)) were decreased. Scanning electron microscopy investigation of tensile fracture surfaces confirmed that co-incorporation of NR/HNTs/R-PET would improve the dispersion of R-PET and enhanced the interactions between fillers and NR matrix rather than NR/Silica/R-PET composites.
引用
收藏
页码:622 / 627
页数:6
相关论文
共 29 条
  • [1] Compatibilization of recycled and virgin PET with radiation-oxidized HDPE
    Burillo, G
    Herrera-Franco, P
    Vazquez, M
    Adem, E
    [J]. RADIATION PHYSICS AND CHEMISTRY, 2002, 63 (3-6) : 241 - 244
  • [2] Charles A. H., 2006, HDB PLASTICS TECHNOL
  • [3] Characteristics of mortar and concrete containing fine aggregate manufactured from recycled waste polyethylene terephthalate bottles
    Choi, Yun Wang
    Moon, Dae Joong
    Kim, Yong Jic
    Lachemi, Mohamed
    [J]. CONSTRUCTION AND BUILDING MATERIALS, 2009, 23 (08) : 2829 - 2835
  • [4] Curlee TR., 1991, Plastic Wastes - Management, Control, Recycling and Disposal
  • [5] Rice-husk-ash-filled natural rubber. II. Partial replacement of commercial fillers and the effect on the vulcanization process
    da Costa, HM
    Visconte, LLY
    Nunes, RCR
    Furtado, CRG
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2003, 87 (09) : 1405 - 1413
  • [6] Application of hybrid sphere/carbon nanotube particles in nanofluids
    Han, Z. H.
    Yang, B.
    Kim, S. H.
    Zachariah, M. R.
    [J]. NANOTECHNOLOGY, 2007, 18 (10)
  • [7] *IM TABL AS LTD, TECHN REP IM TABL AS
  • [8] Effects of Palm Ash Loading and Maleated Natural Rubber as a Coupling Agent on the Properties of Palm-Ash-Filled Natural Rubber Composites
    Ismail, H.
    Haw, F. S.
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2008, 110 (05) : 2867 - 2876
  • [9] Morphological, thermal and tensile properties of halloysite nanotubes filled ethylene propylene diene monomer (EPDM) nanocomposites
    Ismail, H.
    Pasbakhsh, Pooria
    Fauzi, M. N. Ahmad
    Abu Bakar, A.
    [J]. POLYMER TESTING, 2008, 27 (07) : 841 - 850
  • [10] Ismail H, 2003, J THERMOPLAST COMPOS, V16, P121, DOI [10.1177/0892705703016002871, 10.1106/089270503025871]