Effect of high energy ball milling on strengthening of Cu-ZrO2 nanocomposites

被引:78
作者
Abu-Oqail, A. [1 ]
Wagih, A. [2 ]
Fathy, A. [2 ]
Elkady, O. [3 ]
Kabeel, A. M. [2 ]
机构
[1] Beni Suef Univ, Fac Ind Educ, Mech Dept, Bani Suwayf, Egypt
[2] Zagazig Univ, Fac Engn, Dept Mech Design & Prod Engn, POB 44519, Zagazig, Egypt
[3] Cent Met R&D Inst, Mfg Dept, Powder Met Div, PO 87, Cairo 11421, Egypt
关键词
Copper matrix composites; Microhardness; Mechanical milling; Scan electron microscope; MECHANICAL-PROPERTIES; FE SIMULATION; COPPER; MICROSTRUCTURE; ELECTRODEPOSITION; COMPRESSIBILITY; INDENTATION; COMPOSITES; STRAIN; SIZE;
D O I
10.1016/j.ceramint.2018.12.053
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this paper, copper matrix nanocomposites reinforced by 5 and 10 wt% ZrO2 particles were produced by mechanical milling technique at different milling times. The produced nanocomposite powders were investigated by X-ray diffraction technique and transmission electron microscopy. The effect of high energy ball milling on the morphology, microstructure and microhardness of the produced composites has been investigated. After that cold compaction was applied to the prepared powders under a pressure of 700 MPa and sintered at 950 degrees C for 2 h in hydrogen atmosphere. The results showed that increasing milling time improves microhardness of the prepared nanocomposites. The microhardness of Cu-10%ZrO2 after 20 h milling is 3.76 times larger than pure Cu. This improvement is attributed firstly to the presence of ZrO2 nanoparticles in addition to the improvement coming from the grain refinement and crystallite size reduction occurred due to mechanical alloying. So, in spite of the crystallite size of Cu-10%ZrO2 nanocomposite is reduced to 10.75 nm compared to 105.5 nm for pure Cu, the presence of ZrO2 nanoparticles plays a major role on mechanical properties improvement.
引用
收藏
页码:5866 / 5875
页数:10
相关论文
共 47 条
  • [41] Processing of Cu-Al2O3 metal matrix nanocomposite materials by using high energy ball milling
    Ying, DY
    Zhang, DL
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 286 (01): : 152 - 156
  • [42] Preparation by mechanical alloying, characterization and sintering of Cu-20 wt.% Al2O3 nanocomposites
    Zawrah, M. F.
    Zayed, Hamdia A.
    Essawy, Raghieba A.
    Nassar, Amira H.
    Taha, Mohammed A.
    [J]. MATERIALS & DESIGN, 2013, 46 : 485 - 490
  • [43] Microstructure evaluation of Al-Al2O3 composite produced by mechanical alloying method
    Zebarjad, SM
    Sajjadi, SA
    [J]. MATERIALS & DESIGN, 2006, 27 (08): : 684 - 688
  • [44] Processing Ti3Al-SiC nanocomposites using high energy mechanical milling
    Zhang, DL
    Liang, J
    Wu, J
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2004, 375 : 911 - 916
  • [45] Processing of advanced materials using high-energy mechanical milling
    Zhang, DL
    [J]. PROGRESS IN MATERIALS SCIENCE, 2004, 49 (3-4) : 537 - 560
  • [46] Electrodeposition of Ni matrix composite coatings containing ZrC particles
    Zhang, Z.
    Wu, X.
    Jiang, C.
    Ma, N.
    [J]. SURFACE ENGINEERING, 2014, 30 (01) : 21 - 25
  • [47] Critical grain size for nanocrystalline-to-amorphous phase transition in Al solid solution
    Zhang, Zhihui
    Li, Ying
    Vogt, Rustin
    Zhou, Yizhang
    Schoenung, Julie M.
    Lavernia, Enrique J.
    [J]. PHILOSOPHICAL MAGAZINE LETTERS, 2012, 92 (05) : 235 - 244