Cavitation-crazing transition in rubber toughening of poly(lactic acid)-cellulose nanocrystal composites

被引:34
作者
Muiruri, Joseph K. [1 ,2 ]
Liu, Songlin [2 ]
Teo, Wern Sze [3 ]
Yeo, Jayven Chee Chuan [1 ,2 ]
Thitsartarn, Warintorn [2 ]
He, Chaobin [1 ,2 ]
机构
[1] Natl Univ Singapore, Dept Mat Sci & Engn, 9 Engn Dr 1, Singapore 117576, Singapore
[2] ASTAR, Inst Mat Res & Engn, 2 Fusionopolis Way,Innovis 08-03, Singapore 138634, Singapore
[3] ASTAR, Singapore Inst Mfg Technol, 2 Fusionopolis Way,Innovis 08-04, Singapore 138634, Singapore
基金
中国国家自然科学基金;
关键词
Functional composites; Mechanical properties; Deformation; Injection moulding; IN-SITU SAXS; STEREOCOMPLEX CRYSTALLIZATION; POLYMERS; NANOPARTICLES; DEFORMATION; POLYLACTIDE; MORPHOLOGY; BEHAVIOR; PLA;
D O I
10.1016/j.compscitech.2018.08.021
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this work, the mechanism behind rubber toughening of poly(lactic acid)/cellulose nanocrystal-g-rubber-g-poly(D-lactide) (CNC-rDx-PDLA) composites was elucidated through systematic study of the effects of rubber segment content (length) in CNC-rDx-PDLA nanofillers and the nanofiller concentrations on the deformation behavior of the nanocomposites. It was shown that with an increase of rubber segment length and rubber filler concentration, the elongation at break of the resulting composites increased. Moreover, a dramatic increase in elongation at break (from 20% to 200%) was observed when the rubber segment content (length) in the CNC-rDx-PDLA nanofillers was increased from 52 to 68%. Cavitation mechanism was found dominant when the rubber segment content in the nanofillers was 52% and below, whereas, stable crazes were formed and followed by fibrillation when the rubber segment content in the nanofillers was increased to 68%, which was evident by small angle X-ray scattering (SAXS) study and scanning electron microscopy (SEM) analysis. The existence of a transition from cavitation to crazing in the composite systems could be attributed to a more mobile rubber phase because of longer rubber chain length. Our study suggests that the effective toughening mechanism for thermoplastics such as PLA is crazing induced plastic deformation.
引用
收藏
页码:12 / 19
页数:8
相关论文
共 36 条
[11]  
Lebarbe T., 2013, SYNTHESIS NOVEL GREE
[12]   Biodegradable silica rubber core-shell nanoparticles and their stereocomplex for efficient PLA toughening [J].
Li, Zibiao ;
Muiruri, Joseph K. ;
Thitsartarn, Warintorn ;
Zhang, Xing ;
Tan, Beng Hoon ;
He, Chaobin .
COMPOSITES SCIENCE AND TECHNOLOGY, 2018, 159 :11-17
[13]   Recent advances in stereocomplexation of enantiomeric PLA-based copolymers and applications [J].
Li, Zibiao ;
Tan, Beng Hoon ;
Lin, Tingting ;
He, Chaobin .
PROGRESS IN POLYMER SCIENCE, 2016, 62 :22-72
[14]   Facile Layer-by-Layer Self-Assembly toward Enantiomeric Poly(lactide) Stereocomplex Coated Magnetite Nanocarrier for Highly Tunable Drug Deliveries [J].
Li, Zibiao ;
Yuan, Du ;
Jin, Guorui ;
Tan, Beng H. ;
He, Chaobin .
ACS APPLIED MATERIALS & INTERFACES, 2016, 8 (03) :1842-1853
[15]   Research Progress in Toughening Modification of Poly(lactic acid) [J].
Liu, Hongzhi ;
Zhang, Jinwen .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 2011, 49 (15) :1051-1083
[16]  
Lotz B., 2017, CRYSTAL POLYMORPHISM
[17]  
Ma P, 2011, THESIS TECHNISCHE U
[18]   Highly Biodegradable and Tough Polylactic Acid-Cellulose Nanocrystal Composite [J].
Muiruri, Joseph K. ;
Liu, Songlin ;
Teo, Wern Sze ;
Kong, Junhua ;
He, Chaobin .
ACS SUSTAINABLE CHEMISTRY & ENGINEERING, 2017, 5 (05) :3929-3937
[19]   Toughening of polylactide by tailoring phase-morphology with P[CL-co-LA] random copolyesters as biodegradable impact modifiers [J].
Odent, Jeremy ;
Leclere, Philippe ;
Raquez, Jean-Marie ;
Dubois, Philippe .
EUROPEAN POLYMER JOURNAL, 2013, 49 (04) :914-922
[20]   Mechanism of Toughening in Rubber Toughened Polyolefin-A Review [J].
Panda, Bishnu P. ;
Mohanty, Smita ;
Nayak, Sanjay K. .
POLYMER-PLASTICS TECHNOLOGY AND ENGINEERING, 2015, 54 (05) :462-473