Impact of crystallization firing process on the microstructure and flexural strength of zirconia-reinforced lithium silicate glass-ceramics

被引:66
作者
Riquieri, Hilton [1 ]
Monteiro, Jaiane Bandoli [1 ]
Viegas, Diogo Cabecinha [2 ]
Bastos Campos, Tiago Moreira [3 ]
de Melo, Renata Marques [1 ]
Ferreira Anzaloni Saavedra, Guilherme de Siqueira [1 ]
机构
[1] Sao Paulo State Univ UNESP, Dept Dent Mat & Prosthodont, Inst Sci & Technol, 777 Engn Francisco Jose Longo Ave, BR-12245000 Sao Jose Dos Campos, SP, Brazil
[2] Lisbon Univ, Fac Med Dent, P-1649003 Lisbon, Portugal
[3] Aeronaut Technol Inst ITA, 50 Praca Marechal Eduardo Gomes, BR-12228900 Sao Jose Dos Campos, SP, Brazil
关键词
Dental materials; Dental ceramics; Computer-aided manufacturing; Biaxial flexural strength; DENTAL CERAMICS; WEAR;
D O I
10.1016/j.dental.2018.06.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The aim of this study was to characterize the microstructure of two zirconia-reinforced lithium silicate (ZLS) glass-ceramics and evaluate their mechanical properties before and after the crystallization firing process (CFP). Methods. Field emission-scanning electron microscope (FE-SEM) and energy-dispersive X-ray spectroscopy (EDS) analyses were performed for microstructural characterization. To evaluate the pattern of crystallization and the molecular composition of ZLS glass-ceramics, was used X-ray diffraction (XRD). Vickers hardness, fracture toughness by the indentation method, and biaxial flexural strength were also measured. One hundred and forty ceramic discs were produced (diameter = 12 mm; thickness = 1.2 mm) and allocated among four groups (n = 30): Sfir, Sunf-ZLS Vita Suprinity; and Cfir and Cunf-ZLS Celtra Duo; fired and unfired, respectively. Statistical analysis was performed and Weibull failure probabilities were calculated. Results. Cfir showed the highest characteristic strength (251.25 MPa) and hardness (693.333 +/- 10.85 GPa). Conversely, Sunf presented the lowest characteristic strength (106.95 MPa) and significantly lowest hardness (597.533 +/- 33.97 GPa). According to Weibull analysis, Sunf had the highest structural reliability (m = 7.07), while Sfir presented the lowest (m = 5.38). The CFP was necessary to crystallize zirconia in the partially crystallized ZLS glass-ceramics. Sfir had a lower percentage of crystallized zirconia than did Cfir. Fracto-graphic analyses showed that all failures initiated from an inherent critical defect in Sunf and from processing defects in the remaining groups. Significance. The CFP had a direct influence on the flexural strength and microstructural characteristics of both ZLS materials. (C) 2018 The Academy of Dental Materials. Published by Elsevier Inc. All rights reserved.
引用
收藏
页码:1483 / 1491
页数:9
相关论文
共 25 条
[1]  
[Anonymous], [No title captured]
[2]  
[Anonymous], 2010, 1607 JISR
[3]  
[Anonymous], ISO6872
[4]  
[Anonymous], 2012, INSTR MAN
[5]  
[Anonymous], ISO15732
[6]  
ASTM International, 2015, STAND TEST METH VICK
[7]  
Aurelio IL, 2017, DENT MATER, V33, P226
[8]   Chairside CAD/CAM materials. Part 1: Measurement of elastic constants and microstructural characterization [J].
Belli, Renan ;
Wendler, Michael ;
de Ligny, Dominique ;
Cicconi, Maria Rita ;
Petschelt, Anselm ;
Peterlik, Herwig ;
Lohbauer, Ulrich .
DENTAL MATERIALS, 2017, 33 (01) :84-98
[9]   Effect of the microstructure on the lifetime of dental ceramics [J].
Borba, Marcia ;
de Araujo, Maico D. ;
Fukushima, Karen A. ;
Yoshimura, Humberto N. ;
Cesar, Paulo F. ;
Griggs, Jason A. ;
Della Bona, Alvaro .
DENTAL MATERIALS, 2011, 27 (07) :710-721
[10]  
Celtra Duo, 2014, CELTRA BLOCK CEREC I