Influence of silanization and filler fraction on aged dental composites

被引:48
作者
Lin, CT
Lee, SY
Keh, ES
Dong, DR
Huang, HM
Shih, YH
机构
[1] Wan Fan Hosp, Taipei, Taiwan
[2] Natl Def Med Ctr, Sch Dent, Taipei, Taiwan
[3] Taipei Med Coll, Dept Dent, Taipei, Taiwan
[4] Taipei Med Coll, Sch Med Technol, Taipei, Taiwan
[5] Taipei Med Coll, Taipei, Taiwan
[6] Taipei Med Coll, Grad Inst Oral Rehabil Sci, Taipei 110, Taiwan
关键词
D O I
10.1046/j.1365-2842.2000.00573.x
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The effect of silanization and filler fraction on the mechnical properties of aged dental composites was investigated. Experimental composites (75/25 Bis-GMA/TEGDMA resin reinforced with 0, 12 .6, 30 .0, and 56 .5 vol% 8 mum silanized/unisilanized BaSiO6) were fabricated into 4 .7 mm diameter x 2 .2 mm thick discs and 3 .5 mm diameter x 7 .3 mm thick discs for diametral tensile and compressive tests, respectively. The effect of immersion in 75% ethanol at 37 degreesC for 0-30 days on the diametral tensile strength (DTS) and compressive strength (CS) of the samples was evaluated and analysed by ANOVA and Tukey LSD test. The fracture interface between filler and resin matrix was then examined by scanning electron microscope. Results and subsequent statistical evidence from DTS (18 .6 +/- 7 .6 MPa, silanized versus 11 .7 +/- 2 .6 MPa, unsilanized) and CS (85 .1 +/- 29 .7 MPa, silanized versus 56 .0 +/- 11 .3 MPa, unsilanized) strongly implies that silanization may greatly enhance the mechanical properties of the resin composites, Furthermore, it also shows that both DTS and CS increased proportionally as the filler fraction of the composites increased. However, in the unsilanized groups, DTS decreased (up to 40%) as the filler fraction increased, and CS showed no relevance to the filler fraction at all. As for the influence of aging, it was found that both DTS and CS showed a significant decrease after immersion in 75% ethanol, and silanization heavily correlated with the filler fraction of aged-resin composites. Microscopic examination of the fractured samples showed that failure primarily occurred within the resin matrix per se for silanized composites and adjacent to the filler particles for unsilanized composites. All the evidence points to the conclusion that mechanical properties of aged-resin composites can be greatly influenced by silanization and the filler fraction.
引用
收藏
页码:919 / 926
页数:8
相关论文
共 17 条
  • [1] PROTECTION HYPOTHESIS FOR COMPOSITE WEAR
    BAYNE, SC
    TAYLOR, DF
    HEYMANN, HO
    [J]. DENTAL MATERIALS, 1992, 8 (5-6) : 305 - 309
  • [2] Bowen R. L., 1962, U. S. Pat., Patent No. [3,066,112, 3066112]
  • [3] CRAIG RG, 1976, INT DENT J, V26, P121
  • [4] FERRACANE JL, 1983, THESIS NW U CHICAGO
  • [5] Food and Drug Administration (FDA), 1976, GUID CHEM TECHN REQ
  • [6] Knock F, 1951, U.S. Patent, Patent No. 2558139
  • [7] EFFECT OF FOOD AND ORAL SIMULATING FLUIDS ON DENTIN BOND AND COMPOSITE STRENGTH
    LEE, SY
    GREENER, EH
    MUELLER, HJ
    CHIU, CH
    [J]. JOURNAL OF DENTISTRY, 1994, 22 (06) : 352 - 359
  • [8] Lee SY, 1998, J ORAL REHABIL, V25, P575
  • [9] EFFECT OF FOOD AND ORAL SIMULATING FLUIDS ON STRUCTURE OF ADHESIVE COMPOSITE SYSTEMS
    LEE, SY
    GREENER, EH
    MUELLER, HJ
    [J]. JOURNAL OF DENTISTRY, 1995, 23 (01) : 27 - 35
  • [10] Detection of leached moieties from dental composites in fluids simulating food and saliva
    Lee, SY
    Greener, EH
    Menis, DL