Effect of surface dissolution on flotation separation of fine ilmenite from titanaugite

被引:128
作者
Zhu Yang-ge [1 ]
Zhang Guo-fan [1 ]
Feng Qi-ming [1 ]
Yan Dai-cui [1 ]
Wang Wei-qing [1 ]
机构
[1] Cent S Univ, Sch Resources Proc & Bioengn, Changsha 410083, Hunan, Peoples R China
关键词
ilmenite; titanaugite; flotation; surface dissolution;
D O I
10.1016/S1003-6326(11)60835-2
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The influence of surface dissolution on flotation separation of fine ilmenite from titanaugite was investigated through infrared spectroscopic (FT-IR) analysis and X-ray photoelectron spectroscopy (XPS) test. The results show that surface dissolution in weak acid solution is helpful to enlarge the floatability difference between ilmenite and titanaugite. In weak acidic solution, as sodium oleate mainly interacts with Fe which results in ilmenite flotation, and surface dissolution is beneficial to its oxidation, the floatability of ilmenite after surface dissolution is increased; meanwhile, sodium oleate interacts with Ca and Mg which results in titanaugite flotation, and the quantities of Ca and Mg on the surface of titanautite are decreased due to the surface dissolution, so the floatability of titanaugite after surface dissolution is depressed. For an ilmenite ore obtained from Panzhihua with TiO(2) grade of 8.41%, flotation after surface dissolution treatment could increase TiO(2) grade of rough concentrate from 26.7% to 31.73%.
引用
收藏
页码:1149 / 1154
页数:6
相关论文
共 23 条
[21]  
Zhu J.G., 2006, MIN METALL ENG, P78
[22]  
Zhu Yang-ge, 2009, Chinese Journal of Nonferrous Metals, V19, P554
[23]  
[邹建新 ZOU Jianxin], 2006, [矿冶工程, Mining and Metallurgical Engineering], V26, P38