Corrosion mechanism associated with Mg2Si and Si particles in Al-Mg-Si alloys

被引:189
作者
Zeng Feng-li [1 ]
Wei Zhong-ling [2 ]
Li Jin-feng [1 ]
Li Chao-xing [1 ]
Tan Xing [1 ]
Zhang Zhao [3 ]
Zheng Zi-qiao [1 ]
机构
[1] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
[2] Jiaxing Key Lab Light Alloy Technol, Jiaxing 314051, Peoples R China
[3] Zhejiang Univ, Dept Chem, Hangzhou 310027, Zhejiang, Peoples R China
基金
中国国家自然科学基金;
关键词
Al-Mg-Si alloys; intergranular corrosion; corrosion mechanism; electrochemical behaviors; Mg2Si; Si; ALUMINUM-ALLOY; INTERGRANULAR CORROSION; LOCALIZED CORROSION; HEAT-TREATMENT; SIMULATION; BEHAVIORS;
D O I
10.1016/S1003-6326(11)61092-3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The electrochemical behaviors and coupling behaviors of the Mg2Si and Si phases with a(Al) were investigated, the corrosion morphologies of Al alloys containing Mg2Si and Si particles were observed, and the corrosion mechanism associated with them in Al-Mg-Si alloys was advanced. The results show that Si particle is always cathodic to the alloy base, Mg2Si is anodic to the alloy base and corrosion occurs on its surface at the beginning. However, during its corrosion process, the preferential dissolution of Mg and the enrichment of Si make Mg2Si transform to cathode from anode, leading to the anodic dissolution and corrosion of the alloy base at its adjacent periphery at a later stage. As the mole ratio of Mg to Si in an Al-Mg-Si alloy is less than 1.73, it contains Mg2Si and Si particles simultaneously in the grain boundary area, and corrosion initiates on the Mg2Si surface and the precipitate-free zone (PFZ) at the adjacent periphery of Si particle. As corrosion time is extended, Si particle leads to severe anodic dissolution and corrosion of the PFZ at its adjacent periphery, expedites the polarity transformation between Mg2Si and the PFZ and accelerates the corrosion of PFZ at the adjacent periphery of Mg2Si particle.
引用
收藏
页码:2559 / 2567
页数:9
相关论文
共 17 条
[1]   Wear and corrosion behaviours of extruded Al-12Si-XMg alloys [J].
Ahlatci, Hayrettin .
MATERIALS LETTERS, 2008, 62 (20) :3490-3492
[2]   Effect of iron-containing intermetallic particles on the corrosion behaviour of aluminium [J].
Ambat, Rajan ;
Davenport, Alison J. ;
Scamans, Geoff M. ;
Afseth, Andreas .
CORROSION SCIENCE, 2006, 48 (11) :3455-3471
[3]  
[Anonymous], RARE METAL MAT ENG
[4]  
[Anonymous], J ELECTROCHEM SOC
[5]  
[Anonymous], HDB ALUMINUM ALLOY F
[6]   Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T3 [J].
Buchheit, RG ;
Grant, RP ;
Hlava, PF ;
Mckenzie, B ;
Zender, GL .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (08) :2621-2628
[7]   The influence of MgSi particle reactivity and dissolution processes on corrosion in Al-Mg-Si alloys [J].
Eckermann, Fabian ;
Suter, Thomas ;
Uggowitzer, Peter J. ;
Afseth, Andreas ;
Schmutz, Patrick .
ELECTROCHIMICA ACTA, 2008, 54 (02) :844-855
[8]   Localized corrosion of 6056 T6 aluminium alloy in chloride media [J].
Guillaumin, V ;
Mankowski, G .
CORROSION SCIENCE, 2000, 42 (01) :105-125
[9]   Localized corrosion mechanism of 2 x x x-series Al alloy containing S(Al2CuMg) and θ′(Al2Cu) precipitates in 4.0% NaCl solution at pH 6.1 [J].
Jin, FL ;
Zheng, ZQ ;
Jiang, N ;
Tan, CY .
MATERIALS CHEMISTRY AND PHYSICS, 2005, 91 (2-3) :325-329
[10]   Intergranular corrosion of copper-containing AA6xxx AlMgSi aluminum alloys [J].
Larsen, Magnus Hurlen ;
Walmsley, John Charles ;
Lunder, Otto ;
Mathiesen, Ragnvald H. ;
Nisancioglu, Kemal .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2008, 155 (11) :C550-C556