Microstructure and mechanical performance of SiCf/BN/SiC mini-composites oxidized at elevated temperature from ambient temperature to 1500 °C in air

被引:48
|
作者
Lu, Zilong [1 ,2 ]
Yue, Jianfing [2 ,3 ]
Fu, Zeyu [2 ,3 ]
Huang, Xiaozhong [2 ,3 ]
Yang, Haitang [2 ,3 ]
机构
[1] Cent South Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Cent South Univ, Sch Aeronaut & Astronaut, Changsha 410083, Hunan, Peoples R China
[3] Cent South Univ, Hunan Prov Key Lab New Specialty Fibers & Composi, Changsha 410083, Hunan, Peoples R China
关键词
SiCf/BN/SiC; Minicomposites; B2O3; Mechanical performance; Microstructure evolution; CERAMIC-MATRIX COMPOSITES; SIC/SIC MINICOMPOSITES; DIELECTRIC-PROPERTIES; SICF/SIC COMPOSITES; OXIDATION; INTERPHASE; RESISTANCE; BEHAVIOR; SYSTEM; DAMAGE;
D O I
10.1016/j.jeurceramsoc.2019.04.013
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
SiCf/BN/SiC mini-composites comprising single tow SiC fibre-reinforced SiC with chemical vapour deposited (CVD) BN interface layers were fabricated. The mechanical performance and binding strength of the composites and the fibre/interface for the oxidized SiCf/BN/SiC mini-composite samples (oxidation at 1000, 1200, 1300, 1400 and 1500 degrees C in air for two hours) were investigated by tensile tests and fibre push-out tests, respectively. The value of oxidation mass change was also measured. Some unusual phenomena for the SiCf/BN/SiC minicomposites oxidized at 1000 degrees C were discovered in this work. The tensile strength reached a maximum value, and the mass gain rate showed as a singular negative value, while the shear strength between the fibre and the matrix was moderate. Scanning electron microscopy, energy dispersive spectrometry, infrared spectroscopy and X-ray diffraction characterization methods were used to reveal the microstructural evolution and investigate the unusual phenomenon during oxidation procedures. This work will provide guidance for predicting the service life of SiCf/BN/SiC composite materials and may enable these materials to become a backbone for thermal structure systems in aerospace applications.
引用
收藏
页码:2821 / 2827
页数:7
相关论文
共 41 条
  • [31] Influence of the SiC matrix introduction time on the microstructure and mechanical properties of Cf/Hf0.5Zr0.5C-SiC ultra-high temperature composites
    Liu, Rongjun
    Yang, Lingwei
    Miao, Huaming
    Jiang, Minshu
    Wang, Yanfei
    Liu, Xingyu
    Wan, Fan
    CERAMICS INTERNATIONAL, 2022, 48 (03) : 3762 - 3770
  • [32] Effect of carbon on the microstructure and sliding wear performance of CoCrMo matrix composites from room temperature to 1000 °C
    Cui, Gongjun
    Li, Sai
    Liu, Huiqiang
    Gao, Guijun
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (05): : 4778 - 4787
  • [33] Effects of high-temperature heat treatment on the microstructure and mechanical performance of hybrid Cf-SiCf-(Al2O3p) reinforced geopolymer composites
    Yan, Shu
    He, Peigang
    Jia, Dechang
    Wang, Jinyan
    Duan, Xiaoming
    Yang, Zhihua
    Wang, Shengjin
    Zhou, Yu
    COMPOSITES PART B-ENGINEERING, 2017, 114 : 289 - 298
  • [34] Microstructure and mechanical properties of 2D laminated C/C-SiC composites prepared by low-temperature reactive melt infiltration with silicon alloy
    Qin, Qianhui
    Han, Yangjie
    Zeng, Yuke
    Cai, Meixia
    Li, Song
    Xiao, Zhichao
    Xia, Hongyan
    Wang, Jiping
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2025, 45 (06)
  • [35] High-temperature mechanical properties and microstructure of 2.5D C/ C-SiC composites applied for the brake disc of high-speed train
    Yang, Liting
    Xu, Ping
    Yang, Chengxing
    Guo, Weinian
    Yao, Shuguang
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (14)
  • [36] High-temperature mechanical properties and microstructure of C/C-ZrC-SiC-ZrB2 composites prepared by a joint process of precursor infiltration and pyrolysis and slurry infiltration
    Jia, Yan
    Chen, Si'an
    Li, Yong
    Wang, Song
    Hu, Haifeng
    JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 811
  • [37] Mechanical properties of ZrB2/SiC/WC ceramic tool materials from room temperature to 1100 °C and cutting performance
    Zhang, Jingbao
    Xiao, Guangchun
    Yi, Mingdong
    Chen, Zhaoqiang
    Zhang, Jingjie
    Chen, Hui
    Shang, Xizuo
    Xu, Chonghai
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2021, 101 (101):
  • [38] Interface design and HfC additive to enhance the cyclic ablation performance of SiC coating for carbon/carbon composites from 1750 °C to room temperature under vertical oxyacetylene torch
    Zhang, Jia-Ping
    Fu, Qian-Gang
    Wang, Yong-Jie
    CORROSION SCIENCE, 2017, 123 : 139 - 146
  • [39] SYNTHESIS AND TRANSFORMATION OF TETRACALCIUM PHOSPHATE IN SOLID-STATE .4. TRANSFORMATIONS OF CA4P2O9 OCCURRING WHILE HEATED IN AIR WITHIN THE TEMPERATURE-RANGE FROM AMBIENT TO 1500-DEGREES-C
    CIESLA, K
    RUDNICKI, R
    POLISH JOURNAL OF CHEMISTRY, 1989, 63 (1-3) : 83 - 91
  • [40] Tribological performance of TiAl matrix self-lubricating composites containing Ag, Ti3SiC2 and BaF2/CaF2 tested from room temperature to 600 °C
    Shi, Xiaoliang
    Yao, Jie
    Xu, Zengshi
    Zhai, Wenzheng
    Song, Siyuan
    Wang, Mang
    Zhang, Qiaoxin
    MATERIALS & DESIGN, 2014, 53 : 620 - 633