Generation of Ultra-Clean Coal from Victorian Brown Coal: Effect of Hydrothermal Treatment and Particle Size on Coal Demineralization and the Extraction Kinetic of Individual Metals

被引:20
作者
Wijaya, Niken [1 ]
Choo, Teck Kwang [1 ]
Zhang, Lian [1 ]
机构
[1] Monash Univ, Dept Chem Engn, Clayton, Vic 3800, Australia
基金
澳大利亚研究理事会;
关键词
ASH-FREE COAL; SOLVENT-EXTRACTION; SODIUM-HYDROXIDE; MINERAL MATTER; ACID; TRANSFORMATION; PRETREATMENT; TEMPERATURE; MOSSBAUER; ELEMENTS;
D O I
10.1021/ef3005459
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
This paper addressed the influences of hydrothermal treatment and particle size on the demineralization extent of Victorian brown coal for the generation of ultra-clean coal to burn directly in a gas turbine combined cycle. Extraction kinetics of individual metals have been investigated. The results for four different sizes of two Victorian brown coal samples showed that, for brown coal that is rich in the aluminum-/silicon-bearing mineral grains, its demineralization extent was dependent on coal particle size, showing the best result for the coal size of 150-300 mu m. In contrast, the ash removal efficiency of brown coal rich in organically bound metals remained unaffected by particle size, substantiating a uniform distribution of ash-forming metals on the coal surface as a weak association with the oxygen-containing functional groups. The elution of most metals followed a pseudo-second-order with a confidence interval >= 90%. The activation energy and pre-exponential factor varied significantly with element type and coal sample. Irrespective of coal sample, the extraction of sodium (Na) was achieved instantaneously upon acid attack, relative to iron (Fe) demonstrating an intraparticle diffusion controlling extraction with an activation energy less than 20 kJ/mol. The coal sample rich in mineral grains exhibited an elution behavior limited by both surface reaction and intraparticle diffusion control with respect to a variety of metals. The mineral-grain-rich coal was further treated with pyroligneous acid, citric acid, and Na-EDTA followed by pyroligneous acid at 200 degrees C to maximize its demineralization extent. As has been confirmed through the use of these three reagents, the overall ash content in coal has been reduced to similar to 1.59, 0.95, and 1.17 dry basis (db)-wt %, respectively, as opposed to 2.49 db-wt % in the corresponding raw coal. This study has demonstrated the potential use of waste pyroligneous acid and citric acid for brown coal leaching to generate ultra-clean coal.
引用
收藏
页码:5028 / 5035
页数:8
相关论文
共 27 条
[21]  
Wibberley L., 2008, 74 AUSTR BLACK COAL
[22]   Generation of ultra-clean coal from Victorian brown coal - Sequential and single leaching at room temperature to elucidate the elution of individual inorganic elements [J].
Wijaya, Niken ;
Choo, Teck Kwang ;
Zhang, Lian .
FUEL PROCESSING TECHNOLOGY, 2011, 92 (11) :2127-2137
[23]   A Critical Review of Coal Demineralization and Its Implication on Understanding the Speciation of Organically Bound Metals and Submicrometer Mineral Grains in Coal [J].
Wijaya, Niken ;
Zhang, Lian .
ENERGY & FUELS, 2011, 25 (01) :1-16
[24]   COAL DEMINERALIZATION USING SODIUM-HYDROXIDE AND ACID-SOLUTIONS [J].
YANG, RT ;
DAS, SK ;
TSAI, BMC .
FUEL, 1985, 64 (06) :735-742
[25]   Relationship between thermal extraction yield and softening temperature for coals [J].
Yoshida, T ;
Takanohashi, T ;
Sakanishi, K ;
Saito, I ;
Fujita, M ;
Mashimo, K .
ENERGY & FUELS, 2002, 16 (04) :1006-1007
[26]   Coordination structures of organically bound paramagnetic metals in coal and their transformation upon solvent extraction [J].
Zhang, Lian ;
Takanohashi, Toshimasa ;
Kutsuna, Shuzo ;
Saito, Ikuo ;
Wang, Qunying ;
Ninomiya, Yoshihiko .
FUEL, 2008, 87 (12) :2628-2640
[27]   Etution of Ti during solvent extraction of coal and the transformation of eluted Ti upon combustion [J].
Zhang, Lian ;
Takanohashi, Toshimasa ;
Saito, Ikuo ;
Wang, Qunying ;
Ninomiya, Yoshihiko .
AICHE JOURNAL, 2008, 54 (06) :1646-1655