Sketching novel nanostructured diamond-consisted thin films on AISI 321 stainless steel: Microstructure, mechanical and tribological properties

被引:7
作者
Sharifi, E. [1 ]
Khamseh, S. [2 ]
Shirani, A. S. [1 ]
Ramezanzadeh, B. [3 ]
机构
[1] Shahid Beheshti Univ, Dept Engn, POB 1983969411, Tehran, Iran
[2] Inst Color Sci & Technol ICST, Dept Nanomat & Nanocoatings, POB 16765-654, 654, Tehran, Iran
[3] Inst Color Sci & Technol ICST, Dept Surface Coating & Corros, POB 16765-654, Tehran, Iran
关键词
Nanostructured (Nb; a -Carbon) films; Cubic diamond; Hexagonal diamond; BM; UBM sputtering; AISI 321 Stainless Steel; Microstructure; Mechanical and tribological properties; HEXAGONAL DIAMOND; CUBIC DIAMOND; CARBON; COATINGS; SURFACE; GROWTH; DEPOSITION; NITRIDE; WEAR; TEMPERATURE;
D O I
10.1016/j.triboint.2022.107891
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In a reactive direct current (DC) magnetron sputtering (MS) system, converting the cathode (target) magnetic field configuration from a balanced magnetron (BM) to an unbalanced magnetron (UBM) is an impressive strategy to enforce the energetic ion bombardment, providing sufficient activation energy for deposition of high -quality nanostructured films. In the present work, the nanostructured (grain size < 100 nm) BM and UBM sputtered Niobium-doped amorphous Carbon (Nb: a-Carbon) films' microstructural, mechanical, and tribological characteristics changes were thoroughly investigated and compared. From the XRD and Raman analysis out-comes both graphite-like Carbon (GLC) and Niobium carbide (NbC) phases were detected in the BM sputtered film. However, novel cubic and hexagonal crystalline Diamond (CD) phases were successfully constructed from the UBM sputtered films besides the GLC and NbC phases. Records displayed that the change over the cathode magnetic field configuration from BM to UBM is a responsible factor for the reduction of the surface roughness (from 32 nm to 25 nm) and increment of the crystallite size (from 14 nm to 15.5 nm), hardness (from 18 GPa to 27 GPa), and elastic modulus (from 210 GPa to 425 GPa) values. On the contrary, via changing BM to UBM sputtering the films' tribological properties were negatively affected, leading to the increase of the coefficient of friction (COF) from 0.09 to 0.11 and the wear rate (WR) from 5.25 x 10-5 mm(3)/N.m to 9 x 10-5 mm3/N.m. The achieved results confirmed that the UBM configuration could be selected as a critical facility over the MS system that gives enough energy to arrange Carbon species in the crystalline Diamond phase at a relatively low temperature. One step further, the Ar/CH4 ratio variation was assessed as an influential factor that leaves consid-erable changes over the UBM sputtered film characteristics. The results indicated that by doubling the Ar/CH4 ratio, the nanocrystalline Diamond phases are still observable. However, this change led to the increase in surface roughness (from 25 nm to 28 nm) and crystallite sizes (NbC, from 15.5 nm to 18.6 nm, cubic Diamond, from 25.8 nm to 36 nm, and hexagonal Diamond from 18.9 nm to 21.6 nm). While the variations adversely affected the UBM sputtered films' hardness (from 27 GPa to 21 GPa) and modulus of elasticity (from 425 GPa to 330 GPa). Simultaneously, the COF and WR endured a slight increment, from 0.11 to 0.14 and 9 x 10-5 mm3/N.m to 9.8 x 10-5 mm3/N.m, respectively.
引用
收藏
页数:13
相关论文
共 66 条
  • [61] Mechanical properties and wear behavior of multi-layer diamond films deposited by hot-filament chemical vapor deposition
    Yan, Guangyu
    Wu, Yuhou
    Cristea, Daniel
    Liu, Lusheng
    Tierean, Mircea
    Wang, Yibao
    Lu, Feng
    Wang, He
    Yuan, Ziyao
    Munteanu, Daniel
    Zhao, Dehong
    [J]. APPLIED SURFACE SCIENCE, 2019, 494 : 401 - 411
  • [62] Microstructure, mechanical and tribological properties of graphite-like carbon coatings doped with tantalum
    Yan, Mingming
    Wang, Xinyu
    Zhou, Haibin
    Liu, Jian
    Zhang, Shuaituo
    Lu, Yan
    Hao, Junying
    [J]. APPLIED SURFACE SCIENCE, 2021, 542
  • [63] Effect of sputtering power on structure and properties of ZTO films
    Yu, Shijin
    Xu, Wanmei
    Zhu, Hua
    Qiu, Wangren
    Fu, Qiuyun
    Kong, Lingbing
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 883
  • [64] Reactive magnetron sputtering deposition and characterization of niobium carbide films
    Zhang, Kan
    Wen, M.
    Cheng, G.
    Li, X.
    Meng, Q. N.
    Lian, J. S.
    Zheng, W. T.
    [J]. VACUUM, 2014, 99 : 233 - 241
  • [65] Excellent mechanical, tribological and anti-corrosive performance of novel Ti-DLC nanocomposite thin films prepared via magnetron sputtering method
    Zhang, Shidong
    Yan, Mufu
    Yang, Yang
    Zhang, Yanxiang
    Yan, Fuyao
    Li, Hongtao
    [J]. CARBON, 2019, 151 : 136 - 147
  • [66] Effects of Cr concentrations on the microstructure, hardness, and temperature-dependent tribological properties of Cr-DLC coatings
    Zou, C. W.
    Wang, H. J.
    Feng, L.
    Xue, S. W.
    [J]. APPLIED SURFACE SCIENCE, 2013, 286 : 137 - 141