Spatially resolved X-ray diffraction mapping of phase transformations in the heat-affected zone of carbon-manganese steel arc welds

被引:57
作者
Elmer, JW [1 ]
Wong, J
Ressler, T
机构
[1] Lawrence Livermore Natl Lab, Chem & Mat Sci Directorate, Livermore, CA 94551 USA
[2] Fritz Haber Inst, Dept Inorgan Chem, D-14195 Berlin, Germany
来源
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 2001年 / 32卷 / 05期
关键词
D O I
10.1007/s11661-001-0127-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Phase transformations that occur in the heat-affected zone (HAZ) of gas tungsten are welds in AISI 1005 carbon-manganese steel were investigated using spatially resolved X-ray diffraction (SRXRD) at the Stanford Synchrotron Radiation Laboratory. In situ SRXRD experiments were performed to probe the phases present in the HAZ during welding of cylindrical steel bars. These real-time observations of the phases present in the HAZ were used to construct a phase transformation map that identifies five principal phase regions between the liquid weld pool and the unaffected base metal: (1) alpha -ferrite that is undergoing annealing, recrystallization, and/or grain growth at subcritical temperatures, (2) partially transformed alpha -ferrite co-existing with gamma -austenite at intercritical temperatures, (3) single-phase gamma -austenite at austenitizing temperatures, (4) delta -ferrite at temperatures near the liquidus temperature, and (5) back transformed alpha -ferrite co-existing with residual austenite at subcritical temperatures behind the weld. The SRXRD experimental results were combined with a heat flow model of the weld to investigate transformation kinetics under both positive and negative temperature gradients in the HAZ. Results show that the transformation from ferrite to austenite on heating requires 3 seconds and 158 degreesC of superheat to attain completion under a heating rate of 102 degreesC/s. The reverse transformation from austenite to ferrite on cooling was shown to require 3.3 seconds at a cooling rate of 45 degreesC/s to transform the majority of the austenite back to ferrite; however, some residual austenite was observed in the microstructure as far as 17 mm behind the weld.
引用
收藏
页码:1175 / 1187
页数:13
相关论文
共 31 条
[1]  
[Anonymous], 1992, Smithells Metals Reference Book, V7
[2]   THE TRANSFORMATION HARDENING OF STEEL SURFACES BY LASER-BEAMS .1. HYPO-EUTECTOID STEELS [J].
ASHBY, MF ;
EASTERLING, KE .
ACTA METALLURGICA, 1984, 32 (11) :1935-&
[3]   A 1ST REPORT ON DIAGRAMS FOR GRAIN-GROWTH IN WELDS [J].
ASHBY, MF ;
EASTERLING, KE .
ACTA METALLURGICA, 1982, 30 (11) :1969-1978
[4]  
*ASM INT, 1979, MET HDB, V3
[5]  
BABU SS, 1994, PROCEEDINGS OF AN INTERNATIONAL CONFERENCE ON SOLID - SOLID PHASE TRANSFORMATIONS, P213
[6]   DEVELOPMENT OF MACROSTRUCTURE AND MICROSTRUCTURE OF CARBON-MANGANESE LOW-ALLOY STEEL WELDS - INCLUSION FORMATION [J].
BABU, SS ;
DAVID, SA ;
VITEK, JM ;
MUNDRA, K ;
DEBROY, T .
MATERIALS SCIENCE AND TECHNOLOGY, 1995, 11 (02) :186-199
[7]   REEVALUATION OF X-RAY ATOMIC ENERGY LEVELS [J].
BEARDEN, JA ;
BURR, AF .
REVIEWS OF MODERN PHYSICS, 1967, 39 (01) :125-&
[8]   HEAT TREATING AND MELTING MATERIAL WITH A SCANNING LASER OR ELECTRON-BEAM [J].
CLINE, HE ;
ANTHONY, TR .
JOURNAL OF APPLIED PHYSICS, 1977, 48 (09) :3895-3900
[9]  
CLLITY BD, 1956, ELEMENTS XRAY DIFFRA, P263
[10]  
EAGAR TW, 1983, WELD J, V62, pS346