Cavitation-crazing transition in rubber toughening of poly(lactic acid)-cellulose nanocrystal composites

被引:34
作者
Muiruri, Joseph K. [1 ,2 ]
Liu, Songlin [2 ]
Teo, Wern Sze [3 ]
Yeo, Jayven Chee Chuan [1 ,2 ]
Thitsartarn, Warintorn [2 ]
He, Chaobin [1 ,2 ]
机构
[1] Natl Univ Singapore, Dept Mat Sci & Engn, 9 Engn Dr 1, Singapore 117576, Singapore
[2] ASTAR, Inst Mat Res & Engn, 2 Fusionopolis Way,Innovis 08-03, Singapore 138634, Singapore
[3] ASTAR, Singapore Inst Mfg Technol, 2 Fusionopolis Way,Innovis 08-04, Singapore 138634, Singapore
基金
中国国家自然科学基金;
关键词
Functional composites; Mechanical properties; Deformation; Injection moulding; IN-SITU SAXS; STEREOCOMPLEX CRYSTALLIZATION; POLYMERS; NANOPARTICLES; DEFORMATION; POLYLACTIDE; MORPHOLOGY; BEHAVIOR; PLA;
D O I
10.1016/j.compscitech.2018.08.021
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this work, the mechanism behind rubber toughening of poly(lactic acid)/cellulose nanocrystal-g-rubber-g-poly(D-lactide) (CNC-rDx-PDLA) composites was elucidated through systematic study of the effects of rubber segment content (length) in CNC-rDx-PDLA nanofillers and the nanofiller concentrations on the deformation behavior of the nanocomposites. It was shown that with an increase of rubber segment length and rubber filler concentration, the elongation at break of the resulting composites increased. Moreover, a dramatic increase in elongation at break (from 20% to 200%) was observed when the rubber segment content (length) in the CNC-rDx-PDLA nanofillers was increased from 52 to 68%. Cavitation mechanism was found dominant when the rubber segment content in the nanofillers was 52% and below, whereas, stable crazes were formed and followed by fibrillation when the rubber segment content in the nanofillers was increased to 68%, which was evident by small angle X-ray scattering (SAXS) study and scanning electron microscopy (SEM) analysis. The existence of a transition from cavitation to crazing in the composite systems could be attributed to a more mobile rubber phase because of longer rubber chain length. Our study suggests that the effective toughening mechanism for thermoplastics such as PLA is crazing induced plastic deformation.
引用
收藏
页码:12 / 19
页数:8
相关论文
共 36 条
[1]   Toughening polylactide [J].
Anderson, Kelly S. ;
Schreck, Kathleen M. ;
Hillmyer, Marc A. .
POLYMER REVIEWS, 2008, 48 (01) :85-108
[2]  
Auras RA, 2011, POLYLACTIC ACID SYNT, V10
[3]  
Fan X., 2016, ACS SUSTAIN CHEM ENG, V5, P1217
[4]   Synthesis of star-like hybrid POSS-(PDMAEMA-b-PDLA)8 copolymer and its stereocomplex properties with PLLA [J].
Fan, Xiaoshan ;
Cao, Mengya ;
Zhang, Xing ;
Li, Zibiao .
MATERIALS SCIENCE AND ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2017, 76 :211-216
[5]   Supertough Polylactide Materials Prepared through In Situ Reactive Blending with PEG-Based Diacrylate Monomer [J].
Fang, Huagao ;
Jiang, Feng ;
Wu, Qianghua ;
Ding, Yunsheng ;
Wang, Zhigang .
ACS APPLIED MATERIALS & INTERFACES, 2014, 6 (16) :13552-13563
[6]   Stereocomplexed polylactides (Neo-PLA) as high-performance bio-based polymers: their formation, properties, and application [J].
Fukushima, Kazuki ;
Kimura, Yoshiharu .
POLYMER INTERNATIONAL, 2006, 55 (06) :626-642
[7]   Improvement of the mechanical properties of poly(D,L-lactide) by orientation [J].
Grijpma, DW ;
Altpeter, H ;
Bevis, MJ ;
Feijen, J .
POLYMER INTERNATIONAL, 2002, 51 (10) :845-851
[8]   In-situ deformation studies of rubber toughened poly(methyl methacrylate): Influence of rubber particle concentration and rubber cross-linking density [J].
He, CB ;
Donald, AM ;
Butler, MF .
MACROMOLECULES, 1998, 31 (01) :158-164
[9]   New Insight on Initiation of Cavitation in Semicrystalline Polymers: In-Situ SAXS Measurements [J].
Humbert, S. ;
Lame, O. ;
Chenal, J. M. ;
Rochas, C. ;
Vigier, G. .
MACROMOLECULES, 2010, 43 (17) :7212-7221
[10]   Mechanisms of plastic deformation in biodegradable polylactide/poly(1,4-cis-isoprene) blends [J].
Kowalczyk, Marcin ;
Piorkowska, Ewa .
JOURNAL OF APPLIED POLYMER SCIENCE, 2012, 124 (06) :4579-4589