Effects of solder thickness on interface behavior and nanoindentation characteristics in Cu/Sn/Cu microbumps

被引:129
作者
Zhang, Zhiyuan [1 ]
Chen, Jieshi [1 ,2 ,3 ]
Wang, Jianing [1 ]
Han, Yuzhu [1 ]
Yu, Zhiyuan [3 ]
Wang, Qinzhao [4 ]
Zhang, Peilei [1 ,2 ]
Yang, Shanglei [1 ,2 ]
机构
[1] Shanghai Univ Engn Sci, Sch Mat Engn, Shanghai 201620, Peoples R China
[2] Shanghai Collaborat Innovat Ctr Laser Adv Mfg Tec, Shanghai 201620, Peoples R China
[3] Shanghai Jiao Tong Univ, Sch Mat Sci & Engn, Shanghai 200240, Peoples R China
[4] Shanghai Sany Heavy Machinery Co Ltd, Shanghai 200241, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Cu; Sn; Cu microbumps; Solder thickness; IMCs; Binary diffusion; Nanoindentation; SN INTERMETALLIC COMPOUND; PB-FREE SOLDER; MECHANICAL-PROPERTIES; CU-SN; IMC GROWTH; CU6SN5; EVOLUTION; SOLIDIFICATION; CU3SN;
D O I
10.1007/s40194-022-01261-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The thickness of the solder, for Cu/Sn/Cu microbumps with dimensions of tens of microns or even a few microns (such as 40 mu m, 15 mu m, 10 mu m, and 6 mu m), can have a significant effect on the interfacial transfer and the performance. During the reflow stage, it was found that the grains of Cu6Sn5 showed "staggered growth" phenomenon in some areas of the microbumps with the solder thickness of 6 mu m and the thickness of intermetallic compounds' (IMCs) layer grew the fastest; that the second fastest growth of 40 mu m; that the third fastest growth of 15 mu m, and that the slowest growth of 10 mu m. After thermal aging at 160 degrees C for 80 h, the thickness of the IMC layer in descending order was the microbumps with the solder thickness of 15 mu m, 10 mu m, 40 mu m, and 6 mu m. These results were caused by the difference in the element concentration. In addition, there were four main components in the microbumps: Cu, Sn, Cu6Sn5, and Cu3Sn. The hardness of Cu and Sn was about 1.37 +/- 0.3 Gpa and 0.13 +/- 0.03 Gpa, respectively. And the hardness of Cu6Sn5 and Cu3Sn was about 6.7 +/- 0.3 Gpa and 6.2 +/- 0.4 Gpa, respectively. The nanoindentation hardness analysis showed a general increase in the hardness of the microbumps after thermal aging for 80 h, compared with that after reflow. And the thinner the solder thickness was, the more obvious the hardness improvement was.
引用
收藏
页码:973 / 983
页数:11
相关论文
共 41 条
[1]   Cu/Sn Microbumps Interconnect for 3D TSV Chip Stacking [J].
Agarwal, Rahul ;
Zhang, Wenqi ;
Limaye, Paresh ;
Labie, Riet ;
Dimcic, Biljana ;
Phommahaxay, Alain ;
Soussan, Philippe .
2010 PROCEEDINGS 60TH ELECTRONIC COMPONENTS AND TECHNOLOGY CONFERENCE (ECTC), 2010, :858-863
[2]   Determination of the elastic properties of Cu3Sn through first-principles calculations [J].
An, Rong ;
Wang, Chunqing ;
Tian, Yanhong ;
Wu, Huaping .
JOURNAL OF ELECTRONIC MATERIALS, 2008, 37 (04) :477-482
[3]   Growth kinetic studies of Cu-Sn intermetallic compound and its effect on shear strength of LCCC SMT solder joints [J].
Chan, YC ;
So, ACK ;
Lai, JKL .
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 1998, 55 (1-2) :5-13
[4]   The Zn accumulation behavior, phase evolution and void formation in Sn-xZn/Cu systems by considering trace Zn: a combined experimental and theoretical study [J].
Chen, Jieshi ;
Zhang, Honglzui ;
Zhang, Peilei ;
Yu, Zhishui ;
Zhang, Yongzhi ;
Yu, Chun ;
Lu, Hao .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2019, 8 (05) :4141-4150
[5]   Effect of substrates on the formation of Kirkendall voids in Sn/Cu joints [J].
Chen, Jieshi ;
Yang, Jin ;
Zhang, Yongzhi ;
Yu, Zhishui ;
Zhang, Peilei .
WELDING IN THE WORLD, 2019, 63 (03) :751-757
[6]   Interface Growth and Void Formation in Sn/Cu and Sn0.7Cu/Cu Systems [J].
Chen, Jieshi ;
Zhang, Yongzhi ;
Yu, Zhishui ;
Zhang, Peilei ;
Zhao, Wanqin ;
Yang, Jin ;
Wu, Di .
APPLIED SCIENCES-BASEL, 2018, 8 (12)
[7]   Nanoindentation measurements on Cu-Sn and Ag-Sn intermetallics formed in Pb-free solder joints [J].
Chromik, RR ;
Vinci, RP ;
Allen, SL ;
Notis, MR .
JOURNAL OF MATERIALS RESEARCH, 2003, 18 (09) :2251-2261
[8]   Measuring the mechanical properties of Pb-free solder and Sn-based intermetallics by nanoindentation [J].
Chromik, RR ;
Vinci, RP ;
Allen, SL ;
Notis, MR .
JOM-JOURNAL OF THE MINERALS METALS & MATERIALS SOCIETY, 2003, 55 (06) :66-69
[9]   Deformation behavior of (Cu, Ag)-Sn intermetallics by nanoindentation [J].
Deng, X ;
Chawla, N ;
Chawla, KK ;
Koopman, M .
ACTA MATERIALIA, 2004, 52 (14) :4291-4303
[10]   Phase-field study of IMC growth in Sn-Cu/Cu solder joints including elastoplastic effects [J].
Durga, A. ;
Wollants, P. ;
Moelans, N. .
ACTA MATERIALIA, 2020, 188 :241-258