Activation of silicon implanted with phosphorus atoms by infrared semiconductor laser annealing

被引:11
作者
Sameshima, Toshiyuki [1 ]
Maki, Masato
Takiuchi, Megumu
Andoh, Nobuyuki
Sano, Naoki
Matsuda, Yasuhiro
Andoh, Yasunori
机构
[1] Tokyo Univ Agr & Technol, Koganei, Tokyo 1848588, Japan
[2] Hightec Syst Corp, Yokohama, Kanagawa 2220033, Japan
[3] Nissin Ion Equip Co Ltd, Koka, Shiga 5280068, Japan
来源
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS | 2007年 / 46卷 / 10A期
关键词
DLC; mobility; carrier density; rapid annealing;
D O I
10.1143/JJAP.46.6474
中图分类号
O59 [应用物理学];
学科分类号
摘要
We activated silicon implanted with phosphorus atoms by infrared semiconductor laser annealing with a diamond-like carbon (DLC) optical absorption layer. The silicon samples implanted with phosphorus atoms at 10 and 70 keV with concentrations of 5 x 10(14), 1 X 10(15), and 2 x 10(15) cm(-2) were coated with 200-nm-thick DLC films. The samples were annealed by irradiation with a 940 nm continuous wave laser at 70 kW/cm(2) with a beam diameter of 180 mu m. The laser beam was scanned using a moving stage at 3-20cm/s, which gave an effective dwell time of 0.9-6.0 ms. The amorphized surface regions were recrystallized by laser annealing longer than 1.2 ins. The in-depth profile of phosphorus concentration hardly changed within 5 nm for laser annealing for 2.6 ms. The sheet resistance markedly decreased to 106 and 46 Omega/sq for the samples implanted with phosphorus atoms at 10 and 70 keV by laser annealing at a dwell time of 2.6 ms, respectively. Phosphorus atoms were effectively activated with a carrier density near the phosphorus concentration for implantation at 70keV. A low carrier generation rate was observed for implantation at 2 x 10(15) cm(-2) and 10keV. An intermediate SiO2 layer effectively blocked carbon incorporation to a level below 10(17)cm(-3).
引用
收藏
页码:6474 / 6479
页数:6
相关论文
共 10 条
  • [2] GOTO K, 1909, IEDM, P931
  • [3] GROVE AS, 1967, PHYS TECHNOL S, pCH3
  • [4] Mehrotra M., 1999, International Electron Devices Meeting 1999. Technical Digest (Cat. No.99CH36318), P419, DOI 10.1109/IEDM.1999.824183
  • [5] Heating layer of diamond-like carbon films used for crystallization of silicon films
    Sameshima, T
    Andoh, N
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS BRIEF COMMUNICATIONS & REVIEW PAPERS, 2005, 44 (10): : 7305 - 7308
  • [6] Electrical properties of pulsed laser crystallized silicon films
    Sameshima, T
    Saitoh, K
    Aoyma, N
    Higashi, S
    Kondo, M
    Matsuda, A
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1999, 38 (4A): : 1892 - 1897
  • [7] SAMESHIMA T, 2004, MAT RES SOC S P, V849
  • [8] SAMESHIMA T, P WORKSH ACT MATR FL
  • [9] Sano N., 2006, Amorphous and Polycrystalline Thin-Film Silicon Science and Technology-2006. Symposium (Materials Research Society Symposium Proceedings Vol.910), P329
  • [10] Deposition and tribological behaviour of sputtered carbon hard coatings
    Yang, S
    Camino, D
    Jones, AHS
    Teer, DG
    [J]. SURFACE & COATINGS TECHNOLOGY, 2000, 124 (2-3) : 110 - 116