Anaerobic biodegradation of the microbial copolymer poly(3-hydroxybutyrate-co-3-hydroxyhexanoate): Effects of comonomer content, processing history, and semi-crystalline morphology

被引:33
作者
Morse, Margaret-Catherine [1 ]
Liao, Qi [2 ]
Criddle, Craig S. [1 ]
Frank, Curtis W. [2 ]
机构
[1] Stanford Univ, Dept Civil & Environm Engn, Stanford, CA 94305 USA
[2] Stanford Univ, Dept Chem Engn, Stanford, CA 94305 USA
关键词
Biodegradable polymer; Polyhydroxyalkanoates; Polymer morphology; DIFFERENTIAL SCANNING CALORIMETRY; SOLID-STATE STRUCTURES; MELTING BEHAVIOR; ENZYMATIC DEGRADABILITIES; BANDED SPHERULITES; SINGLE-CRYSTALS; DEGRADATION; POLY(3-HYDROXYBUTYRATE); FILMS; CRYSTALLIZATION;
D O I
10.1016/j.polymer.2010.11.024
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Films of poly(3-hydroxybutyrate-co-3-hydroxyhexanoate) (P3HB-co-3HHx) containing 3.8-10 mol% of 3-hydroxyhexanoate (3HHx) comonomer were subjected to anaerobic biodegradation to explore the effects of copolymer composition, crystallinity, and morphology on biodegradation. As biodegradation proceeded, samples with higher HHx fraction tended to have faster weight loss: on Day 7 of the degradation experiment, P3HB-co-10 mol%-3HHx lost 80% of its original weight, while P3HB-co-3.8 mol %-3HHx lost only 28%. Scanning electron microscopy (SEM) images revealed that the anaerobic biodegradation proceeded at the surface of the samples, with preferential erosion of the amorphous regions, exposing the crystalline spherulites formed inside the copolymer films. It was observed that copolymers with higher HHx fraction had smaller diameter spherulites, ranging from roughly 40 mu m for P3HB-co-3.8 mol%-3HHx to 10 mu m for P3HB-co-10 mol%-3HHx. A banded spherulite morphology was observed for P3HB-co-6.9 mol%-3HHx and P3HB-co-10 mol%-3HHx, with much wider band spacing (2 mu m) for the former than the latter (0.3 mu m). Different thermal history seemed to affect the morphological properties and, thus, the biodegradability of the P3HB-co-3HHx samples as well. When comparing copolymers with the same copolymer composition, P3HB-co-3HHx annealed at 70 degrees C had 5-30% more weight loss after the same duration of incubation in active sludge compared to the quenched samples. We suggest that annealing of P3HB-co-3HHx likely induces void formation in the semi-crystalline structure, facilitating the movement of water or perhaps enzymes to a higher degree of penetration into the sample and subsequently enhancing microbial degradation. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:547 / 556
页数:10
相关论文
共 46 条
[11]  
Flemming HC, 2001, WATER SCI TECHNOL, V43, pVII
[12]   MORPHOLOGY AND MELTING BEHAVIOR OF SEMI-CRYSTALLINE POLY(ETHYLENE-TEREPHTHALATE) .3. QUANTIFICATION OF CRYSTAL PERFECTION AND CRYSTALLINITY [J].
FONTAINE, F ;
LEDENT, J ;
GROENINCKX, G ;
REYNAERS, H .
POLYMER, 1982, 23 (02) :185-191
[13]   The polymer physics and chemistry of microbial cell attachment and adhesion [J].
Geoghegan, Mark ;
Andrews, Johanna S. ;
Biggs, Catherine A. ;
Eboigbodin, Kevin E. ;
Elliott, David R. ;
Rolfe, Stephen ;
Scholes, Julie ;
Ojeda, Jesus J. ;
Romero-Gonzalez, Maria E. ;
Edyvean, Robert G. J. ;
Swanson, Linda ;
Rutkaite, Ramune ;
Fernando, Rasika ;
Pen, Yu ;
Zhang, Zhenyu ;
Banwart, Steven A. .
FARADAY DISCUSSIONS, 2008, 139 :85-103
[14]   Comparison of cell-specific activity between free-living and attached bacteria using isolates and natural assemblages [J].
Grossart, Hans-Peter ;
Tang, Kam W. ;
Kiorboe, Thomas ;
Ploug, Helle .
FEMS MICROBIOLOGY LETTERS, 2007, 266 (02) :194-200
[15]   Thermal, crystallization, and biodegradation behavior of poly(3-hydroxybutyrate) blends with poly (butylene succinate-co-butylene adipate) and poly(butylene succinate-co-ε-caprolactone) [J].
He, Y ;
Masuda, T ;
Cao, A ;
Yoshie, N ;
Doi, Y ;
Inoue, Y .
POLYMER JOURNAL, 1999, 31 (02) :184-192
[16]   THE APPLICATION OF GAS BARRIER AND THERMAL-EXPANSION TECHNIQUES TO STUDY STRUCTURAL-CHANGES ON ANNEALING [J].
HOLDEN, PS ;
ORCHARD, GAJ ;
WARD, IM .
JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1985, 23 (11) :2295-2306
[17]   Improvement of the Thermal Stability of Polyhydroxybutyrates by Grafting with Maleic Anhydride by Different Methods: Differential Scanning Calorimetry, Thermogravimetric Analysis, and Gel Permeation Chromatography [J].
Hong, Shinn-Gwo ;
Lin, Yi-Che ;
Lin, Chia-Hau .
JOURNAL OF APPLIED POLYMER SCIENCE, 2008, 110 (05) :2718-2726
[18]   Multiple melting behavior of poly (3-hydroxybutyrate-co-3-hydroxyhexanoate) investigated by differential scanning calorimetry and infrared spectroscopy [J].
Hu, Yun ;
Zhang, Jianming ;
Sato, Harumi ;
Noda, Isao ;
Ozaki, Yukihiro .
POLYMER, 2007, 48 (16) :4777-4785
[19]   The effect of initial polymer morphology on the degradation and drug release from polyglycolide [J].
Hurrell, S ;
Cameron, RE .
BIOMATERIALS, 2002, 23 (11) :2401-2409
[20]   Banding in polyethylene and other spherulites [J].
Keith, HD ;
Padden, FJ .
MACROMOLECULES, 1996, 29 (24) :7776-7786