Pressure acid leaching of arid-region nickel laterite ore Part IV: Effect of acid loading and additives with nontronite ores

被引:19
作者
Johnson, JA [1 ]
McDonald, RG [1 ]
Muir, DM [1 ]
Tranne, JP [1 ]
机构
[1] CSIRO Minerals, AJ Parker CRC Hydromet, Bentley, WA 6982, Australia
关键词
nickel laterite; pressure acid leaching; nontronite; acid loading; salinity;
D O I
10.1016/j.hydromet.2005.04.002
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The extraction of nickel from nontronite-rich laterite ores is enhanced by either increasing the acid loading, or the addition of a small amount of sodium to the process water. The results of this study indicate that at least 15% less acid can be used to get the same extraction of nickel from a nontronite-rich laterite ore in process water containing 5 g/L sodium ion, compared with the same ore in fresh process water. In addition, nickel extractions from a second nontronite-rich laterite ore were increased by up to 3% compared with fresh water, if process water sodium ion levels is present at 5-11 g/L at a given acid loading of 420 kg/t ore. Crown Copyright (c) 2005 Published by Elsevier B.V. All rights reserved.
引用
收藏
页码:264 / 270
页数:7
相关论文
共 14 条
  • [1] Adams M, 2004, INTERNATIONAL LATERITE NICKEL SYMPOSIUM-2004, P193
  • [2] BUARZAIGA M, 2004, PRESSURE HJYDROMETAL, P181
  • [3] JOHNSON IA, 2002, CHLORIDE METALLURGY, P339
  • [4] Johnson J.A., 2004, PRESSURE HYDROMETALL, P199
  • [5] JOHNSON JA, IN PRESS MINERALS EN
  • [6] KRAUSE E, 1997, HYDROMETALLURGY REFI, V1, P441
  • [7] MADSEN IC, 2005, UNPUB PRESSURE ACID
  • [8] Marshall D, 2004, INTERNATIONAL LATERITE NICKEL SYMPOSIUM-2004, P263
  • [9] Papangelakis V.G., 1996, IRON CONTROL HYDROME, P263
  • [10] Torres VM, 2004, INTERNATIONAL LATERITE NICKEL SYMPOSIUM-2004, P203