Results of applying a non-evaporative mitigation technique to laser-initiated surface damage on fused-silica

被引:21
作者
Adams, J. J. [1 ]
Bolourchi, M. [1 ]
Bude, J. D. [1 ]
Guss, G. M. [1 ]
Matthews, M. J. [1 ]
Nostrand, M. C. [1 ]
机构
[1] Lawrence Livermore Natl Lab, Livermore, CA 94550 USA
来源
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2010 | 2010年 / 7842卷
关键词
Fused-silica; SiO2; surface damage; damage mitigation; CO2 laser mitigation; CO2; lasers; downstream intensification; residual stress; GROWTH;
D O I
10.1117/12.867652
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
We present results from a study to determine an acceptable CO2 laser-based non-evaporative mitigation protocol for use on surface damage sites in fused-silica optics. A promising protocol is identified and evaluated on a set of surface damage sites created under ICF-type laser conditions. Mitigation protocol acceptability criteria for damage re-initiation and growth, downstream intensification, and residual stress are discussed. In previous work [1], we found that a power ramp at the end of the protocol effectively minimizes the residual stress (<25 MPa) left in the substrate. However, the biggest difficulty in determining an acceptable protocol was balancing between low re-initiation and problematic downstream intensification. Typical growing surface damage sites mitigated with a candidate CO2 laser-based mitigation protocol all survived 351 nm, 5 ns damage testing to fluences >12.5 J/cm(2). The downstream intensification arising from the mitigated sites is evaluated, and all but one of the sites has 100% passing downstream damage expectation values. We demonstrate, for the first time, a successful non-evaporative 10.6 mu m CO2 laser mitigation protocol applicable to fused-silica optics used on fusion-class lasers like the National Ignition Facility (NIF).
引用
收藏
页数:7
相关论文
共 10 条
[1]   Mitigation of laser damage growth in fused silica NIF optics with a galvanometer scanned CO2 laser [J].
Bass, Isaac L. ;
Draggoo, Vaughn G. ;
Guss, Gabriel M. ;
Hackel, Richard P. ;
Norton, Mary A. .
HIGH-POWER LASER ABLATION VI, PTS 1 AND 2, 2006, 6261
[2]   Localized CO2 laser treatment for mitigation of 351 nm damage growth on fused silica [J].
Brusasco, RM ;
Penetrante, BM ;
Butler, JA ;
Hrubesh, LW .
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2001 PROCEEDINGS, 2002, 4679 :40-47
[3]   Mitigation of growth of laser initiated surface damage in fused silica using a 4.6μm wavelength laser [J].
Guss, Gabe ;
Bassa, Isaac ;
Draggoo, Vaughn ;
Hackel, Richard ;
Payne, Steve ;
Lancaster, Mark ;
Mak, Paul .
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2006, 2007, 6403
[4]   Methods for mitigating surface damage growth on NIF final optics [J].
Hrubesh, LW ;
Norton, MA ;
Molander, WA ;
Donohue, EE ;
Maricle, SM ;
Penetrante, BM ;
Brusasco, RM ;
Grundler, W ;
Butler, JA ;
Carr, JW ;
Hill, RM ;
Summers, LJ ;
Feit, MD ;
Rubenchik, A ;
Key, MH ;
Wegner, PJ ;
Burnham, AK ;
Hackel, LA ;
Kozlowski, MR .
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2001 PROCEEDINGS, 2002, 4679 :23-33
[5]  
Matthews M. J., 2005, P SPIE INT SOC OPT E, V7504, P750410
[6]   Downstream intensification effects associated with CO2 laser mitigation of fused silica [J].
Matthews, Manyalibo J. ;
Bass, Isaac L. ;
Guss, Gabriel M. ;
Widmayer, Clay C. ;
Ravizza, Frank L. .
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2007, 2008, 6720
[7]  
Norton M. A., 2005, P SOC PHOTO-OPT INS, V5991
[8]   Design of a production process to enhance optical performance of 3ω optics [J].
Prasad, RR ;
Bruere, JR ;
Halpin, J ;
Lucero, P ;
Mills, S ;
Bernacil, M ;
Hackel, RP .
LASER-INDUCED DAMAGE IN OPTICAL MATERIALS: 2003, 2003, 5273 :296-302
[9]  
Runkel M. J., 2003, Proceedings of the SPIE - The International Society for Optical Engineering, V4932, P405, DOI 10.1117/12.472051
[10]   CARBON-DIOXIDE LASER POLISHING OF FUSED-SILICA SURFACES FOR INCREASED LASER-DAMAGE RESISTANCE AT 1064-NM [J].
TEMPLE, PA ;
LOWDERMILK, WH ;
MILAM, D .
APPLIED OPTICS, 1982, 21 (18) :3249-3255