Delamination crack growth in thermal barrier coatings

被引:0
作者
Brodin, H [1 ]
Li, XH [1 ]
机构
[1] Linkoping Univ, Dept Mech Engn, Div Engn Mat, S-58183 Linkoping, Sweden
来源
THERMAL SPRAY 2004: ADVANCES IN TECHNOLOGY AND APPLICATION, PROCEEDINGS | 2004年
关键词
TBC; crack growth; delamination; fatigue; oxidation;
D O I
暂无
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Thermal barrier coatings (TBC) in general fail by delamination of the ceramic partially stabilised Zirconia (PSZ) top coat (TC) from the underlying metallic bond coat (BC). The process is initiated by crack initiation and growth either in the TC or in the thermally grown oxide (TGO) that will form at the interface between top and bond coat. The aim of the present paper is to describe the degradation due to crack growth in such a way that data can be used for FEM modelling work. Flat rectangular test coupons have been subjected to thermal cyclic fatigue (TCF) in air with a temperature range from 100 degrees C to 1100 degrees C. Identical samples were removed from the TCF furnace at different times of thermal cycling in order to achieve material with different degree of damage. After mounting, cutting and sectioning the specimen were investigated by light optical microscopy (LOM) and scanning electron microscopy (SEM) together with an energy dispersive spectrometer (EDS). Image analysis of LOM micrographs was used for measurement of crack distribution and degree of TC damage. A method for crack growth measurement based on the degree of TC / TGO damage has been developed. Furthermore, a measure of TBC damage as a function of elapsed fatigue cycles was introduced. The TBC material shows a mixed black and white fracture surface after TCF cycling. Delamination crack growth data are presented. Delaminated TC/BC interface surface as a function of fatigue cycles follows an S-curve behaviour.
引用
收藏
页码:1088 / 1091
页数:4
相关论文
共 50 条
[41]   A Simulation Study on the Crack Propagation Behavior of Nanostructured Thermal Barrier Coatings with Tailored Microstructure [J].
Zhang, Lei ;
Wang, Yu ;
Fan, Wei ;
Gao, Yuan ;
Sun, Yiwen ;
Bai, Yu .
COATINGS, 2020, 10 (08)
[42]   Mechanism of crack nucleation and growth in YSZ thermal barrier coatings corroded by CMAS at high temperatures: First-principles calculation [J].
Chen, Zheng ;
Zheng, Haizhong ;
Li, Guifa ;
Li, Hongxia ;
Peng, Ping .
CORROSION SCIENCE, 2018, 142 :258-265
[43]   Thermal fatigue failure induced by delamination in thermal barrier coating [J].
Zhou, YC ;
Hashida, T .
INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (2-4) :407-417
[44]   Analytical prediction model for fatigue crack propagation and delamination growth in Glare [J].
Alderliesten, R. C. .
INTERNATIONAL JOURNAL OF FATIGUE, 2007, 29 (04) :628-646
[45]   Effect of Thermal Growth Oxide Composition and Morphology on Local Stresses in Thermal Barrier Coatings [J].
Ding, Kunying ;
Zhang, Tao ;
Wang, Zhe ;
Yu, Jun ;
Guo, Wansen ;
Yang, Yifei .
MATERIALS, 2022, 15 (23)
[46]   Evaluation of TGO growth in thermal barrier coatings using impedance spectroscopy [J].
Huang Hui ;
Liu Chao ;
Ni Liyong ;
Zhou Chungen .
RARE METALS, 2011, 30 :643-646
[47]   Modelling and analysis of the oxide growth coupling behaviour of thermal barrier coatings [J].
Wang, Xiaokang ;
Fan, Xueling ;
Sun, Yongle ;
Xu, Rong ;
Jiang, Peng .
JOURNAL OF MATERIALS SCIENCE, 2019, 54 (14) :10270-10283
[48]   Calcium-magnesium-alumina-silicate (CMAS) delamination mechanisms in EB-PVD thermal barrier coatings [J].
Chen, X .
SURFACE & COATINGS TECHNOLOGY, 2006, 200 (11) :3418-3427
[49]   Coupling effect of delamination cracks and vertical cracks on local phase transition of ceramic topcoat in thermal barrier coatings [J].
Dong, Hui ;
Xu, Long ;
Zhou, Pan-Hu ;
Yang, Guan-Jun ;
Wang, Li-Shuang ;
Yao, Jian-Tao .
CERAMICS INTERNATIONAL, 2023, 49 (08) :13176-13184
[50]   Delamination Susceptibility of Coatings Under High Thermal Flux [J].
Xue, Z. ;
Evans, A. G. ;
Hutchinson, J. W. .
JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 2009, 76 (04) :1-7