共 50 条
Surface modification of La0.3Sr0.7C0O3-δ ceramic membranes
被引:81
|作者:
Kharton, VV
Kovalevsky, A
Yaremchenko, AA
Figueiredo, FM
Naumovich, EN
Shaulo, AL
Marques, FMB
机构:
[1] Belarusian State Univ, Inst Physicochim Problems, Minsk 220080, BELARUS
[2] Univ Aveiro, UIMC, Dept Ceram & Glass Engn, P-3810193 Aveiro, Portugal
关键词:
ceramic membrane;
surface activation;
oxygen permeation;
ionic transport;
mixed conductivity;
D O I:
10.1016/S0376-7388(01)00567-1
中图分类号:
TQ [化学工业];
学科分类号:
0817 ;
摘要:
The dependence of oxygen permeability of dense La0.3Sr0.7CoO3-delta ceramics on membrane thickness indicates significant surface exchange limitations to the permeation fluxes, which suggests a possibility to increase membrane performance by surface activation. The cobaltite membranes with various porous layers applied onto the permeate-side surface were tested at 850-1120 K, Silver-modified La0.3Sr0.7CoO3-delta membranes showed enhanced permeation at temperatures above 950 K; deposition of porous layers of PrOx and Pr0.7Sr0.3CoO3-delta had no positive effect. The maximum oxygen permeability at. These results 850-1120 K was observed in the case of porous La0.3Sr0.7CoO3-delta layers with surface density about 10 mg cm(-2) suggest that the surface exchange of lanthanum-strontium cobaltite membranes under an oxygen chemical potential gradient is limited by both oxygen sorption at the surface and ion diffusion through the surface oxide layers. Oxygen permeability of La0.3Sr0.7CoO3-delta ceramics was found to increase with increasing grain size due to decreasing grain-boundary resistance to ionic transport. (C) 2002 Elsevier Science B.V. All rights reserved.