Influence of surface and heat treatments on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic

被引:121
作者
Guazzato, M [1 ]
Albakry, M [1 ]
Quach, L [1 ]
Swain, MV [1 ]
机构
[1] Univ Sydney, Fac Dent, Biomat Sci Res Unit, United Dent Hosp, Surry Hills, NSW 2010, Australia
关键词
dental ceramics; strength; surface treatment; heat treatment; alumina; glass; zirconia;
D O I
10.1016/j.dental.2004.07.010
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. The purpose of this study was to investigate the influence of sandblasting, grinding, grinding orientation and polishing before and after heat treatment, on the flexural strength of a glass-infiltrated alumina/zirconia-reinforced dental ceramic (In-Ceram Zirconia). Methods. The uniaxial flexural strength was calculated on 160bar-shaped specimens (20X4X1.2 mm) divided equally into eight groups as follows: sandblasted; sandblasted heated; polished; polished heated; ground parallel to the tensile axis; ground parallel heated; ground perpendicular; and ground perpendicular heated. Data were analyzed with multiple regression analysis, one-way ANOVA and Tukey's pairwise multiple comparisons and Weibull analysis. The treated and fractured surfaces were observed with SEM. The relative content of the monoclinic phase was quantified with an X-ray diffraction analysis. Results. A thin layer of glass was present on the surface of the specimens after heat treatment and contributed to an improvement of the flexural strength. Surface treatment (not followed by heat treatment) generated phase transformation which, however, was not sufficient to avoid strength degradation caused by the flaws introduced with the surface treatments. Sandblasting caused the most marked strength degradation. Polishing alone increased the reliability, but did not improve the strength. The orientation of grinding in respect of the direction of the tensile stresses did not influence the ultimate tensile strength. Significance. The present study suggests that any surface treatment performed on In-Ceram Zirconia should always be followed by heat treatment to avoid strength degradation. 2004 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:454 / 463
页数:10
相关论文
共 34 条
[1]  
[Anonymous], 1995, 6872 ISO
[2]   EFFECT OF THERMAL TEMPERING ON STRENGTH AND CRACK-PROPAGATION BEHAVIOR OF FELDSPATHIC PORCELAINS [J].
ANUSAVICE, KJ ;
HOJJATIE, B .
JOURNAL OF DENTAL RESEARCH, 1991, 70 (06) :1009-1013
[3]   STRENGTHENING OF FELDSPATHIC PORCELAIN BY ION-EXCHANGE AND TEMPERING [J].
ANUSAVICE, KJ ;
SHEN, C ;
LEE, RB .
JOURNAL OF DENTAL RESEARCH, 1992, 71 (05) :1134-1138
[4]   INFLUENCE OF INITIAL FLAW SIZE ON CRACK-GROWTH IN AIR-TEMPERED PORCELAIN [J].
ANUSAVICE, KJ ;
GRAY, A ;
SHEN, C .
JOURNAL OF DENTAL RESEARCH, 1991, 70 (02) :131-136
[5]   Effect of glaze thickness on the fracture toughness and hardness of alumina-reinforced porcelain [J].
Baharav, H ;
Laufer, BZ ;
Pilo, R ;
Cardash, HS .
JOURNAL OF PROSTHETIC DENTISTRY, 1999, 81 (05) :515-519
[6]  
Blixt M, 2000, INT J PROSTHODONT, V13, P221
[7]   Effects of surface finish and fatigue testing on the fracture strength of CAD-CAM and pressed-ceramic crowns [J].
Chen, HY ;
Hickel, R ;
Setcos, JC ;
Kunzelmann, KH .
JOURNAL OF PROSTHETIC DENTISTRY, 1999, 82 (04) :468-475
[8]  
Chong KH, 2002, INT J PROSTHODONT, V15, P183
[9]  
Denry IL, 1999, J BIOMED MATER RES, V48, P791, DOI 10.1002/(SICI)1097-4636(1999)48:6<791::AID-JBM5>3.3.CO
[10]  
2-G