An effective hybrid organic/inorganic inhibitor for alkaline aluminum-air fuel cells

被引:96
作者
Nie, Yujuan [1 ,2 ]
Gao, Jianxin [2 ]
Wang, Erdong [2 ]
Jiang, Luhua [2 ]
An, Liang [3 ]
Wang, Xuyun [1 ]
机构
[1] Qingdao Univ Sci & Technol, Coll Chem Engn, Qingdao 266042, Peoples R China
[2] Chinese Acad Sci, Dalian Inst Chem Phys, Dalian Natl Lab Clean Energy, Div Fuel Cell & Battery, Dalian 116023, Peoples R China
[3] Hong Kong Polytech Univ, Dept Mech Engn, Kowloon, Hong Kong, Peoples R China
关键词
Aluminum; Anode corrosion; Hybrid inhibitor; Casein; Fuel cell; AA5052 ALLOY ANODE; GA-0.1; SN-0.5; MN; PURE ALUMINUM; ELECTROCHEMICAL-BEHAVIOR; CORROSION; PERFORMANCE; ELECTROLYTE; ADDITIVES; BATTERIES; POLYPYRROLE;
D O I
10.1016/j.electacta.2017.07.108
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
An issue associated with aluminum-based batteries is the drastic parasitic corrosion of aluminum anode, which significantly restricts the utilization of aluminum. An effective approach is to add inhibitors in electrolytes to reduce the anode corrosion rate. In this work, Na2SnO3 and casein are proposed to act as a hybrid inhibitor in alkaline aluminum-air fuel cell. It is demonstrated that 0.05 M Na2SnO3 and 0.6 g L-1 casein offers the strongest corrosion protection, reducing the corrosion rate by approximately one order of magnitude. The corrosion inhibition is mainly attributed to the inhibition of cathodic reaction process. In addition, the analysis on the morphology and composition of the aluminum surface suggests that casein can greatly promote the deposition of tin to form a uniform and stable layer on the aluminum surface, due to the strong adsorption of polar functional groups in casein. Furthermore, the use of the hybrid inhibitor in aluminum-air fuel cell contributes to an increase of discharge capacity by 89.3%. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:478 / 485
页数:8
相关论文
共 36 条
[1]   Electrochemical corrosion of an Al-Mg-Cr-Mn alloy containing Fe and Si in inhibited alkaline solutions [J].
Adam, AMMM ;
Borras, N ;
Perez, E ;
Cabot, PL .
JOURNAL OF POWER SOURCES, 1996, 58 (02) :197-203
[2]   CONTROL OF AL CORROSION IN CAUSTIC SOLUTIONS [J].
BOCKSTIE, L ;
TREVETHAN, D ;
ZAROMB, S .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1963, 110 (04) :267-271
[3]   Organic Inhibitors of the Anode Self-Corrosion in Aluminum-Air Batteries [J].
Brito, P. S. D. ;
Sequeira, C. A. C. .
JOURNAL OF FUEL CELL SCIENCE AND TECHNOLOGY, 2014, 11 (01)
[4]   Corrosion and anodic behaviors of pure aluminum in a novel alkaline electrolyte [J].
Chang Xiao-Tu ;
Wang Jian-Ming ;
Shao Hai-Bo ;
Wang Jun-Bo ;
Zeng Xiao-Xu ;
Zhang Jian-Qing ;
Cao Chu-Nan .
ACTA PHYSICO-CHIMICA SINICA, 2008, 24 (09) :1620-1624
[5]   Electrochemical behaviour of aluminium in concentrated NaOH solutions [J].
Doche, ML ;
Rameau, JJ ;
Durand, R ;
Novel-Cattin, F .
CORROSION SCIENCE, 1999, 41 (04) :805-826
[6]   Developments in electrode materials and electrolytes for aluminium-air batteries [J].
Egan, D. R. ;
de Leon, C. Ponce ;
Wood, R. J. K. ;
Jones, R. L. ;
Stokes, K. R. ;
Walsh, F. C. .
JOURNAL OF POWER SOURCES, 2013, 236 :293-310
[7]   Characterization of some aluminium alloys for application as anodes in alkaline batteries [J].
El Abedin, SZ ;
Saleh, AO .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 2004, 34 (03) :331-335
[8]   Study on polyaniline-ZnO used as corrosion inhibitors of 57S aluminium in 2M NaOH solution [J].
Elango, A. ;
Periasamy, V. M. ;
Paramasivam, M. .
ANTI-CORROSION METHODS AND MATERIALS, 2009, 56 (05) :266-270
[9]   Performance of Al-0.6 Mg-0.05 Ga-0.1 Sn-0.1 In as Anode for Al-Air Battery in KOH Electrolytes [J].
Fan, Liang ;
Lu, Huimin ;
Leng, Jing ;
Sun, Zegao .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (14) :A2623-A2627
[10]   Aluminum corrosion mitigation in alkaline electrolytes containing hybrid inorganic/organic inhibitor system for power sources applications [J].
Gelman, Danny ;
Lasman, Itay ;
Elfimchev, Sergey ;
Starosvetsky, David ;
Ein-Eli, Yair .
JOURNAL OF POWER SOURCES, 2015, 285 :100-108