Factors affecting co-valorization of fayalitic and ferronickel slags for the production of alkali activated materials

被引:33
作者
Komnitsas, Konstantinos [1 ]
Yurramendi, Lourdes [2 ]
Bartzas, Georgios [3 ]
Karmali, Vasiliki [1 ]
Petrakis, Evangelos [1 ]
机构
[1] Tech Univ Crete, Sch Mineral Resources Engn, Univ Campus, Kounoupidiana 73100, Chania, Greece
[2] Tecnalia, Energy & Environm Div, Mikeletegi Pasealekuo 2, E-20009 San Sebastian, Spain
[3] Natl Tech Univ Athens, Sch Min & Met Engn, 9 Heroon Polytech Str, Athens 15780, Greece
关键词
Metallurgical slags; Alkali activation; Properties; Reactivity of slags; Alkali activated materials (AMMs); FLY-ASH; MECHANICAL-PROPERTIES; COMPRESSIVE STRENGTH; INORGANIC POLYMERS; SILICATE MODULUS; MOLAR RATIO; GEOPOLYMERS; MICROSTRUCTURE; CONSTRUCTION; TEMPERATURE;
D O I
10.1016/j.scitotenv.2020.137753
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
The first objective of this experimental study is the assessment of the alkali activation potential of two types of fayalitic slags, an as-received one (FS) and the one obtained after plasma treatment (FSP) of the initial FS, for the production of alkali activated materials (AAMs). Furthermore, the second objective is the elucidation of the co-valorization potential of FS and FSP slags when mixed with ferronickel (FeNi) slag (LS). The alkaline activating solution used was a mixture of sodium hydroxide (NaOH) and sodium silicate (Na2SiO3). The effect of various operating parameters, such as H2O/Na2O and SiO2/Na2O ratios present in the activating solution, curing temperature, curing period and ageing period on the compressive strength, density, water adsorption, porosity and toxicity of the produced AAMs was explored. The structural integrity of selected AAMs was investigated after firing specimens for 6 h at temperature up to 500 degrees C, immersion in distilled water and acidic solution or subjection to freeze-thaw cycles for a period of 7 or 30 days. The results of this study show that FS- and FSP-based AAMs acquire compressive strength of 44.8 MPa and 27.2 MPa, respectively. When FS and FSP were mixed with LS at 50:50%wt ratios the compressive strength of the produced specimens increased to 64.3 MPa and 45.8 MPa, respectively. Furthermore, selected AAMs produced after co-valorisation of slags retained sufficient compressive strength after firing at 500 degrees C, 45-68MPa, and exhibited very lowtoxicity. These findings prove the alkali activation potential of fayalitic slags aswell as their co-valorizationwith ferronickel slag for the production of AAMs, an approach which is in line with the principles of zero-waste and circular economy. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:11
相关论文
共 80 条
  • [1] Abdel-Ghani Nour T., 2018, HBRC Journal, V14, P159, DOI 10.1016/j.hbrcj.2016.06.001
  • [2] Impact of pyrometallurgical slags on sunflower growth, metal accumulation and rhizosphere microbial communities
    Agnello, A. C.
    Potysz, A.
    Fourdrin, C.
    Huguenot, D.
    Chauhan, P. S.
    [J]. CHEMOSPHERE, 2018, 208 : 626 - 639
  • [3] Microstructural characteristics and adsorption potential of a zeolitic tuff-metakaolin geopolymer
    Alshaaer, Mazen
    Zaharaki, Dimitra
    Komnitsas, Kostas
    [J]. DESALINATION AND WATER TREATMENT, 2015, 56 (02) : 338 - 345
  • [4] [Anonymous], 1995, 7341 NEN
  • [5] [Anonymous], 2002, EN1245732002 CEN
  • [6] ASTM (American Society for Testing and Materials), 2018, C126210 ASTM ASTM IN
  • [7] Life cycle assessment of ferronickel production in Greece
    Bartzas, Georgios
    Komnitsas, Kostas
    [J]. RESOURCES CONSERVATION AND RECYCLING, 2015, 105 : 113 - 122
  • [8] Evolution of binder structure in sodium silicate-activated slag-metakaolin blends
    Bernal, Susan A.
    Provis, John L.
    Rose, Volker
    Mejia de Gutierrez, Ruby
    [J]. CEMENT & CONCRETE COMPOSITES, 2011, 33 (01) : 46 - 54
  • [9] Effect of silicate modulus and metakaolin incorporation on the carbonation of alkali silicate-activated slags
    Bernal, Susan A.
    Mejla de Gutierrez, Ruby
    Provis, John L.
    Rose, Volker
    [J]. CEMENT AND CONCRETE RESEARCH, 2010, 40 (06) : 898 - 907
  • [10] BSI (British Standards Institute), 2007, 1936 BSI EN