Mesoporous gadolinium doped titania photocatalyst through an aqueous sol-gel method

被引:36
作者
Baiju, K. V. [1 ,2 ]
Periyat, P. [3 ]
Shajesh, P. [1 ]
Wunderlich, W. [4 ]
Manjumol, K. A. [1 ]
Smitha, V. S. [1 ]
Jaimy, K. B. [1 ]
Warrier, K. G. K. [1 ]
机构
[1] CS1R, NIIST, Mat & Minerals Div, Thiruvananthapuram 695019, Kerala, India
[2] Northwestern Univ, Inst Catalysis & Energy Proc, Evanston, IL 60208 USA
[3] Univ Limerick, MSSI, Limerick, Ireland
[4] Tokai Univ, Fac Engr, Dept Mat Sci, Kanagawa 2591292, Japan
关键词
Sol-gel; Titanyl oxysulphate; Photocatalyst; Anatase; Mesoporous; RARE-EARTH; PHASE-TRANSFORMATION; ANATASE PHASE; THIN-FILMS; TIO2; DIOXIDE; KINETICS; OXIDATION; LANTHANA; PHOTOACTIVITY;
D O I
10.1016/j.jallcom.2010.06.028
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
A surfactant-free, aqueous sol-gel synthetic route to a thermally stable gadolinium doped mesoporous nanocrystalline titania is reported for the first time. The mesoporosity was revealed using BET surface area measurements and the pores are stable at temperatures as high as 800 degrees C. The 2 mol% gadolinium doped titania calcined at 800 degrees C, displayed a specific surface area of 22 m(2) g(-1) and a total pore volume 0.142 cm(3) g(-1), whereas undoped titania is non-porous and has a surface area value as low as 0.3364 m(2) g(-1) and total pore volume of 0.00096 cm(3) g(-1). The thermal stability of the anatase phase up to 800 degrees C was achieved due to the reduction of crystallite size as a result of gadolinium doping in the titania lattice. Transmission electron micrographs showed that the crystallite size of 2 mol% gadolinium doped titania is 20 nm at 800 degrees C. whereas undoped titania had a crystallite size of 43 nm at the same temperature. The Bronsted acidity of doped titania was further studied using 2,6-dimethyl pyridine adsorption studies. Finally the photocatalytic performance of this mesoporous TiO2 was analysed using methylene blue degradation and revealed a significantly higher activity than the undoped titania, a factor attributed to the mesoporosity, higher surface area and thermal stability of anatase phase. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:194 / 200
页数:7
相关论文
共 61 条
[1]   Structural effects of codoping of Nb and Sc in titanium dioxide nanoparticles [J].
Ahmad, Akhlaq ;
Shah, Jawad Ali ;
Buzby, Scott ;
Shah, Syed Ismat .
EUROPEAN JOURNAL OF INORGANIC CHEMISTRY, 2008, (06) :948-953
[2]   The design and development of highly reactive titanium oxide photocatalysts operating under visible light irradiation [J].
Anpo, M ;
Takeuchi, M .
JOURNAL OF CATALYSIS, 2003, 216 (1-2) :505-516
[4]   Spectroscopic characterization of the acid properties of metal oxide catalysts [J].
Busca, G .
CATALYSIS TODAY, 1998, 41 (1-3) :191-206
[5]   Enhancement of titania by doping rare earth for photodegradation of organic dye (Direct Blue) [J].
El-Bahy, Zeinhom M. ;
Ismail, Adel A. ;
Mohamed, Reda M. .
JOURNAL OF HAZARDOUS MATERIALS, 2009, 166 (01) :138-143
[6]   Visible and near-IR luminescence via energy transfer in rare earth doped mesoporous titania thin films with nanocrystalline walls [J].
Frindell, KL ;
Bartl, MH ;
Robinson, MR ;
Bazan, GC ;
Popitsch, A ;
Stucky, GD .
JOURNAL OF SOLID STATE CHEMISTRY, 2003, 172 (01) :81-88
[7]  
Fujishima A., 2000, J PHOTOCH PHOTOBIO C, V1, P1, DOI DOI 10.1016/S1389-5567(00)00002-2
[8]   Kinetics of the anatase rutile transformation in TiO2 in the presence of Fe2O3 [J].
Gennari, FC ;
Pasquevich, DM .
JOURNAL OF MATERIALS SCIENCE, 1998, 33 (06) :1571-1578
[9]   Growth of monodisperse nanocrystals of cerium oxide during synthesis and annealing [J].
Ghosh, Swapankumar ;
Divya, Damodaran ;
Remani, Kottayilpadi C. ;
Sreeremya, Thadathil S. .
JOURNAL OF NANOPARTICLE RESEARCH, 2010, 12 (05) :1905-1911
[10]   EVOLUTION OF PORE AND PHASE-STRUCTURE OF SOL-GEL DERIVED LANTHANA DOPED TITANIA AT HIGH-TEMPERATURES [J].
GOPALAN, R ;
LIN, YS .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1995, 34 (04) :1189-1195