摘要
Advanced transparent ceramics with high chemical and thermal stability are gaining increasing interest as replacement of glass-based materials in technical window applications. The mechanical reliability and performance of transparent MgAl2O4 with a grain size of 5 mu m has been characterized at ambient temperature using micro-mechanical indentation and macroscopic bending tests. The measurements focused on elastic modulus, fracture toughness, crack kinetics, and strength, the latter analyzed with Weibull statistics. The effect of slow crack growth is assessed using a strength-probability-time plot. Complementary fractography by optical, confocal and scanning electron microscopy provided a correlation between failure origin and fracture stress. The results and reliability aspects are discussed in terms of linear elastic fracture mechanics.
引用
收藏
页码:4821 / 4826
页数:6
相关论文
共 25 条
[11]   A study on toughening and strengthening of Mg-Al spinel transparent ceramics [J].
Huang, Cunbing ;
Lu, Tiecheng ;
Lin, Libin ;
Lei, Muyun ;
Huang, Cunxin .
High-Performance Ceramics IV, Pts 1-3, 2007, 336-338 :1207-1210
[12]   Transmission physics and consequences for materials selection, manufacturing, and applications [J].
Krell, Andreas ;
Hutzler, Thomas ;
Klimke, Jens .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2009, 29 (02) :207-221
[13]   Measuring mechanical properties of coatings: a methodology applied to nano-particle-filled sol-gel coatings on glass [J].
Malzbender, J ;
den Toonder, JMJ ;
Balkenende, AR ;
de With, G .
MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2002, 36 (2-3) :47-103
[14]   Comment on hardness definitions [J].
Malzbender, J .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (09) :1355-1359
[15]   Threshold fracture stress of thin ceramic components [J].
Malzbender, Juergen ;
Steinbrech, Rolf W. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2008, 28 (01) :247-252
[16]   Fracture test of thin sheet electrolytes for solid oxide fuel cells [J].
Malzbender, Juergen ;
Steinbrech, Rolf W. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2007, 27 (07) :2597-2603
[17]   Dynamic Ring-on-Ring Equibiaxial Flexural Strength of Borosilicate Glass [J].
Nie, Xu ;
Chen, Weinong W. ;
Templeton, Douglas W. .
INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2010, 7 (05) :616-624
[18]   EVALUATION OF KLC OF BRITTLE SOLIDS BY THE INDENTATION METHOD WITH LOW CRACK-TO-INDENT RATIOS [J].
NIIHARA, K ;
MORENA, R ;
HASSELMAN, DPH .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1982, 1 (01) :13-16
[19]  
Palchaev DK, 1985, GLASS CERAM, V40, P319
[20]   Mechanical properties and lifetime predictions for Ba0.5Sr0.5Co0.8Fe0.2O3-δ membrane material [J].
Pecanac, G. ;
Baumann, S. ;
Malzbender, J. .
JOURNAL OF MEMBRANE SCIENCE, 2011, 385 (1-2) :263-268