Effect of pre-annealing on microstructure and compactibility of gas-atomized Al-Si alloy powders
被引:9
作者:
Cai, Zhi-yong
论文数: 0引用数: 0
h-index: 0
机构:
Jiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Cai, Zhi-yong
[1
,2
]
Zhang, Chun
论文数: 0引用数: 0
h-index: 0
机构:
Jiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Zhang, Chun
[1
,2
]
Wang, Ri-chu
论文数: 0引用数: 0
h-index: 0
机构:
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Wang, Ri-chu
[2
]
Peng, Chao-qun
论文数: 0引用数: 0
h-index: 0
机构:
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Peng, Chao-qun
[2
]
Qiu, Ke
论文数: 0引用数: 0
h-index: 0
机构:
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Qiu, Ke
[2
]
Wang, Nai-guang
论文数: 0引用数: 0
h-index: 0
机构:
Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R ChinaJiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
Wang, Nai-guang
[2
]
机构:
[1] Jiangxi Univ Sci & Technol, Sch Mat Sci & Engn, Ganzhou 341000, Peoples R China
[2] Cent S Univ, Sch Mat Sci & Engn, Changsha 410083, Hunan, Peoples R China
Effect of pre-annealing treatment temperature on compactibility of gas-atomized Al-27% Si alloy powders was investigated. Microstructure and hardness of the annealed powders were characterized. Pre-annealing results in decreasing Al matrix hardness, dissolving of needle-like eutectic Si phase, precipitation and growth of supersaturated Si atoms, and spheroidisation of primary Si phase. Compactibility of the alloy powders is gradually improved with increasing the annealing temperature to 400 degrees C. However, it decreases when the temperature is above 400 degrees C owing to the existence of Si-Si phase clusters and the densely distributed Si particles. A maximum relative density of 96.1% is obtained after annealing at 400 degrees C for 4 h. In addition, the deviation of compactibility among the pre-annealed powders reaches a maximum at a pressure of 175 MPa. Therefore, a proper pre-annealing treatment can significantly enhance the cold compactibility of gas-atomized Al-Si alloy powders.