The effect of TiSiN interlayers on the bond strength of ceramic to NiCr and CoCr alloys

被引:22
作者
Vladescu, A. [1 ]
Dinu, M. [1 ,2 ]
Braic, M. [1 ]
Vitelaru, C. [1 ]
Balaceanu, M. [1 ]
Tarcolea, M. [2 ]
Braic, V. [1 ]
Baciu, F. [2 ]
Cotrut, C. M. [2 ]
机构
[1] Natl Inst Optoelect, Magurele, Romania
[2] Univ Politehn Bucuresti, Bucharest, Romania
关键词
Films; Interfaces; Mechanical properties; Porcelain; Nitrides; GOLD ALLOY; MECHANICAL-PROPERTIES; PORCELAIN ADHERENCE; FLEXURAL STRENGTH; GLASS-CERAMICS; TITANIUM; SURFACE; TIN; INTERFACES; COATINGS;
D O I
10.1016/j.ceramint.2015.03.001
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
High bonding between the NiCr or CoCr alloys and the ceramic layer is essential for the clinical success of dental prostheses restorations. Aiming to enhance the bond strength between metal and dental ceramics in prosthetic restorations, TiSiN coatings were deposited as interlayers. The coatings were deposited on NiCr and CoCr dental alloys by using the cathodic arc technique at various substrate bias voltage values and characterized in terms of elemental composition, crystalline structure, mechanical properties, surface roughness and contact angle. The bond strength of the metal ceramic system, with and without TiSiN interlayers, was evaluated by using a three-point bending test. The coatings consisted of nanocrystalline solid solutions (grain sizes of 3.6-4.3 nm) with a face-centered cubic structure. The film hardness, ranging from approximately 21-38 GPa, was observed to increase with increasing substrate bias, irrespective of the substrate type. The best adhesion values (critical loads of similar to 54 N) were obtained on both substrates for coatings deposited at of -100 V bias voltage. The deposition of the TiSiN coatings determined the roughness decrease of both NiCr and CoCr coated alloys. The contact angle measurements indicated a hydrophobic character for the films deposited at bias voltages ranging from -50 to -150 V and a hydrophilic character at a bias of -200 V. The results indicated that TiSiN coatings improved the bond strength of NiCr ceramic systems. Based on these results an increase of the clinical service life of the dental restorations having a TiSiN interlayer between the metallic support and the ceramic layer is expected. (C) 2015 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
引用
收藏
页码:8051 / 8058
页数:8
相关论文
共 63 条
[1]   Effects of airborne-particle abrasion, sodium hydroxide anodization, and electrical discharge machining on porcelain adherence to cast commercially pure titanium [J].
Acar, Asli ;
Inan, Ozgur ;
Halkaci, Selcuk .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2007, 82B (01) :267-274
[2]   Effect of surface treatment on bond strength of low-fusing porcelain to commercially pure titanium [J].
Al Hussaini, I ;
Al Wazzan, KA .
JOURNAL OF PROSTHETIC DENTISTRY, 2005, 94 (04) :350-356
[3]   Microstructural Evidence of Beryllium in Commercial Dental Ni-Cr Alloys [J].
Alkmin, Luciano Braga ;
Araujo Pinto da Silva, Antonio Augusto ;
Nunes, Carlos Angelo ;
dos Santos, Claudinei ;
Coelho, Gilberto Carvalho .
MATERIALS RESEARCH-IBERO-AMERICAN JOURNAL OF MATERIALS, 2014, 17 (03) :627-631
[4]   Study of TiN and ZrN thin films grown by cathodic arc technique [J].
Arias, D. F. ;
Arango, Y. C. ;
Devia, A. .
APPLIED SURFACE SCIENCE, 2006, 253 (04) :1683-1690
[5]   Effect of silicon content on PVD film mechanical properties and cutting performance of coated cemented carbide inserts [J].
Bouzakis, K. -D. ;
Bouzakis, E. ;
Kombogiannis, S. ;
Paraskevopoulou, R. ;
Skordaris, G. ;
Makrimallakis, S. ;
Katirtzoglou, G. ;
Pappa, M. ;
Gerardis, S. ;
M'Saoubi, R. ;
Andersson, J. M. .
SURFACE & COATINGS TECHNOLOGY, 2013, 237 :379-389
[6]  
Braic M, 2005, J OPTOELECTRON ADV M, V7, P671
[7]  
BUNSHAH RF, 1995, HDB DEPOSITION TECHN
[8]   Evaluation of interface characterization and adhesion of glass ceramics to commercially pure titanium and gold alloy after thermal- and mechanical-loading [J].
Ccahuana Vasqueza, Vanessa Zulema ;
Ozcan, Mutlu ;
Kimpara, Estevao Tomomitsu .
DENTAL MATERIALS, 2009, 25 (02) :221-231
[9]   Bonding agents of low fusing cpTi porcelains: Elemental and morphological characterization [J].
Chakmakchi, Makdad ;
Eliades, George ;
Zinelis, Spiros .
JOURNAL OF PROSTHODONTIC RESEARCH, 2009, 53 (04) :166-171
[10]   Influence of bias voltages on the structure and wear properties of TiSiN coating synthesized by cathodic arc plasma evaporation [J].
Chang, Chi-Lung ;
Lin, Chao-Te ;
Tsai, Pi-Chuen ;
Ho, Wei-Yu ;
Wang, Da-Yung .
THIN SOLID FILMS, 2008, 516 (16) :5324-5329